Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.758 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.12 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap2.140 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPbcm [57] |
Hall-P 2c 2b |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 0 1> | 298.6 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 268.7 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 223.9 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 223.9 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 89.6 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 116.6 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 268.7 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 223.9 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 268.7 |
Te2W (mp-22693) | <0 1 1> | <0 1 0> | 179.1 |
Te2W (mp-22693) | <1 1 0> | <0 0 1> | 223.9 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 223.9 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 298.6 |
LiNbO3 (mp-3731) | <1 0 0> | <0 0 1> | 74.6 |
BN (mp-984) | <0 0 1> | <0 0 1> | 223.9 |
BN (mp-984) | <1 1 0> | <0 1 0> | 268.7 |
BN (mp-984) | <1 1 1> | <0 1 0> | 268.7 |
SiC (mp-7631) | <0 0 1> | <0 1 1> | 116.6 |
LiTaO3 (mp-3666) | <1 0 0> | <0 0 1> | 74.6 |
MgO (mp-1265) | <1 1 0> | <0 1 1> | 233.2 |
Mg (mp-153) | <1 0 0> | <0 1 1> | 116.6 |
Mg (mp-153) | <1 0 1> | <0 1 0> | 268.7 |
Mg (mp-153) | <1 1 0> | <0 1 1> | 116.6 |
BaTiO3 (mp-5986) | <1 0 0> | <0 1 0> | 268.7 |
NdGaO3 (mp-3196) | <1 1 1> | <0 1 0> | 268.7 |
SiC (mp-11714) | <0 0 1> | <0 1 1> | 116.6 |
SiC (mp-11714) | <1 0 1> | <0 0 1> | 298.6 |
SiC (mp-11714) | <1 1 0> | <0 1 0> | 268.7 |
MoSe2 (mp-1634) | <1 0 0> | <0 1 0> | 268.7 |
WS2 (mp-224) | <1 0 0> | <0 0 1> | 223.9 |
C (mp-48) | <1 0 0> | <0 1 0> | 268.7 |
C (mp-48) | <1 1 0> | <0 1 0> | 268.7 |
C (mp-48) | <1 1 1> | <0 1 0> | 268.7 |
CdWO4 (mp-19387) | <1 0 0> | <0 0 1> | 223.9 |
NaCl (mp-22862) | <1 1 1> | <0 0 1> | 223.9 |
TiO2 (mp-390) | <0 0 1> | <0 1 1> | 116.6 |
ZnO (mp-2133) | <1 1 0> | <0 1 0> | 89.6 |
ZrO2 (mp-2858) | <0 0 1> | <0 0 1> | 223.9 |
ZrO2 (mp-2858) | <0 1 0> | <0 0 1> | 298.6 |
ZrO2 (mp-2858) | <1 0 -1> | <0 1 0> | 179.1 |
ZrO2 (mp-2858) | <1 0 0> | <0 1 1> | 116.6 |
ZrO2 (mp-2858) | <1 0 1> | <0 0 1> | 298.6 |
Ge(Bi3O5)4 (mp-23352) | <1 1 0> | <0 0 1> | 149.3 |
GaTe (mp-542812) | <1 0 0> | <0 0 1> | 298.6 |
Ge (mp-32) | <1 1 1> | <0 0 1> | 223.9 |
LiAlO2 (mp-3427) | <0 0 1> | <0 0 1> | 223.9 |
YAlO3 (mp-3792) | <0 0 1> | <0 0 1> | 223.9 |
YAlO3 (mp-3792) | <0 1 0> | <0 1 1> | 116.6 |
YAlO3 (mp-3792) | <0 1 1> | <0 0 1> | 149.3 |
SiC (mp-8062) | <1 1 0> | <0 0 1> | 298.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
MnPO4 (mp-540022) | 0.7050 | 0.318 | 3 |
Zn2P2O7 (mp-559319) | 0.3144 | 0.000 | 3 |
NaPO3 (mp-555118) | 0.7355 | 0.000 | 3 |
Li2S2O7 (mp-1020013) | 0.5410 | 0.000 | 3 |
MnPO4 (mp-694537) | 0.7113 | 0.318 | 3 |
LiCoP2O7 (mp-705301) | 0.4471 | 0.155 | 4 |
LiCrP2O7 (mp-705361) | 0.4221 | 0.190 | 4 |
Li2MnP2O7 (mp-31959) | 0.4439 | 0.025 | 4 |
LiFeP2O7 (mp-695816) | 0.4435 | 0.060 | 4 |
LiMnP2O7 (mp-697744) | 0.4569 | 0.212 | 4 |
P3N5 (mp-1954) | 0.6782 | 0.099 | 2 |
BaZn2As3HO11 (mp-758313) | 0.6370 | 0.007 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Zn As O |
Final Energy/Atom-5.5357 eV |
Corrected Energy-526.4709 eV
-526.4709 eV = -487.1427 eV (uncorrected energy) - 39.3282 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)