Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.313 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density9.93 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP421c [114] |
HallP 4 2n |
Point Group42m |
Crystal Systemtetragonal |
Topological ClassificationTI*
|
SubclassificationSEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
KP(HO2)2 (mp-23959) | <0 0 1> | <0 0 1> | 216.1 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 108.0 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 216.1 |
LiNbO3 (mp-3731) | <1 0 0> | <1 0 0> | 147.2 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 206.1 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 351.1 |
Mg (mp-153) | <1 0 1> | <1 0 0> | 265.0 |
BN (mp-984) | <1 1 0> | <1 0 1> | 199.8 |
TiO2 (mp-390) | <1 0 0> | <1 1 0> | 333.2 |
Si (mp-149) | <1 0 0> | <1 0 1> | 119.9 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 249.9 |
CeO2 (mp-20194) | <1 0 0> | <1 0 1> | 119.9 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 117.8 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 265.0 |
GaSb (mp-1156) | <1 0 0> | <0 0 1> | 351.1 |
NdGaO3 (mp-3196) | <1 0 0> | <1 0 0> | 88.3 |
C (mp-48) | <0 0 1> | <1 0 1> | 199.8 |
Ni (mp-23) | <1 1 0> | <1 0 0> | 294.5 |
CdS (mp-672) | <1 1 1> | <1 1 0> | 208.2 |
SiC (mp-7631) | <1 0 0> | <1 0 0> | 235.6 |
MgF2 (mp-1249) | <1 0 0> | <0 0 1> | 216.1 |
ZrO2 (mp-2858) | <0 1 1> | <0 0 1> | 351.1 |
CdSe (mp-2691) | <1 0 0> | <0 0 1> | 351.1 |
LiAlO2 (mp-3427) | <1 1 0> | <0 0 1> | 324.1 |
MgAl2O4 (mp-3536) | <1 0 0> | <0 0 1> | 135.0 |
YAlO3 (mp-3792) | <0 1 0> | <1 0 0> | 117.8 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 351.1 |
TiO2 (mp-390) | <1 0 1> | <1 0 0> | 117.8 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 135.0 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 124.9 |
TeO2 (mp-2125) | <0 1 0> | <1 0 0> | 206.1 |
LiAlO2 (mp-3427) | <1 0 1> | <0 0 1> | 216.1 |
LiAlO2 (mp-3427) | <0 0 1> | <0 0 1> | 27.0 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 54.0 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 0> | 166.6 |
ZnO (mp-2133) | <1 1 1> | <1 1 0> | 124.9 |
GaP (mp-2490) | <1 0 0> | <1 0 1> | 119.9 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 235.6 |
Te2Mo (mp-602) | <0 0 1> | <1 0 1> | 119.9 |
Te2W (mp-22693) | <0 1 0> | <1 0 1> | 159.8 |
SiC (mp-11714) | <0 0 1> | <1 0 0> | 265.0 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 265.0 |
SiC (mp-11714) | <1 0 1> | <1 0 1> | 159.8 |
SiC (mp-7631) | <1 0 1> | <1 0 0> | 235.6 |
GaSe (mp-1943) | <1 0 1> | <1 0 1> | 279.7 |
NaCl (mp-22862) | <1 1 0> | <1 0 0> | 323.9 |
YAlO3 (mp-3792) | <1 0 0> | <1 1 1> | 198.5 |
ZrO2 (mp-2858) | <1 0 0> | <1 0 1> | 199.8 |
PbS (mp-21276) | <1 0 0> | <1 0 0> | 323.9 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 29.4 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
218 | 109 | 121 | 0 | 0 | 0 |
109 | 218 | 121 | 0 | 0 | 0 |
121 | 121 | 188 | 0 | 0 | 0 |
0 | 0 | 0 | 28 | 0 | 0 |
0 | 0 | 0 | 0 | 28 | 0 |
0 | 0 | 0 | 0 | 0 | 44 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
7.5 | -1.7 | -3.7 | 0 | 0 | 0 |
-1.7 | 7.5 | -3.7 | 0 | 0 | 0 |
-3.7 | -3.7 | 10.1 | 0 | 0 | 0 |
0 | 0 | 0 | 35.8 | 0 | 0 |
0 | 0 | 0 | 0 | 35.8 | 0 |
0 | 0 | 0 | 0 | 0 | 23 |
Shear Modulus GV38 GPa |
Bulk Modulus KV147 GPa |
Shear Modulus GR36 GPa |
Bulk Modulus KR147 GPa |
Shear Modulus GVRH37 GPa |
Bulk Modulus KVRH147 GPa |
Elastic Anisotropy0.35 |
Poisson's Ratio0.38 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
RbPrTe4 (mp-7199) | 0.6851 | 0.000 | 3 |
KGdTe4 (mp-542281) | 0.6949 | 0.001 | 3 |
Cu2PPd2 (mp-1001022) | 0.4352 | 0.004 | 3 |
RbNdTe4 (mp-11011) | 0.6817 | 0.003 | 3 |
RbGdTe4 (mp-19914) | 0.6916 | 0.000 | 3 |
Pd4Se (mp-7818) | 0.3769 | 0.000 | 2 |
Mn4Si7 (mp-568121) | 0.6842 | 0.000 | 2 |
Mn15Si26 (mp-752) | 0.6784 | 0.005 | 2 |
Mg2Si (mp-1074753) | 0.6059 | 0.131 | 2 |
Mg2Si (mp-1074759) | 0.6624 | 0.174 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Pd S |
Final Energy/Atom-5.1487 eV |
Corrected Energy-52.8141 eV
-52.8141 eV = -51.4872 eV (uncorrected energy) - 1.3269 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)