material

CdP4

ID:

mp-7904

DOI:

10.17188/1307809


Tags: Cadmium tetraphosphide Cadmium phosphide (1/4)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.062 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.011 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.72 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
CdP2 + P
Band Gap
0.526 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P21/c [14]
Hall
-P 2ybc
Point Group
2/m
Crystal System
monoclinic

Electronic Structure

Topological data for ICSD ID 25605 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
AlN (mp-661) <1 0 0> <1 0 1> 0.002 156.8
CdWO4 (mp-19387) <1 0 0> <1 0 1> 0.005 156.8
SiO2 (mp-6930) <1 0 0> <1 1 -1> 0.009 303.0
SiO2 (mp-6930) <1 1 1> <1 0 -1> 0.013 315.1
LiNbO3 (mp-3731) <1 0 0> <0 0 1> 0.018 222.0
BN (mp-984) <1 1 1> <1 0 -1> 0.023 135.0
SiC (mp-8062) <1 1 1> <0 0 1> 0.033 166.5
LiF (mp-1138) <1 0 0> <1 0 0> 0.034 200.6
SiC (mp-7631) <0 0 1> <0 0 1> 0.036 83.2
Mg (mp-153) <1 0 0> <0 0 1> 0.036 83.2
SiC (mp-11714) <0 0 1> <0 0 1> 0.037 83.2
MgF2 (mp-1249) <1 0 0> <0 1 0> 0.041 202.9
Si (mp-149) <1 0 0> <1 0 0> 0.044 120.3
SiC (mp-11714) <1 0 1> <1 0 0> 0.044 160.5
Te2W (mp-22693) <0 1 0> <1 0 0> 0.045 160.5
CeO2 (mp-20194) <1 0 0> <1 0 0> 0.046 120.3
Ge (mp-32) <1 0 0> <1 0 0> 0.046 200.6
Ga2O3 (mp-886) <1 0 0> <1 1 1> 0.051 198.5
Mg (mp-153) <1 1 0> <1 0 0> 0.053 200.6
SiC (mp-11714) <1 0 0> <1 0 1> 0.054 156.8
Ni (mp-23) <1 1 0> <1 1 0> 0.055 228.3
YAlO3 (mp-3792) <0 1 0> <1 0 1> 0.056 156.8
MgF2 (mp-1249) <1 1 0> <0 1 1> 0.056 245.8
YAlO3 (mp-3792) <1 0 1> <0 0 1> 0.058 194.2
SiC (mp-8062) <1 1 0> <0 1 1> 0.059 295.0
ZrO2 (mp-2858) <0 0 1> <0 0 1> 0.061 27.7
NdGaO3 (mp-3196) <0 0 1> <0 0 1> 0.064 277.5
GaN (mp-804) <1 0 0> <0 0 1> 0.064 83.2
MgF2 (mp-1249) <1 0 1> <1 0 -1> 0.067 315.1
GaP (mp-2490) <1 0 0> <1 0 0> 0.069 120.3
TiO2 (mp-2657) <1 0 0> <0 1 1> 0.073 245.8
GaAs (mp-2534) <1 0 0> <1 0 0> 0.075 200.6
BN (mp-984) <1 1 0> <1 0 -1> 0.076 135.0
SiC (mp-7631) <1 0 1> <1 0 0> 0.078 240.7
Au (mp-81) <1 0 0> <0 1 1> 0.080 245.8
GaN (mp-804) <1 0 1> <1 0 -1> 0.084 135.0
C (mp-48) <1 1 0> <1 0 -1> 0.084 135.0
BN (mp-984) <1 0 0> <1 0 1> 0.089 156.8
AlN (mp-661) <1 1 0> <1 1 -1> 0.090 303.0
YAlO3 (mp-3792) <0 1 1> <0 0 1> 0.091 194.2
Ni (mp-23) <1 0 0> <0 0 1> 0.091 111.0
YAlO3 (mp-3792) <0 0 1> <0 0 1> 0.095 27.7
C (mp-48) <1 1 1> <1 0 -1> 0.100 135.0
ZnSe (mp-1190) <1 0 0> <1 0 0> 0.101 200.6
Ga2O3 (mp-886) <1 0 1> <1 1 0> 0.102 228.3
CaF2 (mp-2741) <1 0 0> <1 0 0> 0.103 120.3
BaTiO3 (mp-5986) <1 1 0> <0 1 0> 0.103 284.1
GaTe (mp-542812) <1 0 0> <0 0 1> 0.107 222.0
MgF2 (mp-1249) <0 0 1> <0 0 1> 0.107 111.0
GaN (mp-804) <0 0 1> <0 0 1> 0.115 249.7
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
111 33 35 0 6 0
33 89 40 0 -2 0
35 40 83 0 -4 0
0 0 0 36 0 2
6 -2 -4 0 16 0
0 0 0 2 0 36
Compliance Tensor Sij (10-12Pa-1)
11.2 -2.7 -3.6 0 -5 0
-2.7 14.9 -5.9 0 1.8 0
-3.6 -5.9 16.4 0 3.9 0
0 0 0 27.7 0 -1.3
-5 1.8 3.9 0 64.5 0
0 0 0 -1.3 0 28.1
Shear Modulus GV
29 GPa
Bulk Modulus KV
55 GPa
Shear Modulus GR
26 GPa
Bulk Modulus KR
55 GPa
Shear Modulus GVRH
28 GPa
Bulk Modulus KVRH
55 GPa
Elastic Anisotropy
0.68
Poisson's Ratio
0.29

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
13.10 0.00 0.71
0.00 13.38 0.00
0.71 0.00 11.75
Dielectric Tensor εij (total)
18.88 0.00 0.11
0.00 27.22 0.00
0.11 0.00 29.22
Polycrystalline dielectric constant εpoly
(electronic contribution)
12.75
Polycrystalline dielectric constant εpoly
(total)
25.11
Refractive Index n
3.57
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
LiFeF3 (mp-849232) 0.5908 0.032 3
Ca2Pt3O8 (mp-8710) 0.6367 0.000 3
Co2(GeSe)3 (mp-5094) 0.6390 0.000 3
Li5InO4 (mp-753783) 0.6350 0.054 3
Na(CoO2)3 (mp-690518) 0.6380 0.235 3
Zn2BiWO6 (mvc-5039) 0.6151 0.099 4
Li4Sb(TeO4)3 (mp-753363) 0.6494 0.097 4
LiMnOF2 (mp-766924) 0.5799 0.097 4
LiMnOF2 (mp-765076) 0.6429 0.080 4
Zn2CoWO6 (mvc-6162) 0.6296 0.057 4
MgAs4 (mp-7623) 0.4497 0.000 2
Te2Ir (mp-569322) 0.6415 0.012 2
Mn2O3 (mp-565203) 0.6729 0.000 2
ZnP4 (mp-14587) 0.2932 0.063 2
MgP4 (mp-384) 0.1377 0.000 2
Li4ZrNb(TeO6)2 (mp-756177) 0.6643 0.058 5
Li4Fe2TeWO12 (mp-768021) 0.6838 0.085 5
Li4Cr2TeWO12 (mp-775566) 0.6781 0.080 5
Li4Mn2TeWO12 (mp-768044) 0.6862 0.058 5
Li4V2CrTeO12 (mp-775632) 0.6669 0.104 5
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Cd P
Final Energy/Atom
-4.5773 eV
Corrected Energy
-45.7733 eV
Uncorrected energy = -45.7733 eV Corrected energy = -45.7733 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 25605
  • 620212
Submitted by
User remarks:
  • Cadmium phosphide (1/4)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)