Final Magnetic Moment31.010 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.967 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.967 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.35 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToFe2O3 + Cr2O3 + Li4CrFe3O8 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2 [5] |
HallC 2y |
Point Group2 |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <0 0 1> | 138.6 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 201.4 |
AlN (mp-661) | <1 0 1> | <0 1 1> | 273.3 |
AlN (mp-661) | <1 1 1> | <1 0 -1> | 280.3 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 231.0 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 184.8 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 231.0 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 138.6 |
GaN (mp-804) | <1 0 1> | <0 1 1> | 136.7 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 138.6 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 138.6 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 201.4 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 323.4 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 231.0 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 138.6 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 277.2 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 251.8 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 272.0 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 1> | 218.9 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 231.0 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 323.4 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 201.4 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 0> | 251.8 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 323.4 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 100.7 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 251.8 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 323.4 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 151.1 |
YVO4 (mp-19133) | <1 1 1> | <0 1 0> | 251.8 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 181.3 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 277.2 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 277.2 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 323.4 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 92.4 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 138.6 |
BN (mp-984) | <0 0 1> | <0 1 0> | 251.8 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 46.2 |
BN (mp-984) | <1 0 0> | <0 0 1> | 231.0 |
BN (mp-984) | <1 0 1> | <0 1 1> | 205.0 |
Al (mp-134) | <1 1 1> | <0 1 0> | 251.8 |
Al (mp-134) | <1 0 0> | <0 0 1> | 323.4 |
TeO2 (mp-2125) | <0 1 0> | <0 1 0> | 201.4 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 138.6 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 231.0 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 0> | 251.8 |
LiGaO2 (mp-5854) | <1 1 1> | <1 0 -1> | 280.3 |
LiTaO3 (mp-3666) | <1 0 0> | <0 0 1> | 138.6 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 46.2 |
MgO (mp-1265) | <1 0 0> | <0 1 0> | 251.8 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 323.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li5Fe5O12 (mp-762602) | 0.1428 | 0.695 | 3 |
Li5Cr5O12 (mp-762528) | 0.1632 | 0.103 | 3 |
Li3V7O12 (mp-762285) | 0.1708 | 0.078 | 3 |
Li5V5O12 (mp-762939) | 0.1597 | 0.156 | 3 |
Li2Fe(NiO3)2 (mp-762917) | 0.1796 | 0.164 | 4 |
Li3Fe5(CoO6)2 (mp-773618) | 0.1737 | 0.130 | 4 |
Li3Mn5Cr2O12 (mp-850947) | 0.1438 | 0.084 | 4 |
Li3Mn2Ni5O12 (mp-762611) | 0.1168 | 0.061 | 4 |
Li3Mn5(NiO6)2 (mp-762753) | 0.1768 | 0.099 | 4 |
Ni6O7 (mp-767815) | 0.3007 | 0.047 | 2 |
Ni5O6 (mp-782702) | 0.2813 | 0.041 | 2 |
V6C5 (mp-28731) | 0.3110 | 0.000 | 2 |
Fe7O8 (mp-715333) | 0.3571 | 0.064 | 2 |
Ni6Cl7 (mp-1022720) | 0.3086 | 0.376 | 2 |
Li6Mn3Cr2Fe3O16 (mp-861553) | 0.3829 | 0.882 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eVFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Cr_pv Fe_pv O |
Final Energy/Atom-6.5412 eV |
Corrected Energy-170.0251 eV
-170.0251 eV = -143.9067 eV (uncorrected energy) - 17.6910 eV (MP Advanced Correction) - 8.4275 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)