Final Magnetic Moment4.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.246 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.144 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.99 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMnPO4 + LiMnPHO5 |
Band Gap0.619 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/m [11] |
Hall-P 2yb |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 0 1> | 126.5 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 210.8 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 244.4 |
CeO2 (mp-20194) | <1 0 0> | <1 1 -1> | 246.3 |
CeO2 (mp-20194) | <1 1 0> | <1 0 -1> | 126.1 |
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 262.8 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 168.6 |
GaN (mp-804) | <1 0 0> | <1 0 -1> | 252.3 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 210.2 |
GaN (mp-804) | <1 1 0> | <1 1 1> | 297.0 |
GaN (mp-804) | <1 1 1> | <1 1 -1> | 246.3 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 262.8 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 244.4 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 168.6 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 241.8 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 -1> | 246.3 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 315.4 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 305.4 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 210.8 |
InAs (mp-20305) | <1 1 1> | <0 1 0> | 262.8 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 262.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 210.2 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 -1> | 252.3 |
CdS (mp-672) | <0 0 1> | <1 1 -1> | 246.3 |
CdS (mp-672) | <1 0 0> | <1 0 1> | 83.9 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 244.4 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 244.4 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 262.8 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 262.8 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 210.8 |
YVO4 (mp-19133) | <1 0 1> | <0 1 0> | 210.2 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 315.4 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 210.8 |
Ag (mp-124) | <1 1 0> | <0 1 1> | 202.1 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 -1> | 189.2 |
GaSe (mp-1943) | <1 0 1> | <1 1 1> | 198.0 |
BN (mp-984) | <0 0 1> | <0 1 1> | 202.1 |
BN (mp-984) | <1 0 1> | <0 0 1> | 337.2 |
LiNbO3 (mp-3731) | <0 0 1> | <1 1 -1> | 164.2 |
LiNbO3 (mp-3731) | <1 1 1> | <0 1 0> | 262.8 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 1 -1> | 246.3 |
MoS2 (mp-1434) | <0 0 1> | <1 1 -1> | 246.3 |
MoS2 (mp-1434) | <1 1 0> | <1 1 -1> | 246.3 |
Al (mp-134) | <1 0 0> | <0 1 0> | 210.2 |
Al (mp-134) | <1 1 0> | <1 0 -1> | 252.3 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 0> | 305.4 |
TeO2 (mp-2125) | <1 1 0> | <0 0 1> | 295.1 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 295.1 |
Fe3O4 (mp-19306) | <1 1 1> | <1 0 1> | 251.7 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 295.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Fe3(P2O7)2 (mvc-12221) | 0.5288 | 0.327 | 3 |
V3(P2O7)2 (mp-32416) | 0.4856 | 0.033 | 3 |
Mn3(P2O7)2 (mp-694554) | 0.5248 | 0.162 | 3 |
P4W3O14 (mvc-1031) | 0.4940 | 0.315 | 3 |
Fe3(P2O7)2 (mp-540486) | 0.4975 | 0.327 | 3 |
LiCoP2O7 (mp-705332) | 0.4435 | 0.080 | 4 |
LiNiP2O7 (mp-705331) | 0.3995 | 0.071 | 4 |
LiFeP2O7 (mp-697758) | 0.4495 | 0.190 | 4 |
Li3Cr4(PO4)6 (mp-767848) | 0.4103 | 0.052 | 4 |
Li3V4(PO4)6 (mp-767790) | 0.4381 | 0.062 | 4 |
Cr5O12 (mp-19575) | 0.6749 | 0.142 | 2 |
VO2 (mvc-6918) | 0.7310 | 0.095 | 2 |
MoO2 (mvc-6944) | 0.7132 | 0.281 | 2 |
VCrP2(HO5)2 (mp-766804) | 0.4872 | 0.046 | 5 |
MnVP2(HO5)2 (mp-766980) | 0.4986 | 0.046 | 5 |
VFeP2(HO5)2 (mp-765969) | 0.4484 | 0.052 | 5 |
CaV2P3HO12 (mp-735589) | 0.5033 | 0.113 | 5 |
LiMnPO4F (mp-762774) | 0.5169 | 0.324 | 5 |
InBP2H5NO9 (mp-752709) | 0.6280 | 0.000 | 6 |
LiMgCr3Se2(SO6)4 (mp-769552) | 0.5690 | 0.257 | 6 |
NaLi3Ti2Cr2(PO4)6 (mp-777190) | 0.6171 | 0.020 | 6 |
Li2MgCr3Se3(SO8)3 (mp-773983) | 0.6250 | 0.331 | 6 |
NaLiMn2Fe4(PO4)6 (mp-777193) | 0.6001 | 0.018 | 6 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.5644 | 0.068 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv P H O |
Final Energy/Atom-6.8556 eV |
Corrected Energy-225.0328 eV
-225.0328 eV = -205.6682 eV (uncorrected energy) - 12.6412 eV (MP Anion Correction) - 6.7234 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)