Final Magnetic Moment4.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.855 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.122 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.25 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTi5(PO5)4 + Ni12P5 + TiP2O7 + Ni3P |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3 [146] |
HallR 3 |
Point Group3 |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 263.2 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 329.0 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 197.4 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 197.4 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 65.8 |
GaN (mp-804) | <0 0 1> | <1 0 1> | 187.9 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 65.8 |
InAs (mp-20305) | <1 0 0> | <1 0 1> | 187.9 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 263.2 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 65.8 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 197.4 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 197.4 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 197.4 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 263.2 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 263.2 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 263.2 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 263.2 |
BN (mp-984) | <0 0 1> | <0 0 1> | 65.8 |
BN (mp-984) | <1 1 0> | <0 0 1> | 65.8 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 197.4 |
Al (mp-134) | <1 1 1> | <0 0 1> | 197.4 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 131.6 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 197.4 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 329.0 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 176.0 |
TiO2 (mp-2657) | <1 1 1> | <1 0 0> | 176.0 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <0 0 1> | 197.4 |
C (mp-66) | <1 1 1> | <0 0 1> | 65.8 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 329.0 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 329.0 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 263.2 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 65.8 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 329.0 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 263.2 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 65.8 |
ZrO2 (mp-2858) | <0 1 1> | <0 0 1> | 197.4 |
CaCO3 (mp-3953) | <0 0 1> | <0 0 1> | 65.8 |
CaCO3 (mp-3953) | <1 0 0> | <0 0 1> | 263.2 |
YAlO3 (mp-3792) | <1 0 0> | <0 0 1> | 329.0 |
YAlO3 (mp-3792) | <1 1 0> | <0 0 1> | 329.0 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 197.4 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 65.8 |
SiC (mp-8062) | <1 1 0> | <0 0 1> | 329.0 |
MoSe2 (mp-1634) | <1 1 0> | <0 0 1> | 263.2 |
Si (mp-149) | <1 1 0> | <0 0 1> | 329.0 |
Si (mp-149) | <1 1 1> | <0 0 1> | 197.4 |
Au (mp-81) | <1 1 1> | <0 0 1> | 263.2 |
CdSe (mp-2691) | <1 0 0> | <0 0 1> | 197.4 |
CdSe (mp-2691) | <1 1 0> | <0 0 1> | 263.2 |
CdSe (mp-2691) | <1 1 1> | <0 0 1> | 65.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Fe7(PO5)4 (mp-761434) | 0.3450 | 0.768 | 3 |
MnPO4 (mp-773411) | 0.3356 | 0.344 | 3 |
VPO4 (mp-861584) | 0.2086 | 0.079 | 3 |
FePO4 (mp-773675) | 0.2657 | 0.045 | 3 |
TiPO4 (mp-779587) | 0.1275 | 0.077 | 3 |
CrNi5(PO4)6 (mp-772386) | 0.1101 | 0.087 | 4 |
Ti5Mn(PO4)6 (mp-777450) | 0.1033 | 0.089 | 4 |
Ti5V(PO4)6 (mp-772584) | 0.0726 | 0.077 | 4 |
NbNi5(PO4)6 (mp-772455) | 0.1141 | 0.087 | 4 |
Ti5Cr(PO4)6 (mp-776640) | 0.1142 | 0.090 | 4 |
VO2 (mp-777469) | 0.7289 | 0.038 | 2 |
VO2 (mvc-6918) | 0.6687 | 0.095 | 2 |
MoO2 (mvc-6944) | 0.6188 | 0.281 | 2 |
CrFe3Co2(PO4)6 (mp-762179) | 0.1015 | 0.883 | 5 |
MnFe3Co2(PO4)6 (mp-762041) | 0.1166 | 0.036 | 5 |
CrFe3Ni2(PO4)6 (mp-850902) | 0.1195 | 1.089 | 5 |
VFe3Co2(PO4)6 (mp-777311) | 0.1012 | 0.055 | 5 |
Cr2Fe3Co(PO4)6 (mp-776058) | 0.1243 | 1.623 | 5 |
Li4Mn3CrCo2(PO4)6 (mp-763479) | 0.5937 | 0.080 | 6 |
NaLi3Ti2Fe2(PO4)6 (mp-850140) | 0.5613 | 0.114 | 6 |
NaLi3Ti2Cr2(PO4)6 (mp-777190) | 0.5230 | 0.020 | 6 |
LiTi3MnCr(PO4)6 (mp-772224) | 0.4035 | 0.001 | 6 |
Li2Ti2MnCr2(PO4)6 (mp-777244) | 0.5423 | 0.015 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesNi: 6.2 eV |
PseudopotentialsVASP PAW: Ti_pv Ni_pv P O |
Final Energy/Atom-7.7842 eV |
Corrected Energy-299.2509 eV
-299.2509 eV = -280.2319 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction) - 2.1640 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)