Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.143 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.079 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.63 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNa2VPCO7 + V2O3 + CO2 + Na2CO3 |
Band Gap0.008 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFdd2 [43] |
HallF 2 2d |
Point Groupmm2 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 195.7 |
CdS (mp-672) | <1 1 0> | <0 1 0> | 197.7 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 195.7 |
Ni (mp-23) | <1 0 0> | <0 1 0> | 197.7 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 195.7 |
CdSe (mp-2691) | <1 0 0> | <0 0 1> | 195.7 |
MgF2 (mp-1249) | <0 0 1> | <0 1 0> | 197.7 |
GaSb (mp-1156) | <1 0 0> | <0 0 1> | 195.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li9Cr19O48 (mp-851274) | 0.7481 | 0.074 | 3 |
Ca4GdB3O10 (mp-6943) | 0.7195 | 0.000 | 4 |
Li9V12Fe7O48 (mp-850893) | 0.7411 | 0.064 | 4 |
Ca4SmB3O10 (mp-6388) | 0.7161 | 0.000 | 4 |
Ca4LaB3O10 (mp-6076) | 0.7376 | 0.000 | 4 |
Li9Mn7V12O48 (mp-851270) | 0.7365 | 0.059 | 4 |
Na5Cr2P(CO4)4 (mp-777120) | 0.1226 | 0.135 | 5 |
Na5Mn2P(CO4)4 (mp-776863) | 0.2011 | 0.206 | 5 |
Na5Co2P(CO4)4 (mp-771779) | 0.2361 | 0.100 | 5 |
Na5Cr2P(CO4)4 (mp-778332) | 0.0586 | 0.136 | 5 |
Li9Cr4C8(SO16)2 (mp-776706) | 0.2283 | 0.075 | 5 |
Na2Li4Co2C4SO16 (mp-765657) | 0.5344 | 0.166 | 6 |
Na2Li4Ni2C4SO16 (mp-765655) | 0.5406 | 0.097 | 6 |
Na2Li4Mn2C4SO16 (mp-765654) | 0.4834 | 0.223 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Na_pv V_pv P C O |
Final Energy/Atom-6.8443 eV |
Corrected Energy-412.4812 eV
-412.4812 eV = -383.2799 eV (uncorrected energy) - 22.4733 eV (MP Anion Correction) - 6.7280 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)