Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-2.742 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.066 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.12 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToFe2O3 + Li3FeF6 + LiF |
Band Gap2.802 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 0 0> | 179.3 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 123.9 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 304.6 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 203.1 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 143.4 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 286.8 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 322.7 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 179.3 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 174.7 |
GaN (mp-804) | <1 1 0> | <1 0 -1> | 306.7 |
GaN (mp-804) | <1 1 1> | <1 0 -1> | 153.3 |
SiO2 (mp-6930) | <0 0 1> | <1 1 -1> | 216.1 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 304.6 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 143.4 |
SiO2 (mp-6930) | <1 1 1> | <1 1 1> | 101.0 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 322.7 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 322.7 |
InAs (mp-20305) | <1 0 0> | <1 0 -1> | 153.3 |
InAs (mp-20305) | <1 1 0> | <1 0 -1> | 51.1 |
InAs (mp-20305) | <1 1 1> | <1 0 -1> | 255.6 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 286.8 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 143.4 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 -1> | 204.5 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 251.0 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 179.3 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 247.7 |
LiF (mp-1138) | <1 1 0> | <1 0 -1> | 204.5 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 203.1 |
Te2W (mp-22693) | <0 1 0> | <0 1 1> | 160.2 |
Te2W (mp-22693) | <0 1 1> | <1 1 -1> | 288.2 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 309.7 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 179.3 |
Te2Mo (mp-602) | <0 0 1> | <1 0 1> | 87.3 |
Te2Mo (mp-602) | <1 0 0> | <1 1 0> | 310.8 |
Te2Mo (mp-602) | <1 1 0> | <1 0 0> | 179.3 |
Te2Mo (mp-602) | <1 1 1> | <0 0 1> | 185.8 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 35.9 |
Ag (mp-124) | <1 1 0> | <1 0 -1> | 51.1 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 61.9 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 0> | 358.5 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 286.8 |
BN (mp-984) | <0 0 1> | <1 0 -1> | 153.3 |
BN (mp-984) | <1 0 0> | <1 0 0> | 286.8 |
BN (mp-984) | <1 1 0> | <1 0 -1> | 255.6 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 185.8 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 179.3 |
Bi2Se3 (mp-541837) | <1 0 0> | <1 0 0> | 251.0 |
Al (mp-134) | <1 1 0> | <1 0 -1> | 204.5 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 0> | 304.6 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 0> | 253.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Zn(MoO2)2 (mvc-6278) | 0.2123 | 0.182 | 3 |
ZnCr2O4 (mvc-5335) | 0.2186 | 0.682 | 3 |
MgCr2O4 (mvc-5278) | 0.2195 | 2.774 | 3 |
Zn(MoO2)2 (mvc-9995) | 0.2165 | 0.285 | 3 |
Mg2PtO4 (mp-33940) | 0.2255 | 0.000 | 3 |
Li2CoOF3 (mp-782693) | 0.1941 | 0.046 | 4 |
Li9Fe3(OF7)2 (mp-780155) | 0.2222 | 0.039 | 4 |
Li2MnOF3 (mp-766805) | 0.1790 | 0.033 | 4 |
Li2VOF3 (mp-765855) | 0.0754 | 0.062 | 4 |
Li3V3O3F5 (mp-765397) | 0.2019 | 0.081 | 4 |
Fe3O4 (mp-542433) | 0.2656 | 0.075 | 2 |
Fe3O4 (mp-650112) | 0.2612 | 0.060 | 2 |
Fe3O4 (mp-715558) | 0.2725 | 0.785 | 2 |
Fe3O4 (mp-716052) | 0.2853 | 0.781 | 2 |
Fe3O4 (mp-715811) | 0.2756 | 0.037 | 2 |
Li4Cr3Ni3(SnO8)2 (mp-775690) | 0.2581 | 0.113 | 5 |
Li4Ti3Cr3(SnO8)2 (mp-776780) | 0.2548 | 0.138 | 5 |
Li4Co3Ni3(SbO8)2 (mp-762169) | 0.2603 | 0.025 | 5 |
Li4Fe3Cu3(SnO8)2 (mp-775631) | 0.2495 | 0.037 | 5 |
Li4Cr3Fe3(SnO8)2 (mp-775073) | 0.2613 | 1.088 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv O F |
Final Energy/Atom-5.3224 eV |
Corrected Energy-162.7684 eV
-162.7684 eV = -149.0273 eV (uncorrected energy) - 10.9320 eV (MP Advanced Correction) - 2.8092 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)