Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.875 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.332 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.76 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiFePO4 + H2O |
Band Gap3.618 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <0 0 1> | 220.2 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 268.1 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 44.0 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 308.3 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 132.1 |
GaAs (mp-2534) | <1 1 0> | <1 0 1> | 92.0 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 220.2 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 1> | 276.1 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 220.2 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 308.3 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 160.9 |
AlN (mp-661) | <1 0 0> | <1 1 -1> | 299.5 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 220.2 |
BaF2 (mp-1029) | <1 1 0> | <1 0 -1> | 168.4 |
GaN (mp-804) | <0 0 1> | <0 1 1> | 208.2 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 152.9 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 268.1 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 88.1 |
GaN (mp-804) | <1 1 1> | <0 1 1> | 208.2 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 220.2 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 268.1 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 176.2 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 220.2 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 44.0 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 220.2 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 1> | 92.0 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 1> | 277.6 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 1> | 184.1 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 132.1 |
ZnSe (mp-1190) | <1 1 0> | <1 0 1> | 92.0 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 220.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 1> | 208.2 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 44.0 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 220.2 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 308.3 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 308.3 |
CdS (mp-672) | <1 0 1> | <1 0 -1> | 168.4 |
CdS (mp-672) | <1 1 1> | <1 0 -1> | 252.6 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 264.2 |
Te2W (mp-22693) | <0 0 1> | <1 1 -1> | 199.7 |
Te2W (mp-22693) | <0 1 0> | <1 0 -1> | 168.4 |
Te2W (mp-22693) | <1 0 0> | <1 0 0> | 305.7 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 176.2 |
Te2Mo (mp-602) | <0 0 1> | <0 1 1> | 208.2 |
Te2Mo (mp-602) | <1 0 0> | <1 0 -1> | 168.4 |
Te2Mo (mp-602) | <1 0 1> | <0 1 1> | 277.6 |
Ag (mp-124) | <1 0 0> | <1 0 1> | 276.1 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 264.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 1> | 276.1 |
GaSe (mp-1943) | <0 0 1> | <1 0 1> | 276.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
MnPO4 (mp-689981) | 0.6830 | 0.093 | 3 |
Hg3(AsO4)2 (mp-8975) | 0.6885 | 0.000 | 3 |
Sn8P2O13 (mp-767039) | 0.6729 | 0.025 | 3 |
Cu2PO4 (mp-17281) | 0.6938 | 0.002 | 3 |
V2Bi4O11 (mp-690568) | 0.6612 | 0.074 | 3 |
K2LiNbO4 (mp-759900) | 0.6148 | 0.000 | 4 |
LiMnPO4 (mp-770763) | 0.6621 | 0.050 | 4 |
Sb4H2SO10 (mp-698480) | 0.5740 | 0.000 | 4 |
LiSnPO4 (mp-757106) | 0.6585 | 0.069 | 4 |
CuSi(HO2)2 (mp-23731) | 0.6598 | 0.067 | 4 |
CuPH6NO5 (mp-733866) | 0.5468 | 0.041 | 5 |
LiVPH2O5 (mp-779915) | 0.5375 | 0.173 | 5 |
LiCrPH2O5 (mp-850156) | 0.5712 | 0.237 | 5 |
LiCuPH2O5 (mp-769159) | 0.4798 | 0.074 | 5 |
LiCrPH2O5 (mp-781961) | 0.3881 | 0.253 | 5 |
KLiPH2O4F (mp-690708) | 0.7154 | 0.038 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv P H O |
Final Energy/Atom-5.9518 eV |
Corrected Energy-263.0486 eV
-263.0486 eV = -238.0708 eV (uncorrected energy) - 14.0458 eV (MP Anion Correction) - 10.9320 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)