Final Magnetic Moment0.057 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.912 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.167 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.03 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToV2O3 + LiF + LiV3(OF3)2 |
Band Gap0.058 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 252.7 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 140.4 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 308.9 |
LaAlO3 (mp-2920) | <1 1 0> | <0 0 1> | 252.7 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 84.2 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 112.3 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 252.1 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 28.1 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 87.4 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 337.0 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 84.2 |
CeO2 (mp-20194) | <1 1 1> | <1 1 1> | 256.8 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 262.1 |
BaF2 (mp-1029) | <1 1 0> | <0 1 1> | 278.4 |
BaF2 (mp-1029) | <1 1 1> | <0 1 1> | 278.4 |
BN (mp-984) | <0 0 1> | <0 0 1> | 168.5 |
BN (mp-984) | <1 0 1> | <0 0 1> | 84.2 |
LiNbO3 (mp-3731) | <0 0 1> | <0 1 1> | 92.8 |
LiNbO3 (mp-3731) | <1 0 0> | <0 0 1> | 224.6 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 224.6 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 28.1 |
LiGaO2 (mp-5854) | <1 1 0> | <1 1 0> | 244.0 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 224.6 |
TeO2 (mp-2125) | <0 1 0> | <0 0 1> | 196.6 |
TeO2 (mp-2125) | <0 1 1> | <0 0 1> | 224.6 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 84.2 |
SiC (mp-7631) | <1 0 0> | <0 0 1> | 337.0 |
SiC (mp-7631) | <1 0 1> | <0 0 1> | 337.0 |
SiC (mp-7631) | <1 1 0> | <0 0 1> | 84.2 |
LiTaO3 (mp-3666) | <0 0 1> | <0 1 1> | 92.8 |
LiTaO3 (mp-3666) | <1 0 0> | <0 0 1> | 140.4 |
LiTaO3 (mp-3666) | <1 0 1> | <0 0 1> | 308.9 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 365.0 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 224.6 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 308.9 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 262.1 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 196.6 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 308.9 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 308.9 |
Ge3(BiO3)4 (mp-23560) | <1 1 0> | <0 0 1> | 168.5 |
C (mp-66) | <1 0 0> | <0 0 1> | 308.9 |
C (mp-66) | <1 1 0> | <0 0 1> | 56.2 |
C (mp-66) | <1 1 1> | <0 0 1> | 308.9 |
GdScO3 (mp-5690) | <0 0 1> | <0 0 1> | 224.6 |
GdScO3 (mp-5690) | <0 1 0> | <0 0 1> | 224.6 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 0> | 262.1 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 140.4 |
Mg (mp-153) | <1 0 0> | <0 1 0> | 84.0 |
Mg (mp-153) | <1 0 1> | <1 1 -1> | 243.9 |
Mg (mp-153) | <1 1 0> | <0 0 1> | 28.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li3Cu2F8 (mp-753199) | 0.5760 | 0.056 | 3 |
Li3TiF6 (mp-21540) | 0.5818 | 0.000 | 3 |
Li3FeF6 (mp-776684) | 0.5731 | 0.178 | 3 |
Fe7(OF3)3 (mp-781010) | 0.5752 | 0.087 | 3 |
Li3AlF6 (mp-556020) | 0.5753 | 0.006 | 3 |
Li11V6O5F19 (mp-850254) | 0.2986 | 0.058 | 4 |
Li3V4(OF3)3 (mp-779400) | 0.3597 | 0.094 | 4 |
Li11V6O5F19 (mp-780480) | 0.3932 | 0.068 | 4 |
Li3V4(OF3)3 (mp-779062) | 0.4267 | 0.178 | 4 |
Li11V6O5F19 (mp-777941) | 0.3464 | 0.075 | 4 |
V5O9 (mp-714932) | 0.6490 | 0.017 | 2 |
Ti6O11 (mp-559964) | 0.7089 | 0.008 | 2 |
V7O13 (mp-715598) | 0.7057 | 0.143 | 2 |
Ti4O7 (mp-558097) | 0.7203 | 0.005 | 2 |
V5O9 (mp-704305) | 0.6928 | 0.008 | 2 |
Li4MnNb2WO12 (mp-771475) | 0.6630 | 0.046 | 5 |
Li4MnSb(WO6)2 (mp-779994) | 0.6379 | 0.041 | 5 |
Li4SbTe2WO12 (mp-765930) | 0.6070 | 0.086 | 5 |
Li4VTe(WO6)2 (mp-778316) | 0.6603 | 0.056 | 5 |
Li7Zr3Nb(TeO6)4 (mp-695434) | 0.6360 | 0.018 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv V_pv O F |
Final Energy/Atom-5.6833 eV |
Corrected Energy-246.6184 eV