Final Magnetic Moment3.004 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-3.479 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.086 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.66 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTb2O3 + O2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4 [82] |
HallI 4 |
Point Group4 |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 0 0> | 239.8 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 191.8 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 95.9 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 135.6 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 239.8 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 143.9 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 335.7 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 143.9 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 335.7 |
SiO2 (mp-6930) | <0 0 1> | <1 0 1> | 86.5 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 143.9 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 239.8 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 48.0 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 203.5 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 239.8 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 239.8 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 335.7 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 135.6 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 0> | 271.3 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 191.8 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 239.8 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 95.9 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 135.6 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 143.9 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 67.8 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 335.7 |
CdS (mp-672) | <1 0 1> | <1 0 1> | 259.5 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 287.7 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 335.7 |
Te2W (mp-22693) | <0 1 1> | <1 0 1> | 173.0 |
YVO4 (mp-19133) | <1 1 0> | <1 0 1> | 259.5 |
BaTiO3 (mp-5986) | <1 0 0> | <1 0 0> | 239.8 |
BaTiO3 (mp-5986) | <1 0 1> | <1 1 0> | 67.8 |
BaTiO3 (mp-5986) | <1 1 0> | <1 0 0> | 48.0 |
NdGaO3 (mp-3196) | <0 0 1> | <1 1 0> | 271.3 |
NdGaO3 (mp-3196) | <1 0 1> | <1 1 0> | 271.3 |
SiC (mp-11714) | <1 1 1> | <1 1 0> | 271.3 |
Ga2O3 (mp-886) | <1 0 -1> | <1 0 0> | 239.8 |
Ga2O3 (mp-886) | <1 0 0> | <1 1 0> | 271.3 |
Au (mp-81) | <1 1 0> | <1 1 0> | 203.5 |
CdSe (mp-2691) | <1 0 0> | <1 0 0> | 239.8 |
WS2 (mp-224) | <0 0 1> | <1 0 0> | 335.7 |
WS2 (mp-224) | <1 1 0> | <1 0 0> | 239.8 |
C (mp-48) | <0 0 1> | <1 0 0> | 335.7 |
C (mp-48) | <1 0 0> | <0 0 1> | 287.9 |
C (mp-48) | <1 1 0> | <1 0 1> | 259.5 |
NaCl (mp-22862) | <1 0 0> | <1 0 0> | 95.9 |
NaCl (mp-22862) | <1 1 0> | <1 1 0> | 135.6 |
ZrO2 (mp-2858) | <0 1 1> | <1 1 0> | 271.3 |
ZrO2 (mp-2858) | <1 1 0> | <1 0 0> | 239.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ce6Th4O19 (mp-676287) | 0.6665 | 0.000 | 3 |
Li14Mn2S9 (mp-756198) | 0.6890 | 0.000 | 3 |
Ce6Y2O15 (mp-758094) | 0.5462 | 0.016 | 3 |
Yb6U3O17 (mp-675015) | 0.5555 | 0.000 | 3 |
Ce4ThO9 (mp-753456) | 0.3488 | 0.075 | 3 |
Ce5O9 (mp-760323) | 0.3490 | 0.000 | 2 |
Pr6O11 (mp-559771) | 0.4154 | 0.074 | 2 |
Ce5O9 (mp-32613) | 0.4130 | 0.007 | 2 |
Ce11O20 (mp-505619) | 0.4671 | 0.000 | 2 |
Tb11O20 (mp-556069) | 0.3880 | 0.076 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Tb_3 O |
Final Energy/Atom-7.8631 eV |
Corrected Energy-116.4043 eV
-116.4043 eV = -110.0837 eV (uncorrected energy) - 6.3206 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)