Final Magnetic Moment6.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.662 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.110 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.85 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNb2(PO4)3 + NbPO5 + NbP2 + Li4P2O7 |
Band Gap0.155 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP3c1 [165] |
Hall-P 3 2"c |
Point Group3m |
Crystal Systemtrigonal |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 263.7 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 140.8 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 263.7 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 87.9 |
SiO2 (mp-6930) | <1 0 0> | <1 0 1> | 166.0 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 263.7 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 140.8 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 140.8 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 140.8 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 263.7 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 87.9 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 87.9 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 87.9 |
BN (mp-984) | <0 0 1> | <0 0 1> | 87.9 |
BN (mp-984) | <1 1 0> | <0 0 1> | 263.7 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 263.7 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 1> | 166.0 |
C (mp-66) | <1 1 1> | <0 0 1> | 87.9 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 263.7 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 263.7 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 263.7 |
CdSe (mp-2691) | <1 1 1> | <0 0 1> | 263.7 |
Au (mp-81) | <1 1 1> | <0 0 1> | 87.9 |
NaCl (mp-22862) | <1 1 0> | <1 0 0> | 140.8 |
CaCO3 (mp-3953) | <0 0 1> | <0 0 1> | 87.9 |
ZnO (mp-2133) | <0 0 1> | <0 0 1> | 263.7 |
GaSb (mp-1156) | <1 1 1> | <0 0 1> | 263.7 |
Ge (mp-32) | <1 1 0> | <1 0 0> | 140.8 |
Al2O3 (mp-1143) | <0 0 1> | <0 0 1> | 263.7 |
Cu (mp-30) | <1 0 0> | <0 0 1> | 263.7 |
ZnTe (mp-2176) | <1 1 1> | <0 0 1> | 263.7 |
Fe2O3 (mp-24972) | <1 0 0> | <1 0 0> | 140.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li2V5O12 (mp-776871) | 0.6261 | 0.019 | 3 |
Li2Cr5O12 (mp-773797) | 0.6227 | 0.077 | 3 |
Fe4(P2O7)3 (mp-578661) | 0.6474 | 0.001 | 3 |
Cr2P4O13 (mp-562181) | 0.6378 | 0.011 | 3 |
V6P7O24 (mp-32423) | 0.6230 | 0.023 | 3 |
Li9V3P8O29 (mp-504366) | 0.2505 | 0.004 | 4 |
Li9Sn3P8O29 (mp-779010) | 0.1802 | 0.080 | 4 |
Li9Fe3P8O29 (mp-579738) | 0.2952 | 0.003 | 4 |
Li9P8W3O29 (mp-777285) | 0.0667 | 0.026 | 4 |
Li9Sb3P8O29 (mp-776589) | 0.2575 | 0.056 | 4 |
Li8Fe7Sn(PO4)12 (mp-777579) | 0.4418 | 0.011 | 5 |
Li8TiFe7(PO4)12 (mp-777217) | 0.4249 | 0.011 | 5 |
Li8Fe7Co(PO4)12 (mp-781112) | 0.4378 | 0.023 | 5 |
Li8CrFe7(PO4)12 (mp-849438) | 0.4354 | 0.020 | 5 |
Li8NbFe7(PO4)12 (mp-776163) | 0.4222 | 0.006 | 5 |
Li4TiNi3Sn2(PO4)6 (mp-778249) | 0.6446 | 0.065 | 6 |
NaLi3Ti2Fe2(PO4)6 (mp-744690) | 0.6257 | 0.022 | 6 |
NaLi5Ti3Cr3(PO4)9 (mp-744549) | 0.6439 | 0.020 | 6 |
NaLi3Ti2Fe2(PO4)6 (mp-850140) | 0.6295 | 0.011 | 6 |
NaLi3Ti2Cr2(PO4)6 (mp-777190) | 0.6771 | 0.020 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Nb_pv P O |
Final Energy/Atom-7.0254 eV |
Corrected Energy-729.2253 eV
-729.2253 eV = -688.4924 eV (uncorrected energy) - 40.7328 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)