Final Magnetic Moment1.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.424 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.054 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.96 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi6V3P8O29 + VPO5 + VP2O7 + PH3O4 |
Band Gap1.024 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21 [4] |
HallP 2yb |
Point Group2 |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 1 1> | 272.1 |
CeO2 (mp-20194) | <1 1 1> | <1 0 1> | 107.6 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 231.5 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 231.5 |
BaF2 (mp-1029) | <1 1 0> | <1 0 -1> | 168.6 |
BaF2 (mp-1029) | <1 1 1> | <1 0 1> | 215.2 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 -1> | 84.3 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 -1> | 252.8 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 1> | 215.2 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 232.7 |
AlN (mp-661) | <1 0 1> | <0 1 1> | 90.7 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 139.1 |
CeO2 (mp-20194) | <1 1 0> | <1 0 -1> | 84.3 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 154.4 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 207.8 |
KCl (mp-23193) | <1 1 1> | <1 0 1> | 215.2 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 231.5 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 231.5 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 231.5 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 231.5 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 231.5 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 308.7 |
CdS (mp-672) | <1 0 1> | <1 0 -1> | 168.6 |
CdS (mp-672) | <1 1 1> | <0 1 0> | 208.7 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 231.5 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 231.5 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 290.9 |
Te2W (mp-22693) | <0 1 0> | <1 0 -1> | 168.6 |
Te2W (mp-22693) | <1 0 0> | <1 0 0> | 308.7 |
Te2W (mp-22693) | <1 1 0> | <0 0 1> | 116.4 |
YVO4 (mp-19133) | <0 0 1> | <0 1 0> | 208.7 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 232.7 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 290.9 |
TePb (mp-19717) | <1 1 1> | <1 0 1> | 215.2 |
LiTaO3 (mp-3666) | <0 0 1> | <1 0 1> | 215.2 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 232.7 |
Te2Mo (mp-602) | <1 0 0> | <1 0 -1> | 168.6 |
Te2Mo (mp-602) | <1 0 1> | <0 1 1> | 272.1 |
Ag (mp-124) | <1 1 0> | <1 1 -1> | 218.6 |
MgO (mp-1265) | <1 1 0> | <0 1 1> | 181.4 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 154.4 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 174.6 |
Ag (mp-124) | <1 1 1> | <1 0 1> | 215.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 174.6 |
C (mp-66) | <1 0 0> | <1 0 -1> | 252.8 |
C (mp-66) | <1 1 0> | <0 0 1> | 290.9 |
GdScO3 (mp-5690) | <0 1 0> | <0 0 1> | 174.6 |
GdScO3 (mp-5690) | <1 0 1> | <1 0 0> | 231.5 |
Mg (mp-153) | <1 0 0> | <1 1 -1> | 218.6 |
Mg (mp-153) | <1 0 1> | <1 1 0> | 207.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mn4P7O24 (mp-540414) | 0.5505 | 0.016 | 3 |
Fe5(P3O11)2 (mp-31872) | 0.5884 | 0.038 | 3 |
V4As2O13 (mp-32447) | 0.5988 | 0.004 | 3 |
V4P2O13 (mp-768034) | 0.5162 | 0.019 | 3 |
Mn5(P3O11)2 (mp-31954) | 0.5670 | 0.028 | 3 |
Li3Fe4(PO4)6 (mp-767797) | 0.5816 | 0.063 | 4 |
LiCr2(PO4)3 (mp-697757) | 0.5835 | 0.047 | 4 |
Li3Cr4(PO4)6 (mp-868663) | 0.5522 | 0.047 | 4 |
LiV(PO4)2 (mp-32422) | 0.5577 | 0.108 | 4 |
Li3V4(PO4)6 (mp-767872) | 0.5761 | 0.018 | 4 |
LiV2P4(HO8)2 (mp-850766) | 0.1636 | 0.054 | 5 |
LiV2P4(HO8)2 (mp-850229) | 0.1165 | 0.059 | 5 |
LiV2P4(HO8)2 (mp-779938) | 0.1062 | 0.056 | 5 |
LiV2P4(HO8)2 (mp-777090) | 0.1449 | 0.054 | 5 |
LiV2P4(HO8)2 (mp-781070) | 0.0931 | 0.055 | 5 |
LiVFeP2(O4F)2 (mp-777635) | 0.6110 | 0.028 | 6 |
LiVCrP2(O4F)2 (mp-868574) | 0.6193 | 0.006 | 6 |
LiVCrP2(O4F)2 (mp-765305) | 0.6314 | 0.008 | 6 |
LiVCrP2(O4F)2 (mp-765118) | 0.6256 | 0.007 | 6 |
LiVCrP2(O4F)2 (mp-765173) | 0.6289 | 0.007 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv V_pv P H O |
Final Energy/Atom-6.9346 eV |
Corrected Energy-375.9296 eV
-375.9296 eV = -346.7283 eV (uncorrected energy) - 22.4733 eV (MP Anion Correction) - 6.7280 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)