Final Magnetic Moment5.992 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.678 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.096 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.54 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTi5(PO5)4 + SbPO4 + CrPO4 + TiP2O7 + Sb |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3 [146] |
HallR 3 |
Point Group3 |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 64.8 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 194.3 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 64.8 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 323.8 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 189.6 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 323.8 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 194.3 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 64.8 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 194.3 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 259.0 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 259.0 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 194.3 |
BN (mp-984) | <1 1 0> | <0 0 1> | 64.8 |
Al (mp-134) | <1 1 1> | <0 0 1> | 194.3 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 129.5 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 194.3 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 323.8 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <0 0 1> | 194.3 |
C (mp-66) | <1 1 1> | <0 0 1> | 64.8 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 259.0 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 323.8 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 64.8 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 259.0 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 323.8 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 259.0 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 64.8 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 194.3 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 259.0 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 323.8 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 64.8 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 64.8 |
CdSe (mp-2691) | <1 1 1> | <0 0 1> | 64.8 |
BaTiO3 (mp-5986) | <1 1 0> | <0 0 1> | 194.3 |
SiC (mp-11714) | <0 0 1> | <0 0 1> | 259.0 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 259.0 |
C (mp-48) | <0 0 1> | <1 0 0> | 189.6 |
WSe2 (mp-1821) | <1 1 1> | <0 0 1> | 259.0 |
Ge(Bi3O5)4 (mp-23352) | <1 1 1> | <0 0 1> | 194.3 |
CdSe (mp-2691) | <1 0 0> | <0 0 1> | 194.3 |
YAlO3 (mp-3792) | <0 1 0> | <0 0 1> | 323.8 |
YAlO3 (mp-3792) | <1 0 0> | <0 0 1> | 323.8 |
WSe2 (mp-1821) | <0 0 1> | <0 0 1> | 259.0 |
WSe2 (mp-1821) | <1 1 0> | <0 0 1> | 259.0 |
ZrO2 (mp-2858) | <0 1 1> | <0 0 1> | 194.3 |
SiC (mp-8062) | <1 1 0> | <0 0 1> | 323.8 |
CaCO3 (mp-3953) | <0 0 1> | <0 0 1> | 64.8 |
CaCO3 (mp-3953) | <1 0 0> | <0 0 1> | 259.0 |
GaSb (mp-1156) | <1 1 1> | <0 0 1> | 64.8 |
SiC (mp-8062) | <1 0 0> | <0 0 1> | 194.3 |
ZnO (mp-2133) | <0 0 1> | <0 0 1> | 64.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
MnPO4 (mp-773411) | 0.2193 | 0.344 | 3 |
VPO4 (mp-861584) | 0.3026 | 0.079 | 3 |
MnPO4 (mp-504382) | 0.4391 | 0.070 | 3 |
CoPO4 (mp-510669) | 0.4758 | 0.197 | 3 |
TiPO4 (mp-779587) | 0.4211 | 0.077 | 3 |
Fe2Sn(PO4)3 (mp-775649) | 0.1422 | 0.326 | 4 |
Cr2Te(PO4)3 (mp-775273) | 0.1919 | 0.094 | 4 |
Ti2Sb(PO4)3 (mp-773711) | 0.0947 | 0.118 | 4 |
V2Sb(PO4)3 (mp-773573) | 0.0983 | 0.223 | 4 |
Fe2Sb(PO4)3 (mp-849513) | 0.1481 | 0.272 | 4 |
Cr5O12 (mp-773920) | 0.7148 | 0.000 | 2 |
Mo4O11 (mp-565865) | 0.7387 | 0.026 | 2 |
V5O12 (mp-778252) | 0.6849 | 0.024 | 2 |
CrFe3Sb2(PO4)6 (mp-775989) | 0.1039 | 0.852 | 5 |
Ti3VSb2(PO4)6 (mp-775706) | 0.0934 | 0.085 | 5 |
CdFeSn(PO4)3 (mp-705344) | 0.1182 | 0.074 | 5 |
TiCdFe(PO4)3 (mp-743598) | 0.1271 | 0.134 | 5 |
V3CrSb2(PO4)6 (mp-765776) | 0.0933 | 0.074 | 5 |
Na2Li3Ti3Al(PO4)6 (mp-769078) | 0.4670 | 0.068 | 6 |
Zr12Si2Bi2P16PbO72 (mp-693759) | 0.4411 | 0.009 | 6 |
LiTi3MnCr(PO4)6 (mp-772224) | 0.2957 | 0.001 | 6 |
Na2LiTi3Al(PO4)6 (mp-769074) | 0.4700 | 0.011 | 6 |
Na2LiTi3Al(PO4)6 (mp-769073) | 0.4672 | 0.014 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eV |
PseudopotentialsVASP PAW: Ti_pv Cr_pv Sb P O |
Final Energy/Atom-7.5105 eV |
Corrected Energy-289.2449 eV
-289.2449 eV = -270.3769 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction) - 2.0130 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)