Final Magnetic Moment15.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.134 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.049 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.04 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiFeO2 + Li2CrO4 + Fe2O3 + LiCrO2 |
Band Gap0.644 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 0 0> | 177.3 |
AlN (mp-661) | <1 0 0> | <1 0 -1> | 251.7 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 122.9 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 301.2 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 200.8 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 141.9 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 283.7 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 319.2 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 251.0 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 238.0 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 173.6 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 319.2 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 283.7 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 319.2 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 283.7 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 319.2 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 319.2 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 283.7 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 141.9 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 200.8 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 248.3 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 177.3 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 245.8 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 70.9 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 177.3 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 200.8 |
Te2W (mp-22693) | <0 1 0> | <0 1 1> | 158.7 |
Te2W (mp-22693) | <0 1 1> | <0 1 0> | 301.2 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 307.2 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 177.3 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 35.5 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 50.2 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 61.4 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 122.9 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 319.2 |
BN (mp-984) | <0 0 1> | <0 0 1> | 307.2 |
BN (mp-984) | <1 0 0> | <1 0 0> | 283.7 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 184.3 |
LiNbO3 (mp-3731) | <1 0 0> | <0 1 0> | 150.6 |
LiNbO3 (mp-3731) | <1 0 1> | <0 0 1> | 307.2 |
LiNbO3 (mp-3731) | <1 1 0> | <1 0 1> | 260.4 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 248.3 |
Bi2Se3 (mp-541837) | <1 0 0> | <1 0 0> | 248.3 |
Al (mp-134) | <1 0 0> | <1 0 0> | 141.9 |
Al (mp-134) | <1 1 0> | <0 1 0> | 200.8 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 0> | 301.2 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 212.8 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 1> | 317.4 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 141.9 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 177.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li3Ti4O8 (mp-752879) | 0.1320 | 0.044 | 3 |
Li3(CoO2)4 (mp-763750) | 0.1200 | 0.099 | 3 |
Li3Cr4O8 (mp-771288) | 0.0675 | 0.031 | 3 |
Li3(CoO2)4 (mvc-16807) | 0.1552 | 0.164 | 3 |
Li3(FeO2)4 (mp-769726) | 0.0767 | 0.027 | 3 |
Li3Cr2(NiO4)2 (mp-780743) | 0.1023 | 0.086 | 4 |
Li3Cr3CoO8 (mp-765438) | 0.0926 | 0.020 | 4 |
Li3VCr3O8 (mp-771672) | 0.0737 | 0.063 | 4 |
Li3VFe3O8 (mp-773273) | 0.0631 | 0.061 | 4 |
Li3CoNi3O8 (mp-765439) | 0.0952 | 0.015 | 4 |
Fe7O8 (mp-705548) | 0.2154 | 0.077 | 2 |
V8C7 (mp-542730) | 0.2082 | 0.009 | 2 |
Fe7O8 (mp-32939) | 0.1825 | 0.077 | 2 |
Fe7O8 (mp-715333) | 0.2302 | 0.038 | 2 |
Ni9O10 (mp-656884) | 0.2380 | 0.050 | 2 |
Li6Mn3Cr2Fe3O16 (mp-861553) | 0.5302 | 0.079 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eVFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Cr_pv Fe_pv O |
Final Energy/Atom-6.5530 eV |
Corrected Energy-113.4048 eV
-113.4048 eV = -98.2945 eV (uncorrected energy) - 9.4920 eV (MP Advanced Correction) - 5.6183 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)