Final Magnetic Moment26.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.392 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.026 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.53 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi3CrO4 + LiCrO2 + Li32Ti11Cr5O48 |
Band Gap1.137 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 265.2 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 176.8 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 309.4 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 132.6 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 309.4 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 309.4 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 221.0 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 309.4 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 132.6 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 221.0 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 353.6 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 353.6 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 221.0 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 44.2 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 221.0 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 309.4 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 88.4 |
CdS (mp-672) | <1 0 1> | <1 1 -1> | 194.9 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 309.4 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 221.0 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 353.6 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 265.2 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 353.6 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 265.2 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 309.4 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 353.6 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 88.4 |
Ag (mp-124) | <1 1 0> | <1 -1 0> | 194.6 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 265.2 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 265.2 |
BN (mp-984) | <1 0 1> | <0 0 1> | 265.2 |
BN (mp-984) | <1 1 0> | <0 0 1> | 132.6 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 296.1 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 88.4 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 132.6 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 88.4 |
BN (mp-984) | <0 0 1> | <0 0 1> | 44.2 |
BN (mp-984) | <1 0 0> | <0 0 1> | 309.4 |
BN (mp-984) | <1 1 1> | <0 0 1> | 132.6 |
Al (mp-134) | <1 1 0> | <0 0 1> | 353.6 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 353.6 |
LiGaO2 (mp-5854) | <1 1 1> | <0 0 1> | 265.2 |
Al (mp-134) | <1 0 0> | <0 0 1> | 353.6 |
Al (mp-134) | <1 1 1> | <0 0 1> | 88.4 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 221.0 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 132.6 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 0> | 296.1 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 353.6 |
TeO2 (mp-2125) | <1 0 1> | <0 0 1> | 309.4 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 353.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li17Ni11O28 (mp-767977) | 0.1339 | 0.043 | 3 |
LiCoO2 (mp-868388) | 0.1392 | 0.090 | 3 |
Li2CrO3 (mp-770628) | 0.1480 | 0.025 | 3 |
Li7Ni5O12 (mp-773266) | 0.1396 | 0.007 | 3 |
Na2PrO3 (mp-28429) | 0.1384 | 0.120 | 3 |
Li24TiCr11O36 (mp-780842) | 0.0473 | 0.084 | 4 |
Li32Ti3Cr13O48 (mp-777523) | 0.0423 | 0.104 | 4 |
Li24Ti5Cr7O36 (mp-771365) | 0.0484 | 0.217 | 4 |
Li4TiCrO6 (mp-771228) | 0.0405 | 0.098 | 4 |
Li24Ti5Cr7O36 (mp-771301) | 0.0440 | 0.105 | 4 |
Te2Au (mp-1662) | 0.3659 | 0.018 | 2 |
NaTe3 (mp-28478) | 0.3816 | 0.000 | 2 |
LiTe3 (mp-27466) | 0.4215 | 0.009 | 2 |
Bi4Te3 (mp-28229) | 0.4347 | 0.000 | 2 |
Te2Au (mp-567525) | 0.3558 | 0.018 | 2 |
Na6MnNi3(SbO6)2 (mp-1094109) | 0.3243 | 0.139 | 5 |
Na (mp-999501) | 0.6337 | 0.114 | 1 |
Sb (mp-632286) | 0.5400 | 0.059 | 1 |
Bi (mp-23152) | 0.6476 | 0.000 | 1 |
Te (mp-570459) | 0.5061 | 0.044 | 1 |
Te (mp-105) | 0.6418 | 0.047 | 1 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eV |
PseudopotentialsVASP PAW: Li_sv Ti_pv Cr_pv O |
Final Energy/Atom-6.4327 eV |
Corrected Energy-677.4184 eV
-677.4184 eV = -617.5395 eV (uncorrected energy) - 33.7099 eV (MP Anion Correction) - 26.1690 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)