Final Magnetic Moment4.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.122 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.065 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.57 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiFe(CO3)2 + FePO4 + Li3Fe2(PO4)3 + CO2 + O2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/m [11] |
Hall-P 2yb |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 -1> | 304.3 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 -1> | 121.7 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 218.8 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 262.6 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 306.3 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 200.7 |
CeO2 (mp-20194) | <1 0 0> | <1 1 1> | 239.3 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 334.6 |
BaF2 (mp-1029) | <1 0 0> | <1 0 -1> | 121.7 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 167.3 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 218.8 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 33.5 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 234.2 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 200.7 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 217.5 |
SiO2 (mp-6930) | <1 0 1> | <1 1 1> | 319.1 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 271.8 |
KCl (mp-23193) | <1 0 0> | <1 0 -1> | 121.7 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 234.2 |
InAs (mp-20305) | <1 0 0> | <0 1 0> | 350.1 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 218.8 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 334.6 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 -1> | 243.4 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 100.4 |
Te2W (mp-22693) | <1 0 1> | <0 0 1> | 100.4 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 267.6 |
YVO4 (mp-19133) | <1 0 0> | <1 0 -1> | 182.6 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 167.3 |
TePb (mp-19717) | <1 1 0> | <1 0 -1> | 60.9 |
TePb (mp-19717) | <1 1 1> | <1 0 -1> | 304.3 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 301.1 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 267.6 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 175.0 |
GaSe (mp-1943) | <1 1 0> | <0 0 1> | 234.2 |
GaSe (mp-1943) | <1 1 1> | <0 0 1> | 234.2 |
BN (mp-984) | <0 0 1> | <1 1 0> | 279.2 |
LiNbO3 (mp-3731) | <0 0 1> | <0 1 1> | 165.3 |
LiNbO3 (mp-3731) | <1 0 0> | <0 0 1> | 301.1 |
LiNbO3 (mp-3731) | <1 0 1> | <0 0 1> | 301.1 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 0> | 306.3 |
MoS2 (mp-1434) | <1 0 1> | <1 0 0> | 271.8 |
InAs (mp-20305) | <1 1 1> | <0 1 1> | 330.5 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 167.3 |
LiGaO2 (mp-5854) | <1 0 1> | <1 1 -1> | 224.9 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 306.3 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 167.3 |
CdS (mp-672) | <1 1 1> | <1 0 -1> | 304.3 |
CdTe (mp-406) | <1 0 0> | <1 0 -1> | 182.6 |
CdTe (mp-406) | <1 1 1> | <1 0 -1> | 304.3 |
TeO2 (mp-2125) | <0 1 1> | <0 0 1> | 234.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Bi(BO2)3 (mp-23349) | 0.6787 | 0.001 | 3 |
Bi(BO2)3 (mp-1079609) | 0.6886 | 0.006 | 3 |
Zn3P2H2O9 (mp-554552) | 0.7172 | 0.009 | 4 |
Co3P2H2O9 (mp-604558) | 0.6570 | 0.012 | 4 |
LiV(PO4)2 (mp-32465) | 0.6871 | 0.032 | 4 |
Li3Ni(BO2)5 (mp-771081) | 0.7168 | 0.061 | 4 |
LiMnP2O7 (mp-31971) | 0.7254 | 0.021 | 4 |
LiFePCO7 (mp-779778) | 0.4112 | 0.068 | 5 |
Li3Fe2P2(CO7)2 (mp-770177) | 0.4007 | 0.042 | 5 |
Li3Fe2P2(CO7)2 (mp-770052) | 0.3929 | 0.045 | 5 |
LiFePCO7 (mp-779262) | 0.4077 | 0.067 | 5 |
LiFePCO7 (mp-770077) | 0.4059 | 0.067 | 5 |
KLiMnPCO7 (mp-764256) | 0.6418 | 0.000 | 6 |
NaLiMnPCO7 (mp-763833) | 0.7214 | 0.000 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv P C O |
Final Energy/Atom-6.8496 eV |
Corrected Energy-165.9895 eV
-165.9895 eV = -150.6915 eV (uncorrected energy) - 9.8321 eV (MP Anion Correction) - 5.4660 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)