Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-2.113 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.173 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.49 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToVHO2 + LiVPHO5 + V4P3 + Li3PO4 + H2O |
Band Gap2.086 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPca21 [29] |
HallP 2c 2ac |
Point Groupmm2 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 276.8 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 332.1 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 166.1 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 276.8 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 0> | 194.8 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 257.9 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 276.8 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 171.9 |
Te2W (mp-22693) | <0 1 1> | <0 1 0> | 171.9 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 102.2 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 86.0 |
BN (mp-984) | <1 0 0> | <0 0 1> | 332.1 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 276.8 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 276.8 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 276.8 |
LiNbO3 (mp-3731) | <1 0 0> | <0 0 1> | 221.4 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 276.8 |
Al (mp-134) | <1 1 0> | <0 0 1> | 276.8 |
YVO4 (mp-19133) | <1 1 0> | <0 1 1> | 204.5 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 276.8 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 0> | 86.0 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 0> | 86.0 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 194.8 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 332.1 |
BN (mp-984) | <0 0 1> | <0 1 0> | 257.9 |
BN (mp-984) | <1 0 1> | <0 0 1> | 332.1 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 276.8 |
Al (mp-134) | <1 0 0> | <1 1 0> | 194.8 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 166.1 |
TeO2 (mp-2125) | <0 0 1> | <1 1 0> | 194.8 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 166.1 |
SiC (mp-7631) | <1 0 0> | <0 0 1> | 332.1 |
SiC (mp-7631) | <1 1 0> | <0 0 1> | 166.1 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 276.8 |
LiTaO3 (mp-3666) | <1 0 0> | <0 0 1> | 221.4 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 221.4 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 110.7 |
Mg (mp-153) | <1 1 0> | <0 1 0> | 86.0 |
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <0 0 1> | 110.7 |
C (mp-66) | <1 0 0> | <0 1 0> | 257.9 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 276.8 |
TbScO3 (mp-31119) | <1 0 0> | <0 0 1> | 276.8 |
TbScO3 (mp-31119) | <1 1 0> | <0 1 0> | 257.9 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 332.1 |
GdScO3 (mp-5690) | <1 0 0> | <0 0 1> | 276.8 |
GdScO3 (mp-5690) | <1 1 0> | <0 1 0> | 257.9 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 166.1 |
KP(HO2)2 (mp-23959) | <0 0 1> | <0 0 1> | 221.4 |
KP(HO2)2 (mp-23959) | <0 1 0> | <0 0 1> | 221.4 |
KP(HO2)2 (mp-23959) | <1 0 0> | <0 0 1> | 110.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Sn8P2O13 (mp-767039) | 0.7243 | 0.025 | 3 |
Li2CrO4 (mp-773996) | 0.7448 | 0.088 | 3 |
V3(H3O5)2 (mp-627291) | 0.6565 | 0.071 | 3 |
Na2Si3(HO4)2 (mp-698025) | 0.6826 | 0.003 | 4 |
AsH18N3O7 (mp-720294) | 0.6825 | 0.000 | 4 |
CrP(HO)5 (mp-541142) | 0.6925 | 0.120 | 4 |
Li2Cr(H2O3)2 (mp-541476) | 0.6043 | 0.019 | 4 |
CuP(HO)5 (mp-505785) | 0.6916 | 0.174 | 4 |
CuPH6NO5 (mp-733866) | 0.4673 | 0.041 | 5 |
LiFePH2O5 (mp-780200) | 0.5375 | 0.332 | 5 |
CuPH4O5F (mp-721471) | 0.5655 | 0.000 | 5 |
LiCrPH2O5 (mp-850156) | 0.4562 | 0.237 | 5 |
LiCrPH2O5 (mp-781961) | 0.5503 | 0.253 | 5 |
MnP3H10C3NO9 (mp-743546) | 0.7238 | 0.113 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv V_pv P H O |
Final Energy/Atom-6.3557 eV |
Corrected Energy-550.0045 eV
-550.0045 eV = -508.4569 eV (uncorrected energy) - 28.0916 eV (MP Anion Correction) - 13.4560 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)