Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.230 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.259 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.65 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi3Fe3(PO4)4 + Li3B7O12 + Fe2O3 + Li3PO4 + O2 |
Band Gap0.228 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/m [11] |
Hall-P 2yb |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 -1> | 310.6 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 218.1 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 296.7 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 -1> | 124.2 |
AlN (mp-661) | <0 0 1> | <1 0 -1> | 186.3 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 164.8 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 197.8 |
GaAs (mp-2534) | <1 1 0> | <0 1 1> | 328.1 |
BaF2 (mp-1029) | <1 0 0> | <1 0 -1> | 124.2 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 230.8 |
CeO2 (mp-20194) | <1 0 0> | <1 1 1> | 236.7 |
GaAs (mp-2534) | <1 1 1> | <1 1 -1> | 227.7 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 218.1 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 33.0 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 230.8 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 197.2 |
GaN (mp-804) | <1 1 1> | <1 1 1> | 236.7 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 362.7 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 164.8 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 296.7 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 296.7 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 -1> | 227.7 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 -1> | 310.6 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 -1> | 227.7 |
CdS (mp-672) | <1 0 0> | <1 1 -1> | 227.7 |
CdS (mp-672) | <1 0 1> | <1 1 -1> | 227.7 |
CdS (mp-672) | <1 1 0> | <0 1 0> | 261.7 |
LiF (mp-1138) | <1 0 0> | <1 0 -1> | 248.4 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 218.1 |
Te2W (mp-22693) | <0 0 1> | <1 0 1> | 65.7 |
Te2W (mp-22693) | <0 1 0> | <0 1 0> | 261.7 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 274.0 |
KCl (mp-23193) | <1 0 0> | <1 0 -1> | 124.2 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 230.8 |
YVO4 (mp-19133) | <1 0 0> | <1 0 -1> | 186.3 |
YVO4 (mp-19133) | <1 1 0> | <1 0 1> | 65.7 |
TePb (mp-19717) | <1 0 0> | <1 0 -1> | 124.2 |
Te2Mo (mp-602) | <0 0 1> | <1 0 -1> | 310.6 |
ZnSe (mp-1190) | <1 1 1> | <1 1 -1> | 227.7 |
Ag (mp-124) | <1 0 0> | <1 0 1> | 262.9 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 263.7 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 -1> | 227.7 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 261.7 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 263.7 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 98.9 |
GaSe (mp-1943) | <1 1 1> | <0 0 1> | 230.8 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 263.7 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 98.9 |
Te2W (mp-22693) | <1 0 1> | <0 0 1> | 98.9 |
BN (mp-984) | <1 0 0> | <0 0 1> | 230.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li3V(BO2)5 (mp-770344) | 0.6401 | 0.111 | 4 |
Li3Ni2(PO4)3 (mp-504139) | 0.6751 | 0.242 | 4 |
CoCu2(BO3)2 (mp-620325) | 0.6447 | 0.214 | 4 |
Li9Cr4(BO3)8 (mp-763230) | 0.6311 | 0.086 | 4 |
Li9Cr4(BO3)8 (mp-765270) | 0.6453 | 0.075 | 4 |
Li2AlPCO7 (mp-767214) | 0.1724 | 0.029 | 5 |
Li2NiCSO7 (mp-771489) | 0.3776 | 0.061 | 5 |
Li2MnBAsO7 (mp-772692) | 0.3758 | 0.080 | 5 |
Li2MnBPO7 (mp-772263) | 0.3193 | 0.072 | 5 |
Li2CoPCO7 (mp-25482) | 0.3416 | 0.050 | 5 |
Li12V3CrP4(CO7)4 (mp-767729) | 0.6685 | 0.069 | 6 |
Li12MnNi3P4(CO7)4 (mp-767698) | 0.6658 | 0.040 | 6 |
Li6MnNiP2(CO7)2 (mp-767293) | 0.6624 | 0.046 | 6 |
Li6MnVP2(CO7)2 (mp-767281) | 0.6722 | 0.095 | 6 |
NaLiMnPCO7 (mp-763833) | 0.6165 | 0.000 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv B P O |
Final Energy/Atom-6.5108 eV |
Corrected Energy-171.5574 eV
-171.5574 eV = -156.2594 eV (uncorrected energy) - 9.8321 eV (MP Anion Correction) - 5.4660 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)