Final Magnetic Moment45.174 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.210 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.007 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.69 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi24Mn11CrO36 + Li4MnCrO6 |
Band Gap0.677 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 261.3 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 174.2 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 304.9 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 304.9 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 304.9 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 217.8 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 43.6 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 217.8 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 217.8 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 217.8 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 87.1 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 304.9 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 217.8 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 130.7 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 348.4 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 291.9 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 348.4 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 87.1 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 217.8 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 304.9 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 130.7 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 261.3 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 348.4 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 348.4 |
CdS (mp-672) | <1 0 1> | <1 1 -1> | 193.0 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 87.1 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 348.4 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 261.3 |
BN (mp-984) | <0 0 1> | <0 0 1> | 43.6 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 261.3 |
BN (mp-984) | <1 0 0> | <0 0 1> | 304.9 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 291.9 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 348.4 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 304.9 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 87.1 |
Al (mp-134) | <1 1 1> | <0 0 1> | 87.1 |
BN (mp-984) | <1 0 1> | <0 1 1> | 224.4 |
BN (mp-984) | <1 1 0> | <0 0 1> | 130.7 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 43.6 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 0> | 291.9 |
Al (mp-134) | <1 0 0> | <0 0 1> | 348.4 |
Al (mp-134) | <1 1 0> | <0 0 1> | 348.4 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 217.8 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 130.7 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 304.9 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 348.4 |
TeO2 (mp-2125) | <0 1 1> | <0 0 1> | 304.9 |
TeO2 (mp-2125) | <1 0 1> | <0 0 1> | 304.9 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 261.3 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 304.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li2MnO3 (mp-565799) | 0.1402 | 0.000 | 3 |
Li17Ni11O28 (mp-767977) | 0.1450 | 0.043 | 3 |
Li2CrO3 (mp-770628) | 0.1069 | 0.025 | 3 |
Li2NiO3 (mp-691145) | 0.1226 | 0.001 | 3 |
Li7Ni5O12 (mp-773266) | 0.1238 | 0.007 | 3 |
Li24Mn7Cr5O36 (mp-770366) | 0.0318 | 0.023 | 4 |
Li32Mn13Cr3O48 (mp-779392) | 0.0312 | 0.008 | 4 |
Li32Mn13Cr3O48 (mp-779206) | 0.0251 | 0.007 | 4 |
Li32Mn13Cr3O48 (mp-779189) | 0.0363 | 0.007 | 4 |
Li32Mn13Cr3O48 (mp-778798) | 0.0340 | 0.007 | 4 |
Te2Au (mp-1662) | 0.3767 | 0.018 | 2 |
NaTe3 (mp-28478) | 0.3826 | 0.000 | 2 |
LiTe3 (mp-27466) | 0.3776 | 0.009 | 2 |
TiAs (mp-1822) | 0.4317 | 0.000 | 2 |
Te2Au (mp-567525) | 0.3895 | 0.018 | 2 |
Na6MnNi3(SbO6)2 (mp-1094109) | 0.3636 | 0.139 | 5 |
Na (mp-999501) | 0.6474 | 0.114 | 1 |
Sb (mp-632286) | 0.5357 | 0.059 | 1 |
Bi (mp-23152) | 0.6654 | 0.000 | 1 |
Te (mp-570459) | 0.5284 | 0.044 | 1 |
Te (mp-105) | 0.6157 | 0.047 | 1 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eVCr: 3.7 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv Cr_pv O |
Final Energy/Atom-6.2206 eV |
Corrected Energy-657.8315 eV
Uncorrected energy = -597.1745 eV
Composition-based energy adjustment (-0.687 eV/atom x 48.0 atoms) = -32.9760 eV
Composition-based energy adjustment (-1.668 eV/atom x 13.0 atoms) = -21.6840 eV
Composition-based energy adjustment (-1.999 eV/atom x 3.0 atoms) = -5.9970 eV
Corrected energy = -657.8315 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)