Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.062 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.030 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.54 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToK3AlO3 + K2O |
Band Gap2.221 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 137.8 |
LiF (mp-1138) | <1 0 0> | <1 0 -1> | 150.8 |
LiF (mp-1138) | <1 1 1> | <1 1 0> | 171.7 |
Al (mp-134) | <1 1 0> | <1 0 0> | 137.8 |
Al (mp-134) | <1 1 1> | <1 1 0> | 171.7 |
TeO2 (mp-2125) | <0 1 0> | <1 0 0> | 137.8 |
TeO2 (mp-2125) | <1 0 0> | <1 0 0> | 137.8 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 -1> | 150.8 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 234.0 |
CeO2 (mp-20194) | <1 0 0> | <1 0 -1> | 150.8 |
GaN (mp-804) | <1 1 1> | <1 1 -1> | 182.2 |
InAs (mp-20305) | <1 0 0> | <1 0 -1> | 150.8 |
Mg (mp-153) | <1 1 1> | <1 1 -1> | 182.2 |
GaP (mp-2490) | <1 0 0> | <1 0 -1> | 150.8 |
BaTiO3 (mp-5986) | <1 0 0> | <1 0 -1> | 150.8 |
BaTiO3 (mp-5986) | <1 1 1> | <1 1 0> | 171.7 |
NdGaO3 (mp-3196) | <0 0 1> | <1 1 -1> | 182.2 |
MoSe2 (mp-1634) | <0 0 1> | <1 1 0> | 171.7 |
MoSe2 (mp-1634) | <1 1 1> | <1 1 0> | 171.7 |
Ga2O3 (mp-886) | <1 0 -1> | <1 0 -1> | 150.8 |
Si (mp-149) | <1 0 0> | <1 0 -1> | 150.8 |
WSe2 (mp-1821) | <1 1 1> | <1 1 0> | 171.7 |
ZrO2 (mp-2858) | <0 1 1> | <0 1 1> | 155.5 |
ZrO2 (mp-2858) | <1 1 0> | <0 1 0> | 204.7 |
Y3Fe5O12 (mp-19648) | <1 0 0> | <1 0 -1> | 150.8 |
MgF2 (mp-1249) | <1 0 0> | <0 0 1> | 117.0 |
CaF2 (mp-2741) | <1 0 0> | <1 0 -1> | 150.8 |
ZnTe (mp-2176) | <1 0 0> | <1 0 -1> | 150.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li8B2O7 (mp-768921) | 0.5171 | 0.045 | 3 |
Rb8Fe2O7 (mp-770320) | 0.1691 | 0.052 | 3 |
Na2Cr2O7 (mp-743627) | 0.5745 | 0.005 | 3 |
K5As3O10 (mp-27674) | 0.6029 | 0.000 | 3 |
SrSiO3 (mp-561547) | 0.5607 | 0.036 | 3 |
Ca3Mg(SiO4)2 (mp-558079) | 0.6007 | 0.102 | 4 |
LiBiP2O7 (mp-584134) | 0.6025 | 0.035 | 4 |
Na3Sb(PO4)2 (mp-776965) | 0.5625 | 0.011 | 4 |
K8Li3Cr4O16 (mp-782640) | 0.5934 | 0.034 | 4 |
VP2Pb2O9 (mp-645799) | 0.5143 | 0.000 | 4 |
K2LiVPO6 (mp-764301) | 0.6616 | 0.081 | 5 |
SrMgTi(PO4)2 (mvc-2641) | 0.6468 | 0.152 | 5 |
SrCaSn(PO4)2 (mvc-2825) | 0.6654 | 0.051 | 5 |
KNaLi2(SO4)2 (mp-14484) | 0.6164 | 0.000 | 5 |
Na2TeHSO5F3 (mp-696485) | 0.7127 | 0.016 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: K_sv Al O |
Final Energy/Atom-4.7738 eV |
Corrected Energy-344.2816 eV
-344.2816 eV = -324.6175 eV (uncorrected energy) - 19.6641 eV (MP Anion Correction)
|