Final Magnetic Moment2.015 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.604 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.139 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.58 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToVO2 + V3O5 + Li3VO4 + TiO2 |
Band Gap0.877 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 -1 0> | 225.1 |
LaAlO3 (mp-2920) | <1 0 0> | <0 1 0> | 284.5 |
LaAlO3 (mp-2920) | <1 0 1> | <1 -1 0> | 225.1 |
AlN (mp-661) | <0 0 1> | <0 1 -1> | 144.9 |
AlN (mp-661) | <1 0 0> | <0 1 -1> | 108.6 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 126.4 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 158.1 |
AlN (mp-661) | <1 1 1> | <0 1 -1> | 144.9 |
CeO2 (mp-20194) | <1 0 0> | <1 -1 -1> | 148.0 |
CeO2 (mp-20194) | <1 1 0> | <1 -1 0> | 160.8 |
GaAs (mp-2534) | <1 0 0> | <0 1 1> | 101.8 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 239.7 |
GaAs (mp-2534) | <1 1 1> | <1 -1 0> | 225.1 |
BaF2 (mp-1029) | <1 0 0> | <1 -1 0> | 193.0 |
BaF2 (mp-1029) | <1 1 0> | <1 -1 -1> | 111.0 |
BaF2 (mp-1029) | <1 1 1> | <1 -1 0> | 289.5 |
GaN (mp-804) | <0 0 1> | <1 1 -1> | 154.3 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 119.8 |
GaN (mp-804) | <1 0 1> | <1 -1 0> | 128.7 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 277.7 |
GaN (mp-804) | <1 1 1> | <1 -1 -1> | 148.0 |
SiO2 (mp-6930) | <0 0 1> | <1 1 0> | 179.8 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 277.7 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 277.7 |
SiO2 (mp-6930) | <1 1 0> | <1 0 1> | 237.4 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 252.9 |
KCl (mp-23193) | <1 0 0> | <1 -1 -1> | 333.1 |
KCl (mp-23193) | <1 1 1> | <1 -1 0> | 225.1 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 1> | 254.5 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 -1> | 217.3 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 -1> | 325.9 |
Te2Mo (mp-602) | <0 0 1> | <1 -1 0> | 32.2 |
Te2Mo (mp-602) | <1 0 0> | <0 1 0> | 284.5 |
Te2Mo (mp-602) | <1 0 1> | <1 -1 0> | 160.8 |
Te2Mo (mp-602) | <1 1 0> | <1 -1 -1> | 185.0 |
Te2Mo (mp-602) | <1 1 1> | <0 0 1> | 92.6 |
InAs (mp-20305) | <1 0 0> | <1 -1 -1> | 37.0 |
InAs (mp-20305) | <1 1 0> | <1 -1 0> | 257.3 |
InAs (mp-20305) | <1 1 1> | <0 1 1> | 254.5 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 158.1 |
Ag (mp-124) | <1 1 0> | <1 -1 1> | 51.0 |
Ag (mp-124) | <1 1 1> | <1 -1 -1> | 185.0 |
ZnSe (mp-1190) | <1 0 0> | <0 1 1> | 101.8 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 239.7 |
ZnSe (mp-1190) | <1 1 1> | <1 -1 0> | 225.1 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 -1 0> | 225.1 |
KTaO3 (mp-3614) | <1 0 0> | <1 -1 -1> | 148.0 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 1> | 203.6 |
GaSe (mp-1943) | <0 0 1> | <0 1 -1> | 217.3 |
GaSe (mp-1943) | <1 0 0> | <0 0 1> | 277.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Zn(NiO2)4 (mvc-10443) | 0.1846 | 0.082 | 3 |
LiMn4O8 (mp-769702) | 0.1820 | 0.027 | 3 |
Li(CoO2)4 (mvc-16812) | 0.1708 | 0.151 | 3 |
MgMn4O8 (mp-1003484) | 0.1871 | 0.037 | 3 |
Zn(FeO2)4 (mvc-11657) | 0.1906 | 0.222 | 3 |
LiMn3CrO8 (mp-780544) | 0.1898 | 0.056 | 4 |
LiMn3NiO8 (mp-762829) | 0.1642 | 0.339 | 4 |
LiCrCo3O8 (mp-763181) | 0.2023 | 0.141 | 4 |
LiFeCo3O8 (mp-763089) | 0.1894 | 0.078 | 4 |
LiTi3VO8 (mp-768011) | 0.1837 | 0.096 | 4 |
Co15O28 (mp-769432) | 0.5307 | 0.024 | 2 |
Ti8O13 (mp-752989) | 0.5043 | 0.008 | 2 |
Mn5O8 (mp-761290) | 0.1999 | 0.080 | 2 |
Co7O12 (mp-771737) | 0.5133 | 0.124 | 2 |
Ti8C5 (mp-27919) | 0.5118 | 0.000 | 2 |
Li4MnSn(WO6)2 (mp-775961) | 0.7197 | 0.051 | 5 |
Li4CrTe(WO6)2 (mp-777147) | 0.7285 | 0.075 | 5 |
Li4CrSb(TeO6)2 (mp-781050) | 0.7234 | 0.048 | 5 |
Li4FeBi(TeO6)2 (mp-776005) | 0.7209 | 0.035 | 5 |
Li4CrBi(TeO6)2 (mp-775998) | 0.7269 | 0.076 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv Ti_pv V_pv O |
Final Energy/Atom-7.6791 eV |
Corrected Energy-110.4923 eV
-110.4923 eV = -99.8280 eV (uncorrected energy) - 5.6183 eV (MP Anion Correction) - 5.0460 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)