Final Magnetic Moment13.113 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.451 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.085 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.13 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2FeSiO4 + Fe2SiO4 + Fe2O3 + SiO2 |
Band Gap0.633 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 1 1> | 156.7 |
CeO2 (mp-20194) | <1 1 1> | <0 1 0> | 203.0 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 317.0 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 226.4 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 226.4 |
SiO2 (mp-6930) | <1 0 0> | <0 1 -1> | 136.7 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 317.0 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 317.0 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 317.0 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 317.0 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 135.3 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 226.4 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 317.0 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 0> | 203.0 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 203.0 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 226.4 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 135.9 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 90.6 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 181.1 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 45.3 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 226.4 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 135.9 |
Ag (mp-124) | <1 0 0> | <0 1 1> | 278.0 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 135.9 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 90.6 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 114.2 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 135.9 |
BN (mp-984) | <0 0 1> | <0 1 0> | 203.0 |
BN (mp-984) | <1 0 0> | <0 0 1> | 317.0 |
BN (mp-984) | <1 0 1> | <1 -1 0> | 258.1 |
BN (mp-984) | <1 1 0> | <0 0 1> | 135.9 |
BN (mp-984) | <1 1 1> | <0 0 1> | 135.9 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 271.7 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 45.3 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 271.7 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 271.7 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 271.7 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 90.6 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 271.7 |
Al (mp-134) | <1 0 0> | <0 0 1> | 317.0 |
Al (mp-134) | <1 1 1> | <0 1 0> | 203.0 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 0> | 135.3 |
LiGaO2 (mp-5854) | <0 1 0> | <1 -1 0> | 129.0 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 228.3 |
LiGaO2 (mp-5854) | <1 1 0> | <0 1 0> | 203.0 |
LiGaO2 (mp-5854) | <1 1 1> | <0 1 0> | 270.6 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 317.0 |
TeO2 (mp-2125) | <1 0 1> | <0 0 1> | 317.0 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 45.3 |
TiO2 (mp-2657) | <1 0 0> | <0 1 1> | 278.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na2Ti2O5 (mp-762058) | 0.5519 | 0.031 | 3 |
Be(GaO2)2 (mp-676950) | 0.6124 | 0.116 | 3 |
Ca2Si5N8 (mp-28922) | 0.5946 | 0.000 | 3 |
Li4P2O7 (mp-1020666) | 0.5086 | 0.620 | 3 |
BaGe7N10 (mp-1029679) | 0.5701 | 0.011 | 3 |
LiFeSiO4 (mp-767838) | 0.3751 | 0.070 | 4 |
Li2Si5Ni5O16 (mp-761373) | 0.4066 | 0.096 | 4 |
Li2Si3NiO8 (mp-863897) | 0.3626 | 0.093 | 4 |
LiCoSiO4 (mp-763260) | 0.4092 | 0.248 | 4 |
LiCo3(SiO4)2 (mp-849520) | 0.3154 | 0.554 | 4 |
Li3BePCO7 (mp-771341) | 0.5596 | 0.051 | 5 |
YAl6Si18(N15O)2 (mp-677127) | 0.7043 | 0.092 | 5 |
Zn8B4H3O15F (mp-676956) | 0.7296 | 0.013 | 5 |
LaAl2Si5N9O (mp-677482) | 0.5458 | 0.151 | 5 |
YAl6Si30(N15O)3 (mp-677140) | 0.7303 | 0.084 | 5 |
Na2Li2Al3Si3ClO12 (mp-43030) | 0.6040 | 0.003 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv Si O |
Final Energy/Atom-7.0180 eV |
Corrected Energy-336.2090 eV