Final Magnetic Moment2.784 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-0.559 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density9.55 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP4/nmm [129] |
HallP 4ab 2ab 1ab |
Point Group4/mmm |
Crystal Systemtetragonal |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 0 1> | 93.1 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 316.6 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 149.0 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 353.3 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 167.6 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 55.5 |
BaF2 (mp-1029) | <1 1 1> | <1 0 0> | 274.8 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 186.2 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 186.2 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 274.8 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 274.8 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 149.0 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 111.7 |
SiO2 (mp-6930) | <1 0 0> | <1 0 1> | 217.3 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 314.1 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 235.5 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 157.0 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 1> | 347.6 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 279.3 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 130.3 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 204.8 |
AlN (mp-661) | <1 1 0> | <1 0 1> | 217.3 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 37.2 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 117.8 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 157.0 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 1> | 217.3 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 1> | 234.2 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 242.1 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 1> | 217.3 |
KCl (mp-23193) | <1 0 0> | <1 1 0> | 166.6 |
KCl (mp-23193) | <1 1 1> | <1 1 0> | 277.6 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 149.0 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 314.1 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 353.3 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 37.2 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 157.0 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 335.2 |
CdS (mp-672) | <1 0 0> | <1 0 1> | 86.9 |
CdS (mp-672) | <1 1 1> | <1 0 1> | 260.7 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 314.1 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 167.6 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 304.2 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 93.1 |
YVO4 (mp-19133) | <1 1 0> | <1 0 1> | 130.4 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 130.3 |
CdS (mp-672) | <1 1 0> | <1 0 1> | 304.2 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 149.0 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 217.3 |
TePb (mp-19717) | <1 0 0> | <1 1 0> | 166.6 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 117.8 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
105 | 67 | 36 | 0 | 0 | 0 |
67 | 105 | 36 | 0 | 0 | 0 |
36 | 36 | 105 | 0 | 0 | 0 |
0 | 0 | 0 | 37 | 0 | 0 |
0 | 0 | 0 | 0 | 37 | 0 |
0 | 0 | 0 | 0 | 0 | 68 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
16.4 | -9.6 | -2.3 | 0 | 0 | 0 |
-9.6 | 16.4 | -2.3 | 0 | 0 | 0 |
-2.3 | -2.3 | 11.1 | 0 | 0 | 0 |
0 | 0 | 0 | 27.1 | 0 | 0 |
0 | 0 | 0 | 0 | 27.1 | 0 |
0 | 0 | 0 | 0 | 0 | 14.7 |
Shear Modulus GV40 GPa |
Bulk Modulus KV66 GPa |
Shear Modulus GR34 GPa |
Bulk Modulus KR65 GPa |
Shear Modulus GVRH37 GPa |
Bulk Modulus KVRH65 GPa |
Elastic Anisotropy0.89 |
Poisson's Ratio0.26 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CeSbTe (mp-917643) | 0.0566 | 0.000 | 3 |
UAsSe (mp-22595) | 0.0655 | 0.081 | 3 |
NpSbTe (mp-1018824) | 0.1515 | 0.000 | 3 |
ThPS (mp-12876) | 0.1327 | 0.000 | 3 |
CeSbTe (mp-30152) | 0.0738 | 0.000 | 3 |
TbS2 (mp-7135) | 0.1387 | 0.059 | 2 |
NdS2 (mp-7698) | 0.1364 | 0.078 | 2 |
PrSe2 (mp-1018940) | 0.1396 | 0.022 | 2 |
NdSe2 (mp-1018817) | 0.1360 | 0.020 | 2 |
DyS2 (mp-1018675) | 0.1296 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: U Sb Te |
Final Energy/Atom-6.7471 eV |
Corrected Energy-40.4827 eV
-40.4827 eV = -40.4827 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)