Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.381 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.105 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.98 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiCu(PO3)3 + LiPO3 + Cu |
Band Gap1.231 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP212121 [19] |
HallP 2ac 2ab |
Point Group222 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 249.0 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 0> | 249.0 |
LaAlO3 (mp-2920) | <1 1 1> | <1 0 0> | 249.0 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 239.3 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 222.7 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 296.9 |
BaF2 (mp-1029) | <1 1 0> | <1 0 1> | 111.3 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 296.9 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 115.1 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 148.5 |
GaN (mp-804) | <1 1 1> | <0 1 1> | 217.9 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 148.5 |
KCl (mp-23193) | <1 1 0> | <1 0 1> | 111.3 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 0> | 159.5 |
InAs (mp-20305) | <1 1 0> | <1 0 1> | 111.3 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 296.9 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 296.9 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 222.7 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 296.9 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 222.7 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 249.0 |
LiNbO3 (mp-3731) | <1 1 0> | <1 0 0> | 249.0 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 0> | 239.3 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 319.1 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 239.3 |
Ag (mp-124) | <1 1 0> | <1 0 1> | 222.7 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 1> | 217.9 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 0> | 249.0 |
LiGaO2 (mp-5854) | <1 0 1> | <0 1 0> | 319.1 |
CdTe (mp-406) | <1 1 0> | <1 0 0> | 249.0 |
LiNbO3 (mp-3731) | <1 0 0> | <1 0 1> | 222.7 |
LiNbO3 (mp-3731) | <1 1 1> | <1 0 0> | 249.0 |
LiTaO3 (mp-3666) | <1 1 0> | <1 0 0> | 249.0 |
Fe3O4 (mp-19306) | <1 0 0> | <0 0 1> | 74.2 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 296.9 |
LiTaO3 (mp-3666) | <1 1 1> | <1 0 0> | 249.0 |
MgO (mp-1265) | <1 0 0> | <0 1 1> | 109.0 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 148.5 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 83.0 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 296.9 |
C (mp-66) | <1 1 1> | <0 0 1> | 222.7 |
GdScO3 (mp-5690) | <0 0 1> | <0 0 1> | 296.9 |
InSb (mp-20012) | <1 1 0> | <1 0 0> | 249.0 |
Mg (mp-153) | <1 0 1> | <0 1 0> | 319.1 |
Mg (mp-153) | <1 1 0> | <0 0 1> | 148.5 |
NdGaO3 (mp-3196) | <0 1 1> | <0 1 0> | 159.5 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 148.5 |
TbScO3 (mp-31119) | <1 0 1> | <0 1 0> | 159.5 |
Ga2O3 (mp-886) | <1 0 0> | <1 0 0> | 166.0 |
Au (mp-81) | <1 0 0> | <0 0 1> | 296.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
ZnSeO4 (mp-778924) | 0.5116 | 0.000 | 3 |
NaPO3 (mp-864891) | 0.5077 | 0.002 | 3 |
NaAsO3 (mp-17868) | 0.4304 | 0.002 | 3 |
MnPO4 (mp-777460) | 0.5123 | 0.000 | 3 |
CuSeO4 (mp-554040) | 0.4779 | 0.000 | 3 |
VZnP2O7 (mvc-5556) | 0.4715 | 0.047 | 4 |
LiCu(PO3)3 (mp-759435) | 0.4467 | 0.029 | 4 |
Li2Mn3(P2O7)2 (mp-31933) | 0.4784 | 0.030 | 4 |
Li2Ni3(P2O7)2 (mp-32373) | 0.4843 | 0.026 | 4 |
CaTi(SiO3)2 (mvc-6468) | 0.4770 | 0.222 | 4 |
Cr5O12 (mp-19575) | 0.7266 | 0.142 | 2 |
NaLiCu(PO3)3 (mp-775900) | 0.5932 | 0.087 | 5 |
LiMn3P2(HO3)4 (mp-763726) | 0.5705 | 0.479 | 5 |
LiMnPO4F (mp-762774) | 0.5597 | 0.324 | 5 |
SrMgCo(PO4)2 (mvc-2989) | 0.5930 | 0.014 | 5 |
SrZnCo(PO4)2 (mvc-2988) | 0.5883 | 0.022 | 5 |
InBP2H5NO9 (mp-752709) | 0.6869 | 0.000 | 6 |
Li2MgCr3Se3(SO8)3 (mp-773983) | 0.7214 | 0.331 | 6 |
Li2Mg2MnFe(PO4)4 (mp-849669) | 0.7080 | 0.008 | 6 |
LiMnVP2(HO5)2 (mp-765324) | 0.7152 | 0.072 | 6 |
AlBP2H5NO9 (mp-24757) | 0.7193 | 0.000 | 6 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.6437 | 0.068 | 7 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Cu_pv P O |
Final Energy/Atom-6.5385 eV |
Corrected Energy-417.5905 eV
-417.5905 eV = -392.3080 eV (uncorrected energy) - 25.2824 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)