Final Magnetic Moment8.559 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.095 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.049 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.59 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNa2CO3 + FeCO3 + Na2FePCO7 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFd3 [203] |
HallF 2 2 3 1d |
Point Groupm3 |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ca4GdB3O10 (mp-6943) | 0.7379 | 0.000 | 4 |
Ca4SmB3O10 (mp-6388) | 0.7362 | 0.000 | 4 |
Na6V2P(CO4)4 (mp-779855) | 0.1201 | 0.030 | 5 |
Na6Co2P(CO4)4 (mp-770874) | 0.1189 | 0.022 | 5 |
Na6Cr2P(CO4)4 (mp-770548) | 0.1407 | 0.045 | 5 |
Na6Mn2P(CO4)4 (mp-851213) | 0.1328 | 0.025 | 5 |
Na6Ni2P(CO4)4 (mp-780894) | 0.1105 | 0.017 | 5 |
Na2Li4Co2C4SO16 (mp-765657) | 0.6062 | 0.056 | 6 |
Na2Li4Ni2C4SO16 (mp-765655) | 0.6094 | 0.054 | 6 |
Na2Li4Mn2C4SO16 (mp-765654) | 0.5571 | 0.055 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Na_pv Fe_pv P C O |
Final Energy/Atom-6.5664 eV |
Corrected Energy-414.2589 eV
-414.2589 eV = -380.8536 eV (uncorrected energy) - 22.4733 eV (MP Anion Correction) - 10.9320 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)