material

Na3CuO2

ID:

mp-779545

DOI:

10.17188/1306427


Material Details

Final Magnetic Moment
-0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
Non-magnetic
Formation Energy / Atom
-1.332 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.040 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.04 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Na3CuO2
Band Gap
1.722 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
R3c [167]
Hall
-R 3 2"c
Point Group
3m
Crystal System
trigonal

Band Structure

Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.000 274.5
C (mp-48) <0 0 1> <0 0 1> 0.000 274.5
BaF2 (mp-1029) <1 1 1> <0 0 1> 0.003 274.5
SiC (mp-11714) <0 0 1> <0 0 1> 0.003 156.9
GaP (mp-2490) <1 1 1> <0 0 1> 0.003 156.9
WS2 (mp-224) <0 0 1> <0 0 1> 0.004 274.5
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.004 274.5
SiC (mp-7631) <0 0 1> <0 0 1> 0.004 156.9
MoSe2 (mp-1634) <0 0 1> <0 0 1> 0.004 353.0
WSe2 (mp-1821) <0 0 1> <0 0 1> 0.005 353.0
CaF2 (mp-2741) <1 1 1> <0 0 1> 0.012 156.9
Mg (mp-153) <0 0 1> <0 0 1> 0.015 274.5
Si (mp-149) <1 1 1> <0 0 1> 0.017 156.9
CeO2 (mp-20194) <1 1 1> <0 0 1> 0.019 156.9
GaN (mp-804) <0 0 1> <0 0 1> 0.020 117.7
Cu (mp-30) <1 1 1> <0 0 1> 0.022 156.9
Ag (mp-124) <1 0 0> <0 0 1> 0.025 274.5
C (mp-66) <1 1 1> <0 0 1> 0.030 156.9
CaCO3 (mp-3953) <0 0 1> <0 0 1> 0.035 156.9
Ag (mp-124) <1 1 0> <0 0 1> 0.039 196.1
Au (mp-81) <1 1 0> <0 0 1> 0.042 196.1
WSe2 (mp-1821) <1 0 0> <1 0 1> 0.043 100.6
Au (mp-81) <1 0 0> <0 0 1> 0.048 274.5
MgF2 (mp-1249) <1 1 1> <0 0 1> 0.048 274.5
MgAl2O4 (mp-3536) <1 1 1> <0 0 1> 0.057 117.7
TeO2 (mp-2125) <0 0 1> <0 0 1> 0.058 196.1
ZnO (mp-2133) <0 0 1> <0 0 1> 0.061 353.0
LiF (mp-1138) <1 1 1> <0 0 1> 0.063 117.7
Te2Mo (mp-602) <1 0 1> <0 0 1> 0.064 274.5
Ag (mp-124) <1 1 1> <0 0 1> 0.071 117.7
InSb (mp-20012) <1 0 0> <0 0 1> 0.073 313.7
Fe2O3 (mp-24972) <0 0 1> <0 0 1> 0.076 156.9
Bi2Te3 (mp-34202) <0 0 1> <0 0 1> 0.077 117.7
CdTe (mp-406) <1 0 0> <0 0 1> 0.082 313.7
PbSe (mp-2201) <1 1 1> <0 0 1> 0.088 274.5
DyScO3 (mp-31120) <1 0 0> <0 0 1> 0.094 274.5
TbScO3 (mp-31119) <1 0 0> <0 0 1> 0.097 274.5
BaTiO3 (mp-5986) <1 0 1> <0 0 1> 0.102 274.5
MgF2 (mp-1249) <1 1 0> <1 0 0> 0.102 185.2
TiO2 (mp-2657) <1 0 0> <0 0 1> 0.103 274.5
GdScO3 (mp-5690) <0 0 1> <0 0 1> 0.108 196.1
ZrO2 (mp-2858) <0 1 0> <0 0 1> 0.108 313.7
GaSb (mp-1156) <1 1 1> <0 0 1> 0.110 274.5
Au (mp-81) <1 1 1> <0 0 1> 0.116 117.7
CdS (mp-672) <1 0 0> <1 0 1> 0.119 201.2
GdScO3 (mp-5690) <1 0 0> <0 0 1> 0.128 274.5
CdSe (mp-2691) <1 1 1> <0 0 1> 0.128 274.5
TiO2 (mp-2657) <1 1 0> <1 0 0> 0.130 277.8
SiO2 (mp-6930) <0 0 1> <0 0 1> 0.132 156.9
Al (mp-134) <1 0 0> <0 0 1> 0.137 196.1
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
61 21 28 9 0 0
21 61 28 -9 0 0
28 28 141 -0 0 0
9 -9 -0 14 0 0
0 0 0 0 14 9
0 0 0 0 9 20
Compliance Tensor Sij (10-12Pa-1)
26.2 -12 -2.8 -26.4 0 0
-12 26.2 -2.8 26.4 0 0
-2.8 -2.8 8.3 0 0 0
-26.4 26.4 0 109.6 0 0
0 0 0 0 109.6 -52.8
0 0 0 0 -52.8 76.4
Shear Modulus GV
22 GPa
Bulk Modulus KV
46 GPa
Shear Modulus GR
12 GPa
Bulk Modulus KR
40 GPa
Shear Modulus GVRH
17 GPa
Bulk Modulus KVRH
43 GPa
Elastic Anisotropy
3.83
Poisson's Ratio
0.32

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Na3AuS2 (mp-15567) 0.6067 0.000 3
K3AuSe2 (mp-15571) 0.4597 0.000 3
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Na_pv Cu_pv O
Final Energy/Atom
-4.0827 eV
Corrected Energy
-51.8016 eV
-51.8016 eV = -48.9924 eV (uncorrected energy) - 2.8092 eV (MP Anion Correction)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)