Final Magnetic Moment6.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.657 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.023 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.89 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi6V3P8O29 + Mn(PO3)2 + Mn2P2O7 |
Band Gap0.501 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 1> | <0 1 -1> | 194.3 |
AlN (mp-661) | <1 0 0> | <1 0 -1> | 266.9 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 267.6 |
CeO2 (mp-20194) | <1 1 1> | <0 1 -1> | 259.0 |
GaAs (mp-2534) | <1 1 1> | <1 0 0> | 242.0 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 80.7 |
GaN (mp-804) | <1 0 0> | <0 1 -1> | 323.8 |
GaN (mp-804) | <1 0 1> | <0 1 -1> | 323.8 |
GaN (mp-804) | <1 1 1> | <0 1 -1> | 323.8 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 -1> | 323.8 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 161.3 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 161.3 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 242.0 |
CdS (mp-672) | <1 1 1> | <0 1 -1> | 259.0 |
ZnSe (mp-1190) | <1 1 1> | <1 0 0> | 242.0 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 -1> | 323.8 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 267.6 |
CdS (mp-672) | <1 0 1> | <1 -1 0> | 267.3 |
LiF (mp-1138) | <1 1 0> | <0 1 -1> | 323.8 |
Te2W (mp-22693) | <0 1 1> | <0 1 1> | 117.3 |
Te2Mo (mp-602) | <1 0 1> | <0 1 -1> | 323.8 |
Ag (mp-124) | <1 1 0> | <0 1 -1> | 194.3 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 -1> | 259.0 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 242.0 |
LiNbO3 (mp-3731) | <0 0 1> | <0 1 -1> | 259.0 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 242.0 |
BN (mp-984) | <1 0 1> | <0 1 -1> | 259.0 |
MoS2 (mp-1434) | <1 0 1> | <1 1 -1> | 206.9 |
Al (mp-134) | <1 1 0> | <0 1 -1> | 323.8 |
LiGaO2 (mp-5854) | <1 0 1> | <1 -1 0> | 89.1 |
LiGaO2 (mp-5854) | <1 1 0> | <0 1 -1> | 194.3 |
CdTe (mp-406) | <1 1 1> | <1 0 0> | 80.7 |
TiO2 (mp-2657) | <1 0 0> | <1 1 0> | 237.3 |
SiC (mp-7631) | <0 0 1> | <1 0 -1> | 266.9 |
C (mp-66) | <1 0 0> | <0 0 1> | 267.6 |
LiTaO3 (mp-3666) | <0 0 1> | <0 1 -1> | 259.0 |
GdScO3 (mp-5690) | <1 0 0> | <0 1 -1> | 323.8 |
MgO (mp-1265) | <1 0 0> | <0 1 -1> | 323.8 |
Mg (mp-153) | <1 0 1> | <0 1 -1> | 323.8 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 200.7 |
TiO2 (mp-2657) | <1 1 0> | <0 1 1> | 117.3 |
TiO2 (mp-2657) | <1 1 1> | <0 1 -1> | 323.8 |
GdScO3 (mp-5690) | <0 1 1> | <1 0 0> | 161.3 |
TbScO3 (mp-31119) | <1 0 1> | <1 0 0> | 161.3 |
Ni (mp-23) | <1 1 0> | <1 0 0> | 242.0 |
InSb (mp-20012) | <1 1 1> | <1 0 0> | 80.7 |
PbS (mp-21276) | <1 1 1> | <1 0 0> | 242.0 |
BaTiO3 (mp-5986) | <1 0 1> | <0 1 -1> | 323.8 |
InP (mp-20351) | <1 1 1> | <1 0 0> | 242.0 |
TbScO3 (mp-31119) | <0 1 0> | <1 0 -1> | 89.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
V5(P3O11)2 (mp-767351) | 0.4284 | 0.020 | 3 |
Co5(P3O11)2 (mp-31617) | 0.4461 | 0.031 | 3 |
Ni5(P3O11)2 (mp-32359) | 0.3516 | 0.098 | 3 |
Mn5(P3O11)2 (mp-705036) | 0.4504 | 0.065 | 3 |
Fe5(P3O11)2 (mp-705342) | 0.4288 | 0.366 | 3 |
LiVP2O7 (mp-18911) | 0.1210 | 0.025 | 4 |
LiCrP2O7 (mp-19103) | 0.1592 | 0.075 | 4 |
LiFeP2O7 (mp-19294) | 0.1412 | 0.166 | 4 |
LiScP2O7 (mp-10517) | 0.1421 | 0.000 | 4 |
LiTiP2O7 (mp-26629) | 0.1833 | 0.055 | 4 |
Li4MnV3(P2O7)4 (mp-850462) | 0.0400 | 0.087 | 5 |
Li4MnV3(P2O7)4 (mp-778342) | 0.0447 | 0.007 | 5 |
Li2MnV(P2O7)2 (mp-781008) | 0.0358 | 0.015 | 5 |
Li2MnV(P2O7)2 (mp-779842) | 0.0363 | 0.024 | 5 |
Li4MnV3(P2O7)4 (mp-780005) | 0.0445 | 0.000 | 5 |
LiMgCr3Se2(SO6)4 (mp-769552) | 0.5875 | 0.257 | 6 |
Li2MgCr3Se3(SO8)3 (mp-773983) | 0.5075 | 0.331 | 6 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.5493 | 0.068 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eVV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv V_pv P O |
Final Energy/Atom-7.1933 eV |
Corrected Energy-342.8936 eV
-342.8936 eV = -316.5038 eV (uncorrected energy) - 19.6641 eV (MP Anion Correction) - 6.7257 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)