Final Magnetic Moment0.345 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-1.734 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.883 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.36 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi4P2O7 + Mn2P2O7 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2221 [20] |
HallC 2c 2 |
Point Group222 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <0 0 1> | 264.9 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 264.9 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 88.3 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 264.9 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 264.9 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 264.9 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 264.9 |
TeO2 (mp-2125) | <0 1 0> | <0 0 1> | 264.9 |
BN (mp-984) | <1 0 1> | <0 0 1> | 264.9 |
BN (mp-984) | <1 1 0> | <0 0 1> | 264.9 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 264.9 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 176.6 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 176.6 |
LiGaO2 (mp-5854) | <1 1 1> | <0 0 1> | 264.9 |
C (mp-66) | <1 1 1> | <0 0 1> | 88.3 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 264.9 |
SiC (mp-11714) | <1 1 0> | <0 0 1> | 264.9 |
CdSe (mp-2691) | <1 1 1> | <0 0 1> | 264.9 |
CaCO3 (mp-3953) | <0 0 1> | <0 0 1> | 88.3 |
SiC (mp-8062) | <1 0 0> | <0 0 1> | 264.9 |
TiO2 (mp-390) | <1 0 0> | <0 0 1> | 264.9 |
TiO2 (mp-390) | <1 1 0> | <0 0 1> | 264.9 |
SiC (mp-8062) | <1 1 0> | <0 0 1> | 264.9 |
Cu (mp-30) | <1 0 0> | <0 0 1> | 264.9 |
GaSb (mp-1156) | <1 1 1> | <0 0 1> | 264.9 |
LiAlO2 (mp-3427) | <1 1 1> | <0 0 1> | 264.9 |
ZnTe (mp-2176) | <1 1 0> | <0 0 1> | 264.9 |
ZnTe (mp-2176) | <1 1 1> | <0 0 1> | 264.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ni7(P2O7)4 (mp-779819) | 0.4909 | 0.019 | 3 |
Mn6P7O24 (mp-504168) | 0.4792 | 0.003 | 3 |
Cr6P7O24 (mp-504359) | 0.5163 | 0.021 | 3 |
MnSiO3 (mp-19528) | 0.5150 | 0.007 | 3 |
Ni6P7O24 (mp-705425) | 0.4542 | 0.009 | 3 |
LiMn6P7O24 (mp-504167) | 0.4346 | 0.000 | 4 |
LiNi6P7O24 (mp-504371) | 0.4684 | 0.012 | 4 |
LiCo6P7O24 (mp-31557) | 0.4789 | 0.007 | 4 |
LiMnP2O7 (mp-540068) | 0.4528 | 0.146 | 4 |
LiNi6P7O24 (mp-705406) | 0.4657 | 0.012 | 4 |
Li3MnV(PO4)3 (mp-774954) | 0.5749 | 0.241 | 5 |
Li2MnV(PO4)3 (mp-771372) | 0.5209 | 0.240 | 5 |
Li2MnV(PO4)3 (mp-770179) | 0.5544 | 0.039 | 5 |
LiMnPO4F (mp-763235) | 0.5397 | 0.567 | 5 |
Na2ZrCo(P2O7)2 (mp-562673) | 0.5895 | 0.030 | 5 |
LiVFeP2(O4F)2 (mp-777635) | 0.6072 | 0.026 | 6 |
Li4TiNi3Sn2(PO4)6 (mp-778249) | 0.6135 | 0.173 | 6 |
LiMnVP2(HO5)2 (mp-765378) | 0.5744 | 0.046 | 6 |
LiMnVP2(HO5)2 (mp-765324) | 0.5632 | 0.046 | 6 |
LiVCrP2(HO5)2 (mp-765123) | 0.6045 | 0.147 | 6 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.6416 | 0.068 | 7 |
KNa2LiTi2Fe2(SiO3)8 (mp-542926) | 0.7402 | 0.071 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv P O |
Final Energy/Atom-6.5869 eV |
Corrected Energy-654.6435 eV
Uncorrected energy = -592.8195 eV
Composition-based energy adjustment (-0.687 eV/atom x 56.0 atoms) = -38.4720 eV
Composition-based energy adjustment (-1.668 eV/atom x 14.0 atoms) = -23.3520 eV
Corrected energy = -654.6435 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)