Final Magnetic Moment20.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.599 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.054 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.41 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiMn(PO3)3 |
Band Gap4.061 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 204.3 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 272.5 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 204.3 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 268.9 |
InAs (mp-20305) | <1 0 0> | <0 1 0> | 268.9 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 204.3 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 142.9 |
Te2W (mp-22693) | <1 1 0> | <0 1 1> | 112.6 |
YVO4 (mp-19133) | <0 0 1> | <0 1 0> | 268.9 |
Ag (mp-124) | <1 0 0> | <0 1 1> | 225.2 |
LiNbO3 (mp-3731) | <1 1 0> | <1 0 1> | 130.5 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 204.3 |
CdTe (mp-406) | <1 0 0> | <0 1 1> | 225.2 |
TeO2 (mp-2125) | <0 1 0> | <0 1 0> | 268.9 |
TeO2 (mp-2125) | <1 0 0> | <1 1 0> | 142.9 |
SiC (mp-7631) | <1 0 0> | <0 0 1> | 136.2 |
LiTaO3 (mp-3666) | <1 1 0> | <1 0 1> | 130.5 |
Fe3O4 (mp-19306) | <1 0 0> | <1 1 0> | 142.9 |
TiO2 (mp-2657) | <0 0 1> | <1 0 1> | 130.5 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 111.3 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 204.3 |
C (mp-66) | <1 1 0> | <0 0 1> | 272.5 |
Mg (mp-153) | <1 0 1> | <0 1 0> | 268.9 |
LaF3 (mp-905) | <1 0 0> | <0 1 0> | 268.9 |
LaF3 (mp-905) | <1 1 0> | <0 0 1> | 272.5 |
PbS (mp-21276) | <1 0 0> | <1 1 0> | 142.9 |
InP (mp-20351) | <1 0 0> | <1 1 0> | 142.9 |
Ni (mp-23) | <1 0 0> | <0 1 0> | 268.9 |
InSb (mp-20012) | <1 0 0> | <0 1 1> | 225.2 |
PbSe (mp-2201) | <1 0 0> | <0 1 0> | 268.9 |
BaTiO3 (mp-5986) | <0 0 1> | <1 1 0> | 142.9 |
SiC (mp-11714) | <1 0 0> | <0 0 1> | 272.5 |
Ga2O3 (mp-886) | <1 0 -1> | <0 1 0> | 268.9 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 272.5 |
Ga2O3 (mp-886) | <1 0 1> | <0 0 1> | 136.2 |
Au (mp-81) | <1 0 0> | <0 1 1> | 225.2 |
Au (mp-81) | <1 1 0> | <0 1 1> | 225.2 |
CdSe (mp-2691) | <1 0 0> | <0 1 0> | 268.9 |
WS2 (mp-224) | <0 0 1> | <0 0 1> | 204.3 |
C (mp-48) | <1 0 0> | <0 0 1> | 136.2 |
ZrO2 (mp-2858) | <0 0 1> | <0 1 1> | 112.6 |
ZrO2 (mp-2858) | <1 1 -1> | <0 1 1> | 225.2 |
YAlO3 (mp-3792) | <1 1 0> | <0 1 1> | 112.6 |
SiC (mp-8062) | <1 0 0> | <0 1 0> | 268.9 |
CdWO4 (mp-19387) | <0 1 0> | <1 1 1> | 158.3 |
CdWO4 (mp-19387) | <1 1 1> | <0 0 1> | 204.3 |
LiAlO2 (mp-3427) | <0 0 1> | <0 1 0> | 268.9 |
LiAlO2 (mp-3427) | <1 1 1> | <0 0 1> | 272.5 |
YAlO3 (mp-3792) | <0 1 0> | <0 1 0> | 268.9 |
YAlO3 (mp-3792) | <1 0 0> | <0 0 1> | 204.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LiNi(PO3)3 (mp-868384) | 0.2483 | 0.052 | 4 |
LiP2WO8 (mp-763483) | 0.4449 | 0.057 | 4 |
LiFe(PO3)3 (mp-762486) | 0.4089 | 0.044 | 4 |
LiV(PO3)3 (mp-763397) | 0.1589 | 0.075 | 4 |
LiP2WO8 (mp-763410) | 0.4896 | 0.061 | 4 |
Cr19O48 (mp-850874) | 0.6802 | 0.095 | 2 |
Sb2P5O16 (mp-25946) | 0.4656 | 0.006 | 3 |
V4P7O24 (mp-540336) | 0.5123 | 0.004 | 3 |
Fe3(P2O7)2 (mp-565653) | 0.4992 | 0.000 | 3 |
Ni3(P2O7)2 (mp-776065) | 0.5176 | 0.070 | 3 |
Ba2P6O17 (mp-779723) | 0.4570 | 0.015 | 3 |
KMnP3HO10 (mp-763796) | 0.5179 | 0.009 | 5 |
LiVP2HO7 (mp-767683) | 0.5036 | 0.058 | 5 |
LiMnP2HO7 (mp-773554) | 0.4799 | 0.036 | 5 |
LiMnP3HO10 (mp-780889) | 0.5243 | 0.049 | 5 |
LiFeP2HO7 (mp-781683) | 0.5075 | 0.029 | 5 |
NaFeBP2H3O10 (mp-541793) | 0.6930 | 0.001 | 6 |
CaNiBP2H3O10 (mp-25716) | 0.6832 | 0.007 | 6 |
RbScBP2HO9 (mp-23809) | 0.6802 | 0.000 | 6 |
Ba3Li2Mo4P6(ClO14)2 (mp-699932) | 0.6272 | 0.002 | 6 |
KLiMnP3HO10 (mp-764313) | 0.6793 | 0.044 | 6 |
Al2P2H8C2NO8F (mp-708964) | 0.6657 | 0.050 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-points4 |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv P O |
Final Energy/Atom-7.1495 eV |
Corrected Energy-432.3751 eV
-432.3751 eV = -400.3693 eV (uncorrected energy) - 25.2824 eV (MP Anion Correction) - 6.7234 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)