Final Magnetic Moment2.725 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.324 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.170 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.96 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMnPO4 + MnO2 + LiPO3 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 0 0> | <1 1 -1> | 148.3 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 305.8 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 76.5 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 229.4 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 305.8 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 76.5 |
SiO2 (mp-6930) | <0 0 1> | <1 1 0> | 130.3 |
SiO2 (mp-6930) | <1 1 1> | <1 0 -1> | 104.2 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 305.8 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 -1> | 208.3 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 128.9 |
LiF (mp-1138) | <1 1 0> | <1 0 -1> | 208.3 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 152.9 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 152.9 |
Ag (mp-124) | <1 1 0> | <1 1 -1> | 148.3 |
Al (mp-134) | <1 1 0> | <1 0 -1> | 208.3 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 128.9 |
TeO2 (mp-2125) | <1 0 0> | <1 0 -1> | 208.3 |
TeO2 (mp-2125) | <1 1 0> | <1 0 0> | 305.8 |
Al (mp-134) | <1 0 0> | <1 1 -1> | 148.3 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 229.4 |
Fe3O4 (mp-19306) | <1 1 0> | <1 0 -1> | 104.2 |
MgO (mp-1265) | <1 1 0> | <1 0 -1> | 104.2 |
LiTaO3 (mp-3666) | <0 0 1> | <1 0 0> | 229.4 |
Fe3O4 (mp-19306) | <1 0 0> | <1 1 -1> | 148.3 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 305.8 |
TiO2 (mp-2657) | <1 0 0> | <1 0 -1> | 208.3 |
TiO2 (mp-2657) | <1 1 1> | <1 0 0> | 229.4 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 0> | 305.8 |
PbS (mp-21276) | <1 1 0> | <1 0 -1> | 104.2 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 128.9 |
GaP (mp-2490) | <1 0 0> | <1 0 0> | 152.9 |
Ni (mp-23) | <1 1 0> | <1 0 -1> | 104.2 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 128.9 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 128.9 |
NdGaO3 (mp-3196) | <0 0 1> | <1 0 0> | 152.9 |
NdGaO3 (mp-3196) | <1 1 0> | <1 0 0> | 305.8 |
TbScO3 (mp-31119) | <1 1 0> | <1 0 0> | 305.8 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 305.8 |
PbSe (mp-2201) | <1 0 0> | <1 0 0> | 76.5 |
Ga2O3 (mp-886) | <1 0 0> | <1 0 0> | 305.8 |
Si (mp-149) | <1 0 0> | <1 1 -1> | 148.3 |
BaTiO3 (mp-5986) | <1 0 0> | <1 0 0> | 152.9 |
BaTiO3 (mp-5986) | <1 0 1> | <1 0 -1> | 208.3 |
BaTiO3 (mp-5986) | <1 1 1> | <0 0 1> | 257.9 |
NdGaO3 (mp-3196) | <1 1 1> | <0 1 0> | 211.0 |
C (mp-48) | <0 0 1> | <0 1 0> | 105.5 |
WSe2 (mp-1821) | <1 1 0> | <0 0 1> | 257.9 |
Ga2O3 (mp-886) | <0 1 0> | <1 0 -1> | 208.3 |
Au (mp-81) | <1 0 0> | <1 1 0> | 260.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CrFeO4 (mp-769919) | 0.3945 | 0.433 | 3 |
MgCrO4 (mp-540704) | 0.3979 | 0.902 | 3 |
VInO4 (mp-541501) | 0.3556 | 0.020 | 3 |
FeMoO4 (mp-541843) | 0.3890 | 0.399 | 3 |
MnMoO4 (mp-19081) | 0.3777 | 0.000 | 3 |
Li2Fe2(PO4)3 (mp-851285) | 0.3467 | 0.341 | 4 |
Li2Fe2(PO4)3 (mp-776769) | 0.2484 | 0.030 | 4 |
Li2Cr2(PO4)3 (mp-777909) | 0.1816 | 0.099 | 4 |
Li2V2(PO4)3 (mp-762579) | 0.3233 | 0.005 | 4 |
LiCo2(PO4)3 (mp-31602) | 0.3492 | 0.159 | 4 |
V4O9 (mp-715664) | 0.7351 | 0.116 | 2 |
MoO2 (mvc-6944) | 0.6440 | 0.281 | 2 |
Li7FeCo3(PO4)6 (mp-780179) | 0.3947 | 0.127 | 5 |
Li2MnV(PO4)3 (mp-770055) | 0.4010 | 0.030 | 5 |
Li7TiCr3(PO4)6 (mp-850412) | 0.3431 | 0.082 | 5 |
Li8Fe7Co(PO4)12 (mp-781112) | 0.3669 | 0.016 | 5 |
Li2MnV(PO4)3 (mp-770169) | 0.3426 | 0.026 | 5 |
NaLi3Ti2Fe2(PO4)6 (mp-744690) | 0.5417 | 0.193 | 6 |
NaLi3Ti2Fe2(PO4)6 (mp-850140) | 0.3884 | 0.114 | 6 |
NaLi3Ti2Cr2(PO4)6 (mp-777190) | 0.3993 | 0.020 | 6 |
LiTi3MnCr(PO4)6 (mp-772224) | 0.5382 | 0.001 | 6 |
Li2Ti2MnCr2(PO4)6 (mp-777244) | 0.5190 | 0.015 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv P O |
Final Energy/Atom-6.8488 eV |
Corrected Energy-283.8310 eV
-283.8310 eV = -260.2527 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction) - 6.7234 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)