Final Magnetic Moment0.964 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.974 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.067 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.47 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNaCO3 + Bi2CO5 + Na2BiPCO7 + CO2 + Na2CO3 |
Band Gap0.070 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFddd [70] |
HallF 2 2 1d |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li9Cr19O48 (mp-853223) | 0.7426 | 0.063 | 3 |
Ca4GdB3O10 (mp-6943) | 0.6279 | 0.000 | 4 |
Ca5B3O9F (mp-6632) | 0.6629 | 0.000 | 4 |
Ca4SmB3O10 (mp-6388) | 0.6105 | 0.000 | 4 |
Ca4LaB3O10 (mp-6076) | 0.6049 | 0.000 | 4 |
Li9Mn7Cr12O48 (mp-853217) | 0.7458 | 0.257 | 4 |
Na4Sn2C4SO16 (mp-775782) | 0.1034 | 0.094 | 5 |
Na4Bi2C4SO16 (mp-779515) | 0.0454 | 0.025 | 5 |
Na4Sb2C4SO16 (mp-768959) | 0.0883 | 0.060 | 5 |
Na4Bi2B4SO16 (mp-779161) | 0.1865 | 0.068 | 5 |
Li4Cu2C4SO16 (mp-776330) | 0.2087 | 0.100 | 5 |
Na2Li4Mn2C4SO16 (mp-765654) | 0.7008 | 0.254 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Na_pv Bi P C O |
Final Energy/Atom-6.5400 eV |
Corrected Energy-375.1441 eV
Uncorrected energy = -353.1601 eV
Composition-based energy adjustment (-0.687 eV/atom x 32.0 atoms) = -21.9840 eV
Corrected energy = -375.1441 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)