Final Magnetic Moment14.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.468 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.045 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.12 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiMnBO3 + Mn2BO4 + Mn3O4 + Li3B7O12 |
Band Gap0.237 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 1> | <1 0 0> | 200.4 |
CeO2 (mp-20194) | <1 1 1> | <1 -1 0> | 216.8 |
BaF2 (mp-1029) | <1 1 0> | <1 -1 0> | 289.1 |
BaF2 (mp-1029) | <1 1 1> | <1 -1 0> | 72.3 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 238.5 |
SiO2 (mp-6930) | <1 1 1> | <1 0 -1> | 262.0 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 238.5 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 -1> | 255.3 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 -1> | 221.9 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 269.9 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 -1> | 277.3 |
CdS (mp-672) | <0 0 1> | <1 -1 0> | 289.1 |
CdS (mp-672) | <1 0 0> | <1 1 1> | 255.8 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 200.4 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 238.5 |
TePb (mp-19717) | <1 0 0> | <1 -1 0> | 216.8 |
Te2Mo (mp-602) | <1 0 0> | <1 0 -1> | 327.4 |
Te2Mo (mp-602) | <1 1 0> | <1 -1 0> | 289.1 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 -1> | 196.5 |
LaAlO3 (mp-2920) | <1 1 1> | <0 1 1> | 256.4 |
AlN (mp-661) | <0 0 1> | <0 1 1> | 85.5 |
AlN (mp-661) | <1 0 0> | <1 0 -1> | 327.4 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 238.5 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 269.9 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 190.8 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 238.5 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 333.9 |
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 269.9 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 238.5 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 238.5 |
GaN (mp-804) | <1 0 0> | <0 1 -1> | 221.9 |
GaN (mp-804) | <1 0 1> | <1 -1 1> | 265.5 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 238.5 |
SiO2 (mp-6930) | <0 0 1> | <1 -1 0> | 289.1 |
BN (mp-984) | <0 0 1> | <0 0 1> | 190.8 |
BN (mp-984) | <1 0 0> | <0 0 1> | 95.4 |
BN (mp-984) | <1 0 1> | <1 -1 0> | 216.8 |
BN (mp-984) | <1 1 0> | <0 1 0> | 269.9 |
BN (mp-984) | <1 1 1> | <0 0 1> | 333.9 |
KCl (mp-23193) | <1 1 0> | <1 -1 0> | 289.1 |
KCl (mp-23193) | <1 1 1> | <1 -1 0> | 72.3 |
LiNbO3 (mp-3731) | <0 0 1> | <1 -1 0> | 72.3 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 -1 0> | 289.1 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 215.9 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 215.9 |
LiF (mp-1138) | <1 1 0> | <0 1 -1> | 277.3 |
MoS2 (mp-1434) | <0 0 1> | <1 -1 -1> | 253.9 |
MoS2 (mp-1434) | <1 0 0> | <0 1 0> | 269.9 |
TePb (mp-19717) | <1 1 1> | <1 -1 0> | 72.3 |
MoS2 (mp-1434) | <1 0 1> | <1 -1 1> | 265.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li6B4O9 (mp-768875) | 0.7196 | 0.063 | 3 |
Na3CoO3 (mp-777919) | 0.6020 | 0.018 | 3 |
Li6B4O9 (mp-1020024) | 0.6778 | 0.000 | 3 |
Li3Mn4(BO3)4 (mp-781957) | 0.1525 | 0.042 | 4 |
Li2Mn3(BO3)3 (mp-853194) | 0.1484 | 0.044 | 4 |
Li2Mn3(BO3)3 (mp-851005) | 0.1416 | 0.042 | 4 |
Li3Mn4(BO3)4 (mp-780194) | 0.1602 | 0.047 | 4 |
Li3Mn4(BO3)4 (mp-780137) | 0.1625 | 0.037 | 4 |
Li8Mn3Fe5(BO3)8 (mp-775378) | 0.4683 | 0.023 | 5 |
Li2MnFe(BO3)2 (mp-780499) | 0.4685 | 0.018 | 5 |
Li8Mn5Fe3(BO3)8 (mp-774976) | 0.4596 | 0.016 | 5 |
Li8Mn5Fe3(BO3)8 (mp-778882) | 0.4646 | 0.018 | 5 |
Li8Mn3Fe5(BO3)8 (mp-774410) | 0.4654 | 0.023 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv B O |
Final Energy/Atom-7.4395 eV |
Corrected Energy-275.6710 eV
-275.6710 eV = -252.9446 eV (uncorrected energy) - 12.6412 eV (MP Anion Correction) - 10.0851 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)