Final Magnetic Moment2.006 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.489 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.049 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.74 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToV2O3 + Na2V3O7 + Na2B4O7 + Na3VO4 + Na2SO4 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFd3 [203] |
HallF 2 2 3 1d |
Point Groupm3 |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ca4GdB3O10 (mp-6943) | 0.7320 | 0.000 | 4 |
Ca4SmB3O10 (mp-6388) | 0.7243 | 0.000 | 4 |
Ca4LaB3O10 (mp-6076) | 0.7294 | 0.000 | 4 |
Na6Cr2B4SO16 (mp-853192) | 0.0418 | 0.049 | 5 |
Na6Fe2B4PO16 (mp-772422) | 0.2041 | 0.049 | 5 |
Na6Mn2B4SO16 (mp-770500) | 0.1152 | 0.153 | 5 |
Na6Fe2B4SO16 (mp-770356) | 0.1290 | 0.130 | 5 |
Na6Co2B4SO16 (mp-851008) | 0.1156 | 0.069 | 5 |
Na2Li4Co2C4SO16 (mp-765657) | 0.6815 | 0.166 | 6 |
Na2Li4Ni2C4SO16 (mp-765655) | 0.6849 | 0.097 | 6 |
Na2Li4Mn2C4SO16 (mp-765654) | 0.6206 | 0.254 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Na_pv V_pv B S O |
Final Energy/Atom-6.6541 eV |
Corrected Energy-415.7258 eV
Uncorrected energy = -385.9358 eV
Composition-based energy adjustment (-0.503 eV/atom x 2.0 atoms) = -1.0060 eV
Composition-based energy adjustment (-0.687 eV/atom x 32.0 atoms) = -21.9840 eV
Composition-based energy adjustment (-1.700 eV/atom x 4.0 atoms) = -6.8000 eV
Corrected energy = -415.7258 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)