Final Magnetic Moment0.148 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.067 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.23 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3c [226] |
Hall-F 4c 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
InAs (mp-20305) | <1 0 0> | <1 0 0> | 153.3 |
GaP (mp-2490) | <1 0 0> | <1 0 0> | 153.3 |
PbSe (mp-2201) | <1 0 0> | <1 0 0> | 153.3 |
Ga2O3 (mp-886) | <1 0 -1> | <1 0 0> | 153.3 |
CdSe (mp-2691) | <1 0 0> | <1 0 0> | 153.3 |
Y3Fe5O12 (mp-19648) | <1 0 0> | <1 0 0> | 153.3 |
SiC (mp-8062) | <1 0 0> | <1 0 0> | 153.3 |
GaSb (mp-1156) | <1 0 0> | <1 0 0> | 153.3 |
SrTiO3 (mp-4651) | <0 0 1> | <1 0 0> | 153.3 |
CaF2 (mp-2741) | <1 0 0> | <1 0 0> | 153.3 |
ZnTe (mp-2176) | <1 0 0> | <1 0 0> | 153.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LaFe9Si4 (mp-662529) | 0.3249 | 0.020 | 3 |
SrCu9Si4 (mp-11142) | 0.3493 | 0.000 | 3 |
SrCu9Ge4 (mp-11144) | 0.1962 | 0.000 | 3 |
BaCu9Ge4 (mp-11145) | 0.2237 | 0.000 | 3 |
LaCoCu12 (mp-13486) | 0.1628 | 0.002 | 3 |
NaZn13 (mp-950) | 0.0280 | 0.000 | 2 |
CaZn13 (mp-672227) | 0.0605 | 0.005 | 2 |
SrZn13 (mp-672707) | 0.0589 | 0.000 | 2 |
RbZn13 (mp-2504) | 0.0264 | 0.000 | 2 |
BaZn13 (mp-672225) | 0.0486 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: K_sv Zn |
Final Energy/Atom-1.3158 eV |
Corrected Energy-36.8426 eV
-36.8426 eV = -36.8426 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)