Final Magnetic Moment0.016 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-2.605 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.173 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.85 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiVPO5 + Li6V3P8O29 + LiMnPO4 + Li3PO4 |
Band Gap1.505 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 1 1> | 160.4 |
AlN (mp-661) | <1 0 1> | <0 1 -1> | 142.4 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 292.1 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 291.1 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 194.1 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 1> | 264.9 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 1> | 134.9 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 194.1 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 291.1 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 291.1 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 97.4 |
Ag (mp-124) | <1 1 0> | <0 1 1> | 264.9 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 292.1 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 0> | 292.3 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 291.1 |
TiO2 (mp-2657) | <1 0 0> | <0 1 1> | 264.9 |
C (mp-66) | <1 1 0> | <0 0 1> | 291.1 |
GdScO3 (mp-5690) | <0 1 0> | <1 0 1> | 134.9 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 194.1 |
GdScO3 (mp-5690) | <0 1 1> | <0 1 1> | 264.9 |
GdScO3 (mp-5690) | <1 0 0> | <1 1 0> | 135.6 |
TbScO3 (mp-31119) | <0 1 0> | <1 0 1> | 134.9 |
TbScO3 (mp-31119) | <1 0 0> | <1 0 1> | 134.9 |
GaP (mp-2490) | <1 1 1> | <1 1 1> | 160.4 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 291.1 |
NdGaO3 (mp-3196) | <0 1 1> | <0 1 1> | 264.9 |
TbScO3 (mp-31119) | <0 1 1> | <0 1 1> | 264.9 |
SiC (mp-11714) | <0 0 1> | <0 0 1> | 291.1 |
MoSe2 (mp-1634) | <1 0 1> | <0 1 1> | 264.9 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 194.1 |
BaTiO3 (mp-5986) | <1 1 1> | <0 0 1> | 291.1 |
NdGaO3 (mp-3196) | <1 0 0> | <0 1 1> | 132.5 |
SiC (mp-11714) | <1 1 0> | <0 1 1> | 264.9 |
CdSe (mp-2691) | <1 0 0> | <0 0 1> | 194.1 |
NaCl (mp-22862) | <1 1 1> | <0 0 1> | 291.1 |
ZrO2 (mp-2858) | <1 0 -1> | <0 0 1> | 291.1 |
TiO2 (mp-390) | <1 0 0> | <0 1 1> | 264.9 |
TiO2 (mp-390) | <1 1 0> | <0 1 1> | 264.9 |
CsI (mp-614603) | <1 1 0> | <0 1 1> | 264.9 |
MgF2 (mp-1249) | <0 0 1> | <0 1 0> | 194.9 |
MgF2 (mp-1249) | <1 1 0> | <1 0 0> | 292.1 |
ZnO (mp-2133) | <1 0 0> | <0 1 1> | 264.9 |
Cu (mp-30) | <1 1 0> | <0 0 1> | 291.1 |
Ge (mp-32) | <1 1 1> | <0 0 1> | 291.1 |
Al2O3 (mp-1143) | <1 0 0> | <1 0 0> | 194.7 |
CaF2 (mp-2741) | <1 1 0> | <0 1 1> | 132.5 |
CaF2 (mp-2741) | <1 1 1> | <1 1 1> | 160.4 |
Fe2O3 (mp-24972) | <0 0 1> | <1 1 1> | 160.4 |
GaSb (mp-1156) | <1 0 0> | <0 0 1> | 194.1 |
SrTiO3 (mp-4651) | <1 0 0> | <0 1 1> | 132.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
FeSiO3 (mp-630331) | 0.6237 | 0.038 | 3 |
Li2Ge7O15 (mp-5832) | 0.6127 | 0.028 | 3 |
Ni5(P3O11)2 (mp-32359) | 0.6016 | 0.098 | 3 |
Ni7(PO4)6 (mp-32385) | 0.5981 | 0.102 | 3 |
Fe5(P3O11)2 (mp-705342) | 0.6185 | 0.366 | 3 |
Li3Ni2(PO4)3 (mp-705397) | 0.4754 | 0.099 | 4 |
Li3Ni2(PO4)3 (mp-504139) | 0.4276 | 0.242 | 4 |
Li3Cr2(PO4)3 (mp-31681) | 0.4037 | 0.042 | 4 |
LiNiP2O7 (mp-32396) | 0.4604 | 0.082 | 4 |
ZnMoAsO5 (mvc-5904) | 0.4221 | 0.096 | 4 |
CrO2 (mvc-11581) | 0.7461 | 0.351 | 2 |
VO2 (mp-777469) | 0.7397 | 0.038 | 2 |
VO2 (mvc-6918) | 0.7261 | 0.095 | 2 |
MoO2 (mvc-6944) | 0.7152 | 0.387 | 2 |
Li6MnV3(PO4)6 (mp-764655) | 0.2714 | 0.098 | 5 |
Li3MnV(PO4)3 (mp-774954) | 0.4389 | 0.241 | 5 |
Li3MnV(PO4)3 (mp-774311) | 0.5188 | 0.208 | 5 |
K4Li5Ti8(PO5)8 (mp-766028) | 0.5541 | 0.041 | 5 |
Li3MnV(PO4)3 (mp-779860) | 0.1560 | 0.272 | 5 |
Li4TiNi3Sn2(PO4)6 (mp-778249) | 0.6406 | 0.173 | 6 |
NaLi5Ti3Cr3(PO4)9 (mp-744549) | 0.7047 | 0.059 | 6 |
LiMgCr3Se2(SO6)4 (mp-769552) | 0.6558 | 0.003 | 6 |
Li2MgCr3Se3(SO8)3 (mp-773983) | 0.5360 | 0.041 | 6 |
Mn4Si4SnB2(HO9)2 (mp-743890) | 0.6275 | 0.000 | 6 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.5905 | 0.068 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eVV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv V_pv P O |
Final Energy/Atom-6.9018 eV |
Corrected Energy-599.3069 eV
-599.3069 eV = -552.1455 eV (uncorrected energy) - 33.7099 eV (MP Anion Correction) - 13.4514 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)