Final Magnetic Moment14.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.438 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.075 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.14 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiMnBO3 + Mn2BO4 + Mn3O4 + Li3B7O12 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <1 0 0> | 242.5 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 156.8 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 261.3 |
GaAs (mp-2534) | <1 1 0> | <1 0 1> | 141.9 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 156.8 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 274.0 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 313.6 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 209.0 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 261.3 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 156.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 261.3 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 121.2 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 313.6 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 261.3 |
ZnSe (mp-1190) | <1 1 0> | <1 0 1> | 141.9 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 261.3 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 261.3 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 313.6 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 261.3 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 141.9 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 156.8 |
YVO4 (mp-19133) | <1 0 1> | <0 1 0> | 274.0 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 209.0 |
GaSe (mp-1943) | <1 0 0> | <0 0 1> | 261.3 |
BN (mp-984) | <1 0 0> | <0 1 1> | 210.5 |
BN (mp-984) | <1 1 1> | <1 0 0> | 242.5 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 121.2 |
MoS2 (mp-1434) | <1 0 0> | <0 1 0> | 274.0 |
MoS2 (mp-1434) | <1 0 1> | <0 1 0> | 274.0 |
MoS2 (mp-1434) | <0 0 1> | <0 1 1> | 105.2 |
Al (mp-134) | <1 0 0> | <0 0 1> | 261.3 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 261.3 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 209.0 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 104.5 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 313.6 |
TiO2 (mp-2657) | <0 0 1> | <1 1 0> | 151.8 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 313.6 |
GdScO3 (mp-5690) | <0 1 0> | <0 0 1> | 313.6 |
GdScO3 (mp-5690) | <1 0 0> | <1 0 1> | 141.9 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 261.3 |
GdScO3 (mp-5690) | <1 1 0> | <0 0 1> | 261.3 |
Mg (mp-153) | <0 0 1> | <0 1 1> | 105.2 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 209.0 |
LaF3 (mp-905) | <0 0 1> | <0 0 1> | 313.6 |
LaF3 (mp-905) | <1 1 1> | <0 0 1> | 104.5 |
InP (mp-20351) | <1 0 0> | <1 0 1> | 141.9 |
InP (mp-20351) | <1 1 0> | <1 0 0> | 242.5 |
InP (mp-20351) | <1 1 1> | <1 0 0> | 121.2 |
TbScO3 (mp-31119) | <0 1 0> | <0 0 1> | 313.6 |
TbScO3 (mp-31119) | <1 0 0> | <1 0 1> | 141.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
TiPN3 (mp-989613) | 0.6374 | 0.029 | 3 |
Li3BS3 (mp-5614) | 0.6505 | 0.000 | 3 |
Li3BO3 (mp-27275) | 0.6855 | 0.000 | 3 |
Na3CoO3 (mp-777919) | 0.6471 | 0.127 | 3 |
Li6B4O9 (mp-1020024) | 0.5761 | 0.000 | 3 |
Li2Mn3(BO3)3 (mp-850436) | 0.1025 | 0.074 | 4 |
Li2Mn3(BO3)3 (mp-850433) | 0.0883 | 0.923 | 4 |
Li2Mn3(BO3)3 (mp-779390) | 0.0823 | 0.074 | 4 |
Li2Mn3(BO3)3 (mp-778775) | 0.0890 | 0.548 | 4 |
Li2Mn3(BO3)3 (mp-850773) | 0.0783 | 0.947 | 4 |
Li4MnFe2(BO3)4 (mp-767642) | 0.4392 | 0.055 | 5 |
Li2MnFe(BO3)2 (mp-780483) | 0.4415 | 0.010 | 5 |
Li3Mn2Fe(BO3)3 (mp-780294) | 0.4428 | 0.006 | 5 |
Li6Mn5Fe(BO3)6 (mp-779891) | 0.4424 | 0.001 | 5 |
Li3Mn2Fe(BO3)3 (mp-774378) | 0.4371 | 0.005 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv B O |
Final Energy/Atom-7.4095 eV |
Corrected Energy-549.2974 eV
-549.2974 eV = -503.8447 eV (uncorrected energy) - 25.2824 eV (MP Anion Correction) - 20.1702 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)