Final Magnetic Moment38.964 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.512 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.003 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.19 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiMnBO3 + Li8MnFe7(BO3)8 |
Band Gap2.975 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 1 1> | <0 0 1> | 239.3 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 275.8 |
CeO2 (mp-20194) | <1 1 1> | <0 1 1> | 215.7 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 143.6 |
LaAlO3 (mp-2920) | <1 0 0> | <0 1 0> | 275.8 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 143.6 |
LaAlO3 (mp-2920) | <1 1 0> | <0 0 1> | 239.3 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 287.3 |
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 275.8 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 239.3 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 287.1 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 335.0 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 335.0 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 239.3 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 275.8 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 165.5 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 143.6 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 287.1 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 239.3 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 143.6 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 275.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 335.0 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 275.8 |
InAs (mp-20305) | <1 1 1> | <0 1 0> | 331.0 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 335.0 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 275.8 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 220.7 |
Te2W (mp-22693) | <0 1 0> | <0 1 1> | 215.7 |
YVO4 (mp-19133) | <1 0 0> | <0 1 0> | 275.8 |
YVO4 (mp-19133) | <1 1 0> | <0 1 0> | 275.8 |
TePb (mp-19717) | <1 0 0> | <0 1 0> | 220.7 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 239.3 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 143.6 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 335.0 |
BN (mp-984) | <1 1 0> | <0 1 0> | 165.5 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 287.1 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 287.1 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 220.7 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 220.7 |
Ag (mp-124) | <1 1 1> | <0 1 0> | 220.7 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 0> | 275.8 |
Al (mp-134) | <1 0 0> | <0 0 1> | 335.0 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 143.6 |
LiGaO2 (mp-5854) | <0 1 0> | <0 1 0> | 165.5 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 1> | 215.7 |
LiGaO2 (mp-5854) | <1 1 1> | <0 0 1> | 287.1 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 0> | 331.0 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 239.3 |
BN (mp-984) | <0 0 1> | <0 0 1> | 143.6 |
BN (mp-984) | <1 0 0> | <0 1 1> | 287.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li3MnF5 (mp-763332) | 0.7098 | 0.083 | 3 |
Li3BO3 (mp-27275) | 0.6697 | 0.000 | 3 |
Na3CoO3 (mp-777919) | 0.4730 | 0.127 | 3 |
Li6B4O9 (mp-1020024) | 0.6944 | 0.000 | 3 |
Mg3WN4 (mp-1030015) | 0.7307 | 0.000 | 3 |
LiMnBO3 (mp-849500) | 0.0632 | 0.000 | 4 |
LiNiBO3 (mp-766153) | 0.2471 | 0.030 | 4 |
LiMnBO3 (mp-850971) | 0.0481 | 0.006 | 4 |
LiFeBO3 (mp-777711) | 0.1378 | 0.000 | 4 |
LiFeBO3 (mp-783910) | 0.1644 | 0.652 | 4 |
Li8Mn7Fe(BO3)8 (mp-778721) | 0.0220 | 0.003 | 5 |
Li8Mn7Fe(BO3)8 (mp-778763) | 0.0173 | 0.002 | 5 |
Li4Mn3Fe(BO3)4 (mp-850374) | 0.0270 | 0.006 | 5 |
Li8Mn7Fe(BO3)8 (mp-774189) | 0.0112 | 0.003 | 5 |
Li4Mn3Fe(BO3)4 (mp-779804) | 0.0254 | 0.005 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eVFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv Fe_pv B O |
Final Energy/Atom-7.2763 eV |
Corrected Energy-380.6153 eV
-380.6153 eV = -349.2613 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction) - 14.4990 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)