Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.952 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.085 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.17 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToYNbO4 + NbNO |
Band Gap2.515 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21 [4] |
HallP 2yb |
Point Group2 |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 346.6 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 283.6 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 0> | 238.2 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 220.6 |
AlN (mp-661) | <1 0 0> | <1 0 1> | 171.2 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 126.0 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 79.4 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 220.6 |
CeO2 (mp-20194) | <1 0 0> | <1 1 0> | 119.7 |
GaAs (mp-2534) | <1 0 0> | <1 0 1> | 256.8 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 158.8 |
BaF2 (mp-1029) | <1 1 1> | <0 1 0> | 268.8 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 283.6 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 85.6 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 252.1 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 238.2 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 252.1 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 252.1 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 238.2 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 283.6 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 1> | 256.8 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 283.6 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 158.8 |
InAs (mp-20305) | <1 1 1> | <0 1 0> | 268.8 |
ZnSe (mp-1190) | <1 0 0> | <1 0 1> | 256.8 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 1> | 256.8 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 157.6 |
Fe3O4 (mp-19306) | <1 1 1> | <0 0 1> | 126.0 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 252.1 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 220.6 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 126.0 |
MgO (mp-1265) | <1 1 1> | <1 0 0> | 158.8 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 220.6 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 157.6 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 252.1 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 346.6 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 158.8 |
Te2W (mp-22693) | <0 1 1> | <1 0 1> | 171.2 |
YVO4 (mp-19133) | <0 0 1> | <1 0 1> | 256.8 |
YVO4 (mp-19133) | <1 1 1> | <1 1 0> | 239.5 |
Ge3(BiO3)4 (mp-23560) | <1 1 0> | <1 0 0> | 158.8 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 238.2 |
C (mp-66) | <1 0 0> | <0 0 1> | 157.6 |
C (mp-66) | <1 1 0> | <0 0 1> | 346.6 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 315.1 |
Te2Mo (mp-602) | <1 0 0> | <1 0 0> | 158.8 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 283.6 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 126.0 |
GdScO3 (mp-5690) | <1 0 0> | <0 0 1> | 94.5 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 283.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Nb2CdO6 (mp-781861) | 0.3772 | 0.000 | 3 |
MnNb2O6 (mp-640524) | 0.4507 | 0.250 | 3 |
CuReO4 (mp-755115) | 0.4562 | 0.056 | 3 |
Nb3CuO8 (mp-27383) | 0.4235 | 0.038 | 3 |
LiNb3O8 (mp-3368) | 0.3695 | 0.000 | 3 |
YNb2NO5 (mp-775939) | 0.2255 | 0.080 | 4 |
YNb2NO5 (mp-849365) | 0.2140 | 0.074 | 4 |
YNb2NO5 (mp-782062) | 0.1618 | 0.081 | 4 |
YNb2NO5 (mp-776408) | 0.3068 | 0.072 | 4 |
YNb2NO5 (mp-776443) | 0.1292 | 0.085 | 4 |
V5O12 (mp-777580) | 0.7218 | 0.071 | 2 |
ReN2 (mp-1019080) | 0.6394 | 0.067 | 2 |
WN2 (mp-776321) | 0.6391 | 0.143 | 2 |
LiCrCO3F2 (mp-767637) | 0.7071 | 0.099 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Y_sv Nb_pv N O |
Final Energy/Atom-9.1573 eV |
Corrected Energy-344.8452 eV
Uncorrected energy = -329.6612 eV
Composition-based energy adjustment (-0.687 eV/atom x 20.0 atoms) = -13.7400 eV
Composition-based energy adjustment (-0.361 eV/atom x 4.0 atoms) = -1.4440 eV
Corrected energy = -344.8452 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)