Final Magnetic Moment11.763 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingUnknown |
Formation Energy / Atom-0.967 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density10.18 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI43d [220] |
HallI 4bd 2c 3 |
Point Group43m |
Crystal Systemcubic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 94.6 |
GaN (mp-804) | <0 0 1> | <1 1 1> | 115.8 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 133.7 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 66.9 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 200.6 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 267.5 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 66.9 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 267.5 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 94.6 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 267.5 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 189.1 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 267.5 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 283.7 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 94.6 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 0> | 189.1 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 94.6 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 133.7 |
CdTe (mp-406) | <1 1 0> | <1 1 0> | 189.1 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 283.7 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 66.9 |
LiF (mp-1138) | <1 1 1> | <1 1 1> | 115.8 |
TeO2 (mp-2125) | <1 1 0> | <1 0 0> | 200.6 |
GdScO3 (mp-5690) | <0 1 0> | <1 0 0> | 133.7 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 0> | 66.9 |
BN (mp-984) | <1 0 1> | <1 0 0> | 267.5 |
Mg (mp-153) | <1 1 1> | <1 0 0> | 267.5 |
GaP (mp-2490) | <1 0 0> | <1 0 0> | 267.5 |
TeO2 (mp-2125) | <1 0 0> | <1 1 0> | 283.7 |
MgO (mp-1265) | <1 1 0> | <1 1 0> | 283.7 |
TbScO3 (mp-31119) | <0 1 0> | <1 0 0> | 133.7 |
TbScO3 (mp-31119) | <1 0 0> | <1 1 0> | 94.6 |
Ni (mp-23) | <1 1 0> | <1 1 0> | 189.1 |
InSb (mp-20012) | <1 1 0> | <1 1 0> | 189.1 |
BaTiO3 (mp-5986) | <0 0 1> | <1 0 0> | 267.5 |
BaTiO3 (mp-5986) | <1 0 1> | <1 1 0> | 94.6 |
GdScO3 (mp-5690) | <1 0 0> | <1 1 0> | 94.6 |
Mg (mp-153) | <1 0 0> | <1 1 0> | 283.7 |
TbScO3 (mp-31119) | <1 1 0> | <1 0 0> | 66.9 |
MoSe2 (mp-1634) | <0 0 1> | <1 1 1> | 115.8 |
Ga2O3 (mp-886) | <0 1 0> | <1 1 0> | 283.7 |
WSe2 (mp-1821) | <0 0 1> | <1 1 1> | 115.8 |
Ga2O3 (mp-886) | <1 1 0> | <1 1 0> | 283.7 |
Si (mp-149) | <1 0 0> | <1 0 0> | 267.5 |
NaCl (mp-22862) | <1 0 0> | <1 0 0> | 66.9 |
NaCl (mp-22862) | <1 1 0> | <1 1 0> | 94.6 |
ZrO2 (mp-2858) | <0 0 1> | <1 0 0> | 133.7 |
C (mp-48) | <1 0 1> | <1 0 0> | 200.6 |
YAlO3 (mp-3792) | <1 1 0> | <1 0 0> | 267.5 |
CdWO4 (mp-19387) | <0 1 0> | <1 0 0> | 133.7 |
ZnO (mp-2133) | <1 0 0> | <1 0 0> | 267.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Pa3P4 (mp-567978) | 0.0089 | 0.000 | 2 |
U3Sb4 (mp-392) | 0.0142 | 0.000 | 2 |
Np3As4 (mp-568285) | 0.0128 | 0.000 | 2 |
Th3Bi4 (mp-23270) | 0.0273 | 0.000 | 2 |
Th3Sb4 (mp-552) | 0.0243 | 0.000 | 2 |
Nd2UTe4 (mp-33312) | 0.2189 | 0.066 | 3 |
Ce3AsS3 (mp-675514) | 0.2203 | 0.038 | 3 |
Ce2USe4 (mp-676083) | 0.2393 | 0.031 | 3 |
Ce2UTe4 (mp-676497) | 0.1910 | 0.040 | 3 |
EuYb2S4 (mp-676878) | 0.1609 | 0.932 | 3 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-points14 |
U Values-- |
PseudopotentialsVASP PAW: P U |
Final Energy/Atom-8.8959 eV |
Corrected Energy-124.5422 eV
-124.5422 eV = -124.5422 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)