Final Magnetic Moment15.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.992 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.089 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.66 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMnF2 + LiF |
Band Gap3.005 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 0 0> | 172.2 |
GaN (mp-804) | <1 0 1> | <1 0 -1> | 190.4 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 86.1 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 231.2 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 186.0 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 186.0 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 289.0 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 289.0 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 186.0 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 231.2 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 258.2 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 289.0 |
LiF (mp-1138) | <1 1 0> | <1 0 -1> | 190.4 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 172.2 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 186.0 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 289.0 |
BN (mp-984) | <1 1 1> | <0 1 0> | 231.2 |
Al (mp-134) | <1 1 0> | <0 0 1> | 186.0 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 86.1 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 186.0 |
BN (mp-984) | <0 0 1> | <1 0 0> | 258.2 |
BN (mp-984) | <1 0 1> | <0 1 0> | 289.0 |
LiNbO3 (mp-3731) | <0 0 1> | <0 1 0> | 289.0 |
LiNbO3 (mp-3731) | <1 0 0> | <0 1 0> | 289.0 |
LiNbO3 (mp-3731) | <1 0 1> | <0 1 0> | 231.2 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 0> | 231.2 |
LiTaO3 (mp-3666) | <1 0 0> | <0 1 0> | 289.0 |
MoS2 (mp-1434) | <0 0 1> | <0 1 1> | 194.8 |
TeO2 (mp-2125) | <0 0 1> | <1 0 -1> | 190.4 |
C (mp-66) | <1 1 0> | <0 1 0> | 289.0 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 0> | 258.2 |
LiTaO3 (mp-3666) | <0 0 1> | <0 1 0> | 289.0 |
LiTaO3 (mp-3666) | <1 0 1> | <0 1 0> | 231.2 |
Mg (mp-153) | <1 0 0> | <0 1 0> | 289.0 |
Mg (mp-153) | <1 1 0> | <1 0 0> | 86.1 |
GdScO3 (mp-5690) | <0 0 1> | <1 0 -1> | 190.4 |
GdScO3 (mp-5690) | <1 0 0> | <0 0 1> | 186.0 |
Mg (mp-153) | <0 0 1> | <0 1 0> | 173.4 |
TbScO3 (mp-31119) | <0 0 1> | <1 0 -1> | 190.4 |
InSb (mp-20012) | <1 1 0> | <0 0 1> | 186.0 |
SiC (mp-11714) | <1 1 0> | <1 0 0> | 172.2 |
Ni (mp-23) | <1 1 0> | <1 0 -1> | 190.4 |
MoSe2 (mp-1634) | <1 0 0> | <1 0 0> | 258.2 |
MoSe2 (mp-1634) | <1 1 1> | <0 1 0> | 173.4 |
Au (mp-81) | <1 0 0> | <0 1 0> | 289.0 |
BaTiO3 (mp-5986) | <1 1 0> | <1 0 -1> | 190.4 |
NdGaO3 (mp-3196) | <0 0 1> | <0 0 1> | 186.0 |
ZrO2 (mp-2858) | <1 0 -1> | <0 1 0> | 289.0 |
ZrO2 (mp-2858) | <1 0 0> | <1 0 0> | 86.1 |
ZrO2 (mp-2858) | <1 0 1> | <1 0 0> | 86.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li2MnF5 (mp-767572) | 0.5704 | 0.063 | 3 |
Mg3(AsO4)2 (mp-770734) | 0.4426 | 0.043 | 3 |
Zn3(PO4)2 (mp-553958) | 0.6251 | 0.026 | 3 |
Cu3(AsO4)2 (mp-540858) | 0.5584 | 0.004 | 3 |
Na2Ge2O5 (mp-771248) | 0.5894 | 0.012 | 3 |
LiNiPO4 (mp-762243) | 0.6291 | 0.124 | 4 |
Li2CoP2O7 (mp-778917) | 0.5978 | 0.061 | 4 |
LiFeSiO4 (mp-762686) | 0.5906 | 0.088 | 4 |
Li3Fe3(PO4)4 (mp-31797) | 0.6187 | 0.051 | 4 |
ZnSn(GeO3)2 (mvc-8073) | 0.5413 | 0.165 | 4 |
Li7CuAs4ClO14 (mp-769204) | 0.6534 | 0.074 | 5 |
Sr2AlCr2GaO7 (mvc-312) | 0.6664 | 0.186 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv F |
Final Energy/Atom-5.5966 eV |
Corrected Energy-200.3694 eV
-200.3694 eV = -190.2843 eV (uncorrected energy) - 10.0851 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)