material

Fe2O3

ID:

mp-19770


Tags: Diiron trioxide Hematite High pressure experimental phase Iron(III) oxide Iron oxide (2/3)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
AFM
Formation Energy / Atom
-1.907 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.07 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
R3c [167]
Hall
-R 3 2"c
Point Group
3m
Crystal System
trigonal

Electronic Structure

Topological data for ICSD ID 15840 from Topological Materials Database
Topological Classification
TI*
Subclassification
SEBR
* Topological insulator
Split Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Bi2Te3 (mp-34202) <0 0 1> <0 0 1> 0.000 68.6
C (mp-48) <0 0 1> <0 0 1> 0.000 68.6
BaF2 (mp-1029) <1 1 1> <0 0 1> 0.007 68.6
WS2 (mp-224) <0 0 1> <0 0 1> 0.010 274.3
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.010 274.3
TePb (mp-19717) <1 1 1> <0 0 1> 0.022 297.2
Mg (mp-153) <1 0 1> <0 0 1> 0.024 320.0
SiC (mp-8062) <1 1 1> <0 0 1> 0.030 297.2
AlN (mp-661) <0 0 1> <0 0 1> 0.034 160.0
Cu (mp-30) <1 0 0> <1 0 1> 0.042 224.0
Mg (mp-153) <0 0 1> <0 0 1> 0.049 274.3
TiO2 (mp-2657) <1 1 1> <0 0 1> 0.050 205.7
Ag (mp-124) <1 0 0> <0 0 1> 0.058 365.7
Cu (mp-30) <1 1 1> <0 0 1> 0.064 22.9
TiO2 (mp-2657) <1 0 0> <1 1 0> 0.080 123.1
Ni (mp-23) <1 1 1> <0 0 1> 0.082 274.3
Au (mp-81) <1 1 1> <0 0 1> 0.098 91.4
ZnO (mp-2133) <1 0 1> <0 0 1> 0.107 297.2
CaF2 (mp-2741) <1 1 1> <0 0 1> 0.111 160.0
NdGaO3 (mp-3196) <0 1 0> <0 0 1> 0.115 342.9
PbSe (mp-2201) <1 1 0> <0 0 1> 0.117 274.3
GaP (mp-2490) <1 1 0> <0 0 1> 0.117 342.9
GaN (mp-804) <0 0 1> <0 0 1> 0.122 274.3
GaSb (mp-1156) <1 1 0> <0 0 1> 0.122 274.3
Ag (mp-124) <1 1 0> <0 0 1> 0.131 365.7
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.131 205.7
CaF2 (mp-2741) <1 1 0> <0 0 1> 0.132 342.9
Te2W (mp-22693) <0 1 0> <1 0 0> 0.132 213.3
CdSe (mp-2691) <1 1 0> <0 0 1> 0.133 274.3
CdWO4 (mp-19387) <0 0 1> <0 0 1> 0.150 91.4
BaTiO3 (mp-5986) <1 0 0> <1 0 0> 0.166 284.4
SiC (mp-7631) <0 0 1> <0 0 1> 0.177 160.0
SiC (mp-11714) <1 1 0> <0 0 1> 0.177 274.3
SiC (mp-11714) <1 0 0> <1 0 0> 0.179 284.4
GaP (mp-2490) <1 1 1> <0 0 1> 0.186 160.0
Au (mp-81) <1 1 0> <0 0 1> 0.188 365.7
SiC (mp-11714) <0 0 1> <0 0 1> 0.190 160.0
LiGaO2 (mp-5854) <1 1 1> <0 0 1> 0.191 274.3
Ag (mp-124) <1 1 1> <0 0 1> 0.207 91.4
ZnO (mp-2133) <1 0 0> <1 0 1> 0.211 298.7
LiGaO2 (mp-5854) <0 1 0> <0 0 1> 0.211 228.6
C (mp-66) <1 1 0> <0 0 1> 0.219 91.4
BN (mp-984) <0 0 1> <0 0 1> 0.222 205.7
Cu (mp-30) <1 1 0> <0 0 1> 0.225 91.4
Si (mp-149) <1 1 0> <0 0 1> 0.245 342.9
CeO2 (mp-20194) <1 1 0> <0 0 1> 0.255 342.9
TiO2 (mp-390) <1 0 1> <0 0 1> 0.260 274.3
Te2Mo (mp-602) <1 0 1> <0 0 1> 0.260 274.3
ZnTe (mp-2176) <1 1 0> <0 0 1> 0.261 274.3
CdS (mp-672) <1 0 1> <1 0 1> 0.266 224.0
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.

Once you have registered you can also "vote" for full calculation of this material's elastic properties.

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
VCrO3 (mp-770778) 0.1619 0.034 3
LiMnF3 (mp-764337) 0.1585 0.040 3
LiMgH3 (mp-23736) 0.1506 0.009 3
NiSnO3 (mp-770398) 0.0847 0.026 3
CoSnO3 (mp-761574) 0.1622 0.036 3
Mg2VWO6 (mvc-5881) 0.3268 0.018 4
Mg2TiWO6 (mvc-5939) 0.3585 0.128 4
Mg2CrWO6 (mvc-5960) 0.3801 0.047 4
InNi2SbO6 (mp-1078367) 0.2580 0.000 4
ScNi2SbO6 (mp-1078244) 0.3277 0.000 4
In2S3 (mp-22375) 0.0834 0.023 2
Ca3N2 (mp-1047) 0.0635 0.014 2
Fe2O3 (mp-714977) 0.0265 0.000 2
Al2O3 (mp-1143) 0.0621 0.000 2
Fe2O3 (mp-796253) 0.0144 0.000 2
Li4Fe2TeWO12 (mp-768021) 0.5998 0.083 5
Li4Cr2TeWO12 (mp-775566) 0.7250 0.081 5
Li4Mn2TeWO12 (mp-768044) 0.6805 0.054 5
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Synthesis Descriptions

F-doped hematite (F-Fe2O3) nanoparticles were synthesized in aqueous solution using microwave irradiation. In a typical procedure, appropriate amounts of iron nitrate (Junsei, Japan), ammonium fluorid [...]
The oxidation behavior of composite SiAlON/MgAlON phases, synthesized from the leaching residue after the aqueous treatment of salt cake from aluminum remelting, is compared with the oxidation of corr [...]
chef hat mixing beaker

Explore more synthesis descriptions for materials of composition Fe2O3.

Text computed by synthesisproject.org.

Calculation Summary

Structure Optimization

Run Type
GGA+U
Energy Cutoff
520 eV
# of K-points
None
U Values
Fe: 5.3 eV
Pseudopotentials
VASP PAW: Fe_pv O
Final Energy/Atom
-6.7493 eV
Corrected Energy
-80.6388 eV
Uncorrected energy = -67.4928 eV Composition-based energy adjustment (-0.687 eV/atom x 6.0 atoms) = -4.1220 eV Composition-based energy adjustment (-2.256 eV/atom x 4.0 atoms) = -9.0240 eV Corrected energy = -80.6388 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 173655
  • 24791
  • 161287
  • 24004
  • 56372
  • 96074
  • 182839
  • 201098
  • 184766
  • 201096
  • 22505
  • 201101
  • 71194
  • 96072
  • 182847
  • 82137
  • 201099
  • 161290
  • 81248
  • 161285
  • 96076
  • 161284
  • 82136
  • 33643
  • 182844
  • 96070
  • 182843
  • 43465
  • 82903
  • 161288
  • 245851
  • 82134
  • 633032
  • 161291
  • 82135
  • 41541
  • 173653
  • 96071
  • 88418
  • 161286
  • 182848
  • 161293
  • 182846
  • 633039
  • 161289
  • 182845
  • 82904
  • 182840
  • 161292
  • 161294
  • 88417
  • 96073
  • 15840
  • 40142
  • 161283
  • 201097
  • 96075
  • 96069
  • 64599
  • 182841
  • 182842
  • 201100
  • 66756
  • 82902
  • 415251
Submitted by
User remarks:
  • Hematite
  • Iron(III) oxide - alpha

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)