Final Magnetic Moment4.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.321 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.060 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.98 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToFeO + LiFePO4 + Li3PO4 + H2O |
Band Gap3.823 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <0 1 1> | 225.8 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 201.7 |
AlN (mp-661) | <1 0 0> | <1 1 1> | 78.9 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 242.7 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 201.7 |
CeO2 (mp-20194) | <1 1 0> | <1 1 -1> | 215.8 |
CeO2 (mp-20194) | <1 1 1> | <1 1 0> | 303.4 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 201.7 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 1> | 232.7 |
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 350.7 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 182.0 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 282.4 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 161.4 |
CeO2 (mp-20194) | <1 0 0> | <1 1 0> | 60.7 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 208.2 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 148.7 |
GaN (mp-804) | <1 1 1> | <0 1 -1> | 281.5 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 350.7 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 194.8 |
SiO2 (mp-6930) | <1 0 1> | <1 -1 1> | 179.5 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 267.6 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 116.3 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 201.7 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 272.7 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 1> | 174.5 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 327.1 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 208.2 |
SiO2 (mp-6930) | <1 1 0> | <0 1 -1> | 281.5 |
ZnSe (mp-1190) | <1 0 0> | <0 1 -1> | 281.5 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 182.0 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 -1> | 281.5 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 0> | 311.7 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 272.7 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 182.0 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 322.8 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 182.0 |
CdS (mp-672) | <1 0 0> | <0 1 -1> | 201.1 |
LiF (mp-1138) | <1 0 0> | <1 0 -1> | 283.6 |
YVO4 (mp-19133) | <1 0 0> | <0 1 -1> | 321.8 |
CdS (mp-672) | <0 0 1> | <1 0 1> | 232.7 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 267.6 |
CdS (mp-672) | <1 1 0> | <0 1 -1> | 201.1 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 148.7 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 322.8 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 161.4 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 327.1 |
TePb (mp-19717) | <1 0 0> | <1 -1 0> | 306.5 |
Te2Mo (mp-602) | <1 0 1> | <0 1 -1> | 281.5 |
Ag (mp-124) | <1 0 0> | <0 1 -1> | 281.5 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 148.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
La2SiO5 (mp-771045) | 0.7042 | 0.050 | 3 |
Rb2SeO4 (mp-677526) | 0.5638 | 0.014 | 3 |
K2RuO4 (mp-17789) | 0.6864 | 0.000 | 3 |
Na2SO4 (mp-505274) | 0.6208 | 0.006 | 3 |
Ca2SiO4 (mp-758006) | 0.6707 | 0.058 | 3 |
Mg7P2(HO2)8 (mp-699232) | 0.5713 | 0.000 | 4 |
Na3In(PO4)2 (mp-6336) | 0.5843 | 0.000 | 4 |
Mg2PHO5 (mp-23740) | 0.5889 | 0.000 | 4 |
SrNi2(PO4)2 (mp-19647) | 0.5039 | 0.003 | 4 |
Ba3V2S4O3 (mp-19652) | 0.6278 | 0.040 | 4 |
Li2CoPHO5 (mp-943466) | 0.1833 | 0.062 | 5 |
Na3LiSbP2O9 (mp-761144) | 0.5041 | 0.081 | 5 |
Li2VPHO5 (mp-778560) | 0.1687 | 0.079 | 5 |
Li2MnPHO5 (mp-776527) | 0.5028 | 0.055 | 5 |
Li2MnPHO5 (mp-777530) | 0.1332 | 0.057 | 5 |
Li3VCrP2(HO5)2 (mp-767626) | 0.6066 | 0.068 | 6 |
Li3MnVP2(HO5)2 (mp-765960) | 0.7386 | 0.045 | 6 |
Li2MnVP2(HO5)2 (mp-849530) | 0.7134 | 0.026 | 6 |
Li3VFeP2(HO5)2 (mp-765312) | 0.6920 | 0.139 | 6 |
AsC4S2Cl2O2F13 (mp-560424) | 0.6908 | 0.226 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv P H O |
Final Energy/Atom-6.2643 eV |
Corrected Energy-137.7741 eV
-137.7741 eV = -125.2852 eV (uncorrected energy) - 7.0229 eV (MP Anion Correction) - 5.4660 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)