Final Magnetic Moment1.988 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.870 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.142 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.64 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToFe2O3 + Na2SO4 + CO2 + Na2CO3 |
Band Gap0.984 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFddd [70] |
HallF 2 2 1d |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
BaF2 (mp-1029) | <1 0 0> | <0 1 0> | 197.1 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 189.4 |
CdS (mp-672) | <1 1 0> | <0 1 0> | 197.1 |
Ni (mp-23) | <1 0 0> | <0 1 0> | 197.1 |
TiO2 (mp-390) | <0 0 1> | <0 0 1> | 189.4 |
MgF2 (mp-1249) | <0 0 1> | <0 1 0> | 197.1 |
ZnTe (mp-2176) | <1 0 0> | <0 0 1> | 189.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li9Cr19O48 (mp-853223) | 0.7245 | 0.063 | 3 |
Ca4GdB3O10 (mp-6943) | 0.7153 | 0.000 | 4 |
Ca5B3O9F (mp-6632) | 0.7356 | 0.000 | 4 |
Ca4SmB3O10 (mp-6388) | 0.7005 | 0.000 | 4 |
Ca4LaB3O10 (mp-6076) | 0.6999 | 0.000 | 4 |
Na4Fe2P(CO4)4 (mp-779936) | 0.0735 | 0.195 | 5 |
Na4V2C4SO16 (mp-850995) | 0.0659 | 0.029 | 5 |
Na4Co2P(CO4)4 (mp-771217) | 0.0779 | 0.117 | 5 |
Na4Cr2P(CO4)4 (mp-782637) | 0.0887 | 0.064 | 5 |
Na4Cr2C4SO16 (mp-770560) | 0.0336 | 0.083 | 5 |
Na2Li4Mn2C4SO16 (mp-765654) | 0.7330 | 0.223 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Na_pv Fe_pv C S O |
Final Energy/Atom-6.5008 eV |
Corrected Energy-385.7751 eV
-385.7751 eV = -351.0429 eV (uncorrected energy) - 23.8002 eV (MP Anion Correction) - 10.9320 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)