Final Magnetic Moment1.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.499 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.051 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.95 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi6V3P8O29 + VPO5 + Li3V2P4(HO8)2 + VP2O7 + PH3O4 |
Band Gap1.371 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <1 0 -1> | 274.1 |
AlN (mp-661) | <1 0 0> | <0 1 -1> | 140.0 |
AlN (mp-661) | <1 1 0> | <0 1 -1> | 140.0 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 207.7 |
BaF2 (mp-1029) | <1 1 0> | <0 1 -1> | 279.9 |
GaN (mp-804) | <0 0 1> | <0 1 -1> | 279.9 |
GaN (mp-804) | <1 0 0> | <1 0 -1> | 274.1 |
GaN (mp-804) | <1 0 1> | <0 1 -1> | 210.0 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 277.0 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 155.2 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 207.7 |
CdS (mp-672) | <1 1 0> | <0 1 -1> | 210.0 |
CdS (mp-672) | <1 1 1> | <0 1 -1> | 210.0 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 232.9 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 155.2 |
BN (mp-984) | <0 0 1> | <0 1 -1> | 279.9 |
BN (mp-984) | <1 0 1> | <0 1 1> | 119.6 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 138.5 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 0> | 310.5 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 1> | 230.6 |
LiGaO2 (mp-5854) | <1 1 0> | <0 1 1> | 239.3 |
LiGaO2 (mp-5854) | <1 1 1> | <0 0 1> | 277.0 |
SiC (mp-7631) | <0 0 1> | <1 -1 -1> | 124.1 |
SiC (mp-7631) | <1 1 0> | <0 1 1> | 239.3 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 310.5 |
MgO (mp-1265) | <1 1 0> | <1 0 -1> | 182.7 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 277.0 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 207.7 |
C (mp-66) | <1 1 0> | <0 0 1> | 277.0 |
GdScO3 (mp-5690) | <0 1 1> | <1 0 -1> | 274.1 |
Mg (mp-153) | <0 0 1> | <1 -1 0> | 182.8 |
Mg (mp-153) | <1 0 0> | <1 0 -1> | 182.7 |
Mg (mp-153) | <1 0 1> | <0 1 -1> | 279.9 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 277.0 |
GaP (mp-2490) | <1 1 0> | <0 0 1> | 207.7 |
TbScO3 (mp-31119) | <0 1 1> | <1 0 0> | 155.2 |
Ni (mp-23) | <1 0 0> | <1 0 -1> | 182.7 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 277.0 |
NdGaO3 (mp-3196) | <0 1 0> | <0 0 1> | 207.7 |
NdGaO3 (mp-3196) | <0 1 1> | <1 0 0> | 155.2 |
NdGaO3 (mp-3196) | <1 1 1> | <1 -1 0> | 274.3 |
SiC (mp-11714) | <0 0 1> | <1 -1 -1> | 124.1 |
SiC (mp-11714) | <1 1 0> | <0 0 1> | 207.7 |
Ga2O3 (mp-886) | <1 0 0> | <1 0 0> | 310.5 |
Si (mp-149) | <1 1 0> | <0 0 1> | 207.7 |
WS2 (mp-224) | <1 0 1> | <1 0 0> | 232.9 |
C (mp-48) | <0 0 1> | <1 -1 -1> | 248.1 |
C (mp-48) | <1 0 1> | <0 1 1> | 119.6 |
ZrO2 (mp-2858) | <0 0 1> | <1 -1 -1> | 248.1 |
ZrO2 (mp-2858) | <0 1 0> | <1 -1 0> | 274.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cr5(PO4)4 (mp-540446) | 0.6414 | 0.007 | 3 |
Mn2V2O7 (mp-572632) | 0.6507 | 0.004 | 3 |
V4P2O13 (mp-768034) | 0.6611 | 0.019 | 3 |
Cr5(PO4)4 (mp-775246) | 0.6340 | 0.007 | 3 |
CuMoO4 (mp-652716) | 0.6469 | 0.027 | 3 |
Li3Cr4(PO4)6 (mp-868663) | 0.5370 | 0.047 | 4 |
LiCo2(PO4)3 (mp-761746) | 0.5427 | 0.112 | 4 |
Li3V4(PO4)6 (mp-767872) | 0.5173 | 0.018 | 4 |
Ca3Fe4(WO4)6 (mvc-8255) | 0.5857 | 0.102 | 4 |
LiMn2(PO4)3 (mp-762717) | 0.5873 | 0.038 | 4 |
LiVP2HO8 (mp-850369) | 0.1166 | 0.050 | 5 |
LiVP2HO8 (mp-780485) | 0.1464 | 0.047 | 5 |
LiVP2HO8 (mp-780482) | 0.0594 | 0.050 | 5 |
LiVP2HO8 (mp-850512) | 0.1312 | 0.069 | 5 |
LiVP2HO8 (mp-777138) | 0.1476 | 0.048 | 5 |
LiVFeP2(O4F)2 (mp-777635) | 0.6058 | 0.028 | 6 |
LiVCrP2(O4F)2 (mp-868574) | 0.6139 | 0.006 | 6 |
LiVCrP2(O4F)2 (mp-765305) | 0.6224 | 0.008 | 6 |
LiVCrP2(O4F)2 (mp-765118) | 0.6131 | 0.007 | 6 |
LiVCrP2(O4F)2 (mp-765173) | 0.6179 | 0.007 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv V_pv P H O |
Final Energy/Atom-6.9096 eV |
Corrected Energy-388.5015 eV
-388.5015 eV = -359.3003 eV (uncorrected energy) - 22.4733 eV (MP Anion Correction) - 6.7280 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)