Final Magnetic Moment0.005 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.084 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density18.62 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPm3m [221] |
Hall-P 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 345.6 |
LaAlO3 (mp-2920) | <1 1 1> | <1 0 0> | 249.4 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 211.7 |
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 258.7 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 149.7 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 258.7 |
CeO2 (mp-20194) | <1 1 1> | <1 1 1> | 201.6 |
GaAs (mp-2534) | <1 1 1> | <1 1 0> | 282.2 |
AlN (mp-661) | <0 0 1> | <1 1 0> | 164.6 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 211.7 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 199.5 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 199.5 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 211.7 |
BaF2 (mp-1029) | <1 1 1> | <1 1 1> | 201.6 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 33.3 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 47.0 |
GaN (mp-804) | <0 0 1> | <1 1 1> | 115.2 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 282.2 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 199.5 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 249.4 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 83.1 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 86.4 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 299.3 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 83.1 |
KCl (mp-23193) | <1 1 1> | <1 1 1> | 201.6 |
SiO2 (mp-6930) | <1 0 1> | <1 1 1> | 144.0 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 211.7 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 94.1 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 133.0 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 211.7 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 0> | 164.6 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 66.5 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 149.7 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 47.0 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 211.7 |
InAs (mp-20305) | <1 1 1> | <1 1 1> | 201.6 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 33.3 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 47.0 |
ZnSe (mp-1190) | <1 1 1> | <1 1 0> | 282.2 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 16.6 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 23.5 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 1> | 28.8 |
CdS (mp-672) | <0 0 1> | <1 1 1> | 201.6 |
CdS (mp-672) | <1 0 1> | <1 1 0> | 164.6 |
CdS (mp-672) | <1 1 0> | <1 1 1> | 345.6 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 216.2 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 266.1 |
LiF (mp-1138) | <1 1 1> | <1 1 1> | 28.8 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 16.6 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 23.5 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
261 | 145 | 145 | 0 | 0 | 0 |
145 | 261 | 145 | 0 | 0 | 0 |
145 | 145 | 261 | 0 | 0 | 0 |
0 | 0 | 0 | 89 | 0 | 0 |
0 | 0 | 0 | 0 | 89 | 0 |
0 | 0 | 0 | 0 | 0 | 89 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
6.3 | -2.3 | -2.3 | 0 | 0 | 0 |
-2.3 | 6.3 | -2.3 | 0 | 0 | 0 |
-2.3 | -2.3 | 6.3 | 0 | 0 | 0 |
0 | 0 | 0 | 11.2 | 0 | 0 |
0 | 0 | 0 | 0 | 11.2 | 0 |
0 | 0 | 0 | 0 | 0 | 11.2 |
Shear Modulus GV77 GPa |
Bulk Modulus KV184 GPa |
Shear Modulus GR74 GPa |
Bulk Modulus KR184 GPa |
Shear Modulus GVRH75 GPa |
Bulk Modulus KVRH184 GPa |
Elastic Anisotropy0.22 |
Poisson's Ratio0.32 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
ZnCu2Ni (mp-30593) | 0.1125 | 0.005 | 3 |
CrCoPt2 (mp-570863) | 0.0492 | 0.000 | 3 |
LiCa6Ge (mp-12609) | 0.0000 | 0.180 | 3 |
GaFeNi2 (mp-1065359) | 0.0412 | 0.066 | 3 |
GaCo2Ni (mp-1018060) | 0.0157 | 0.075 | 3 |
Cr8Ni50Mo15W2 (mp-767372) | 0.2155 | 0.028 | 4 |
CrFeCoNi (mp-1012640) | 0.3608 | 0.118 | 4 |
CrFeCoNi (mp-1096923) | 0.4019 | 0.193 | 4 |
Sc3In (mp-570428) | 0.0000 | 0.008 | 2 |
EuSn3 (mp-20387) | 0.0000 | 0.000 | 2 |
ErGa3 (mp-398) | 0.0000 | 0.000 | 2 |
NbCo3 (mp-1018021) | 0.0000 | 0.014 | 2 |
LuTl3 (mp-2060) | 0.0000 | 0.000 | 2 |
Na (mp-974558) | 0.0000 | 0.001 | 1 |
Br (mp-998870) | 0.0000 | 0.666 | 1 |
Mn (mp-8634) | 0.0000 | 0.083 | 1 |
Pb (mp-20483) | 0.0000 | 0.000 | 1 |
Cu (mp-30) | 0.0000 | 0.000 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Lu_3 Pt |
Final Energy/Atom-6.7670 eV |
Corrected Energy-27.0681 eV
-27.0681 eV = -27.0681 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)