Final Magnetic Moment12.277 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.395 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.192 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.40 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiMnPO4 + MnPO4 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 0 0> | 252.8 |
AlN (mp-661) | <0 0 1> | <1 0 -1> | 136.3 |
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 286.9 |
GaN (mp-804) | <1 0 0> | <1 0 -1> | 136.3 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 152.4 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 152.4 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 84.3 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 252.8 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 252.8 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 215.2 |
BN (mp-984) | <1 0 0> | <0 1 0> | 215.2 |
LiGaO2 (mp-5854) | <1 0 1> | <1 1 0> | 221.3 |
LiGaO2 (mp-5854) | <1 1 1> | <0 1 0> | 286.9 |
CdTe (mp-406) | <1 1 0> | <1 0 0> | 252.8 |
TeO2 (mp-2125) | <1 1 0> | <0 1 0> | 286.9 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 152.4 |
TiO2 (mp-2657) | <1 1 0> | <0 1 0> | 215.2 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 152.4 |
KP(HO2)2 (mp-23959) | <1 0 1> | <1 0 -1> | 136.3 |
KP(HO2)2 (mp-23959) | <1 1 0> | <1 0 -1> | 136.3 |
GaP (mp-2490) | <1 0 0> | <0 0 1> | 152.4 |
InP (mp-20351) | <1 1 0> | <1 0 0> | 252.8 |
InSb (mp-20012) | <1 1 0> | <1 0 0> | 252.8 |
BaTiO3 (mp-5986) | <1 0 0> | <0 0 1> | 152.4 |
NdGaO3 (mp-3196) | <0 0 1> | <0 1 0> | 215.2 |
SiC (mp-11714) | <1 0 0> | <1 0 0> | 252.8 |
MoSe2 (mp-1634) | <1 0 1> | <0 1 0> | 215.2 |
Ga2O3 (mp-886) | <1 0 -1> | <0 0 1> | 152.4 |
Ga2O3 (mp-886) | <1 0 0> | <1 0 0> | 252.8 |
Si (mp-149) | <1 1 0> | <0 1 0> | 286.9 |
CdSe (mp-2691) | <1 0 0> | <0 0 1> | 152.4 |
C (mp-48) | <0 0 1> | <0 1 0> | 215.2 |
C (mp-48) | <1 0 0> | <1 0 0> | 252.8 |
ZrO2 (mp-2858) | <1 0 -1> | <1 0 0> | 252.8 |
ZrO2 (mp-2858) | <1 1 -1> | <1 1 0> | 221.3 |
SiC (mp-8062) | <1 0 0> | <0 0 1> | 152.4 |
CdWO4 (mp-19387) | <0 1 1> | <0 1 0> | 286.9 |
CdWO4 (mp-19387) | <1 0 0> | <0 1 0> | 286.9 |
MgF2 (mp-1249) | <1 1 1> | <0 1 0> | 215.2 |
GaSb (mp-1156) | <1 0 0> | <0 0 1> | 152.4 |
GaTe (mp-542812) | <1 0 0> | <1 0 -1> | 136.3 |
LiAlO2 (mp-3427) | <1 0 0> | <0 1 0> | 286.9 |
CaF2 (mp-2741) | <1 0 0> | <0 0 1> | 152.4 |
ZnTe (mp-2176) | <1 0 0> | <0 0 1> | 152.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Er2GeO5 (mp-774547) | 0.5134 | 0.005 | 3 |
Li2Cr2O7 (mp-770745) | 0.5246 | 0.068 | 3 |
Mg3(PO4)2 (mp-560623) | 0.5393 | 0.014 | 3 |
Fe3(PO4)2 (mp-19346) | 0.5356 | 0.581 | 3 |
Mn4(PO4)3 (mp-31944) | 0.5462 | 0.029 | 3 |
LiCu4(PO4)3 (mp-761193) | 0.2508 | 0.084 | 4 |
Li3Ti2(PO4)3 (mp-758287) | 0.3326 | 0.098 | 4 |
Na2Fe3(PO4)3 (mp-566867) | 0.3221 | 0.001 | 4 |
Na3In2(AsO4)3 (mp-22804) | 0.2626 | 0.000 | 4 |
Li3V2(PO4)3 (mp-540455) | 0.3093 | 0.085 | 4 |
Li6MnV3(PO4)6 (mp-764970) | 0.4502 | 0.204 | 5 |
Li6MnV3(PO4)6 (mp-764856) | 0.4753 | 0.168 | 5 |
Li6MnV3(PO4)6 (mp-764485) | 0.4512 | 0.114 | 5 |
Li6MnV3(PO4)6 (mp-764756) | 0.4639 | 0.154 | 5 |
Li6MnV3(PO4)6 (mp-779407) | 0.4393 | 0.122 | 5 |
Li2Mg2MnFe(PO4)4 (mp-849669) | 0.5411 | 0.008 | 6 |
NaLiMn2Fe4(PO4)6 (mp-777193) | 0.6464 | 0.018 | 6 |
Li4CrFe2Ni3(PO4)6 (mp-776753) | 0.7488 | 0.778 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv P O |
Final Energy/Atom-7.0678 eV |
Corrected Energy-309.6514 eV
-309.6514 eV = -282.7113 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction) - 10.0851 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)