Final Magnetic Moment3.817 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.409 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.184 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.98 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi5Cr3(PO4)4 + Cr2P2O7 + CrP + Li3PO4 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 1 0> | 266.3 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 301.7 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 226.3 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 174.7 |
BaF2 (mp-1029) | <1 0 0> | <1 0 -1> | 199.0 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 226.3 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 174.7 |
KCl (mp-23193) | <1 0 0> | <1 1 -1> | 166.2 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 226.3 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 301.7 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 87.4 |
CdS (mp-672) | <1 1 0> | <1 0 -1> | 99.5 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 258.8 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 87.4 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 226.3 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 262.1 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 87.4 |
BN (mp-984) | <0 0 1> | <0 0 1> | 301.7 |
LiNbO3 (mp-3731) | <1 0 0> | <1 0 -1> | 298.4 |
BN (mp-984) | <1 1 1> | <0 0 1> | 301.7 |
MoS2 (mp-1434) | <1 0 0> | <1 0 0> | 262.1 |
MoS2 (mp-1434) | <1 1 0> | <0 0 1> | 226.3 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 226.3 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 262.1 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 262.1 |
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <0 0 1> | 226.3 |
GdScO3 (mp-5690) | <0 0 1> | <0 0 1> | 226.3 |
Mg (mp-153) | <1 1 0> | <0 0 1> | 226.3 |
KP(HO2)2 (mp-23959) | <0 0 1> | <0 0 1> | 75.4 |
KP(HO2)2 (mp-23959) | <0 1 0> | <0 0 1> | 75.4 |
KP(HO2)2 (mp-23959) | <1 0 0> | <0 0 1> | 226.3 |
TbScO3 (mp-31119) | <0 0 1> | <0 0 1> | 226.3 |
Ni (mp-23) | <1 1 0> | <1 0 -1> | 298.4 |
Ni (mp-23) | <1 0 0> | <1 0 -1> | 99.5 |
BaTiO3 (mp-5986) | <1 1 0> | <1 0 1> | 258.8 |
SiC (mp-11714) | <1 0 1> | <1 0 0> | 262.1 |
SiC (mp-11714) | <1 1 0> | <0 0 1> | 226.3 |
SiC (mp-11714) | <1 1 1> | <0 0 1> | 226.3 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 301.7 |
Ga2O3 (mp-886) | <1 1 -1> | <1 1 0> | 159.2 |
WS2 (mp-224) | <1 0 0> | <0 0 1> | 301.7 |
C (mp-48) | <0 0 1> | <0 0 1> | 226.3 |
C (mp-48) | <1 1 1> | <0 0 1> | 301.7 |
ZrO2 (mp-2858) | <1 0 0> | <0 0 1> | 226.3 |
ZrO2 (mp-2858) | <1 0 -1> | <1 0 1> | 258.8 |
YAlO3 (mp-3792) | <0 0 1> | <0 0 1> | 226.3 |
SiC (mp-8062) | <1 1 0> | <1 0 -1> | 298.4 |
CdWO4 (mp-19387) | <1 1 1> | <0 0 1> | 150.9 |
TiO2 (mp-390) | <1 1 0> | <0 1 1> | 153.0 |
TiO2 (mp-390) | <1 1 1> | <1 1 0> | 159.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
NaAsO3 (mp-17868) | 0.4968 | 0.002 | 3 |
MgSiO3 (mp-557803) | 0.5344 | 0.031 | 3 |
Sn2Ge2O7 (mp-768877) | 0.5247 | 0.059 | 3 |
MgSiO3 (mp-1020124) | 0.5422 | 0.028 | 3 |
Co3(P2O7)2 (mp-540500) | 0.4950 | 0.122 | 3 |
Li4Mn5(P3O11)2 (mp-540032) | 0.3837 | 0.032 | 4 |
LiTiP2O7 (mp-758145) | 0.3974 | 0.097 | 4 |
LiFe3P3O11 (mp-763776) | 0.4266 | 0.492 | 4 |
Na5Bi2As5O18 (mp-560658) | 0.4183 | 0.000 | 4 |
LiVP2O7 (mp-32476) | 0.4168 | 0.066 | 4 |
NaLiCu(PO3)3 (mp-775900) | 0.4881 | 0.087 | 5 |
Li4MnV3(P2O7)4 (mp-774458) | 0.5239 | 0.000 | 5 |
Li2VCr(P2O7)2 (mp-764239) | 0.5233 | 0.000 | 5 |
Li3MnV(P2O7)2 (mp-850951) | 0.4725 | 0.000 | 5 |
Li3VCr(P2O7)2 (mp-765133) | 0.4420 | 0.018 | 5 |
Na2Gd2MgSi4(O6F)2 (mp-557538) | 0.6588 | 0.000 | 6 |
NaLiMn2Fe4(PO4)6 (mp-777193) | 0.7377 | 0.031 | 6 |
NaInBP2HO9 (mp-757312) | 0.7038 | 0.013 | 6 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.5995 | 0.068 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eV |
PseudopotentialsVASP PAW: Li_sv Cr_pv P O |
Final Energy/Atom-7.0502 eV |
Corrected Energy-572.7492 eV
-572.7492 eV = -521.7184 eV (uncorrected energy) - 30.9008 eV (MP Anion Correction) - 20.1300 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)