Final Magnetic Moment23.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.941 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.098 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.26 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi4MnCrO6 + Li24Mn11CrO36 + NiO + Ni |
Band Gap0.374 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCm [8] |
HallC 2y |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 0 0> | 232.2 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 101.2 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 170.0 |
GaN (mp-804) | <1 1 0> | <0 1 1> | 118.4 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 122.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 245.6 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 174.1 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 202.4 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 290.2 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 174.1 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 122.8 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 290.2 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 245.6 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 290.2 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 58.0 |
BN (mp-984) | <1 0 0> | <0 0 1> | 307.0 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 184.2 |
LiNbO3 (mp-3731) | <1 0 1> | <0 0 1> | 307.0 |
LiNbO3 (mp-3731) | <1 1 0> | <1 0 1> | 255.1 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 307.0 |
YVO4 (mp-19133) | <1 1 0> | <0 1 0> | 202.4 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 61.4 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 122.8 |
GaSe (mp-1943) | <0 0 1> | <1 1 1> | 264.4 |
Al (mp-134) | <1 0 0> | <0 0 1> | 245.6 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 232.2 |
BN (mp-984) | <0 0 1> | <1 0 0> | 174.1 |
BN (mp-984) | <1 1 0> | <0 1 1> | 236.8 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 0> | 290.2 |
SiC (mp-7631) | <1 0 1> | <0 1 1> | 236.8 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 184.2 |
LiTaO3 (mp-3666) | <1 0 1> | <0 0 1> | 307.0 |
Fe3O4 (mp-19306) | <1 1 1> | <0 0 1> | 122.8 |
MgO (mp-1265) | <1 1 0> | <1 0 0> | 174.1 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 61.4 |
TiO2 (mp-2657) | <1 0 0> | <0 1 1> | 236.8 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 307.0 |
C (mp-66) | <1 1 0> | <0 0 1> | 184.2 |
GdScO3 (mp-5690) | <1 0 0> | <1 0 0> | 232.2 |
GdScO3 (mp-5690) | <1 0 1> | <1 0 0> | 58.0 |
Mg (mp-153) | <1 0 1> | <1 0 1> | 170.0 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 245.6 |
InP (mp-20351) | <1 0 0> | <1 0 0> | 174.1 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 245.6 |
TbScO3 (mp-31119) | <1 0 0> | <1 0 0> | 232.2 |
Ni (mp-23) | <1 1 0> | <1 0 0> | 174.1 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 245.6 |
MoSe2 (mp-1634) | <0 0 1> | <1 0 0> | 58.0 |
MoSe2 (mp-1634) | <1 1 0> | <0 0 1> | 184.2 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 184.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li5(NiO2)4 (mp-780518) | 0.2894 | 0.065 | 3 |
Li5(FeO2)4 (mp-780312) | 0.2311 | 0.077 | 3 |
Li12Cr5O16 (mp-764428) | 0.6255 | 0.096 | 3 |
Li5(CoO2)4 (mp-780140) | 0.2799 | 0.105 | 3 |
Li5Cr4O8 (mp-850237) | 0.2352 | 0.101 | 3 |
Li10Mn3Cr5O16 (mp-765030) | 0.2074 | 0.084 | 4 |
Li10Mn3V5O16 (mp-764265) | 0.2153 | 0.083 | 4 |
Li10V3Cr5O16 (mp-764096) | 0.1648 | 0.100 | 4 |
Li5V3CrO8 (mp-764013) | 0.2065 | 0.088 | 4 |
Li5FeNi3O8 (mp-765057) | 0.1883 | 0.073 | 4 |
Li10Fe2Co3Ni3O16 (mp-780632) | 0.2168 | 0.120 | 5 |
Li10Cr3Co2Ni3O16 (mp-778771) | 0.2338 | 0.107 | 5 |
Li10Mn2Fe3Co3O16 (mp-777706) | 0.2074 | 0.092 | 5 |
Li10Cr2Fe3Co3O16 (mp-774310) | 0.2600 | 0.811 | 5 |
Li10Mn3Cr3(NiO8)2 (mp-774408) | 0.2637 | 0.096 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eVCr: 3.7 eV Ni: 6.2 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv Cr_pv Ni_pv O |
Final Energy/Atom-5.9291 eV |
Corrected Energy-228.3850 eV
-228.3850 eV = -201.5878 eV (uncorrected energy) - 15.5606 eV (MP Advanced Correction) - 11.2366 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)