Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
0.000 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
20.53 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P63/mmc [194]
Hall
-P 6c 2c
Point Group
6/mmm
Crystal System
hexagonal

Electronic Structure

Topological data for ICSD ID 40355 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
CsI (mp-614603) <1 1 1> <0 0 1> 0.006 107.2
Si (mp-149) <1 1 1> <0 0 1> 0.009 207.6
SiO2 (mp-6930) <0 0 1> <0 0 1> 0.013 87.1
CeO2 (mp-20194) <1 1 1> <0 0 1> 0.014 207.6
GaN (mp-804) <0 0 1> <0 0 1> 0.020 26.8
YVO4 (mp-19133) <0 0 1> <1 0 1> 0.038 156.1
Al2O3 (mp-1143) <0 0 1> <0 0 1> 0.050 20.1
LiF (mp-1138) <1 1 1> <0 0 1> 0.051 87.1
SrTiO3 (mp-4651) <1 0 1> <0 0 1> 0.055 53.6
LiTaO3 (mp-3666) <1 1 0> <1 0 0> 0.056 125.1
NaCl (mp-22862) <1 1 1> <0 0 1> 0.057 167.5
Cu (mp-30) <1 0 0> <1 0 1> 0.063 156.1
GaTe (mp-542812) <1 0 0> <0 0 1> 0.096 180.8
KCl (mp-23193) <1 1 0> <1 1 0> 0.102 173.3
TeO2 (mp-2125) <0 0 1> <0 0 1> 0.121 160.8
LiNbO3 (mp-3731) <1 1 1> <1 1 0> 0.132 130.0
BN (mp-984) <1 0 1> <1 0 1> 0.139 241.2
GdScO3 (mp-5690) <0 0 1> <0 0 1> 0.155 160.8
Ga2O3 (mp-886) <1 1 1> <0 0 1> 0.155 254.5
Fe3O4 (mp-19306) <1 1 1> <0 0 1> 0.166 127.3
WSe2 (mp-1821) <0 0 1> <0 0 1> 0.174 87.1
MoSe2 (mp-1634) <0 0 1> <0 0 1> 0.176 87.1
Fe2O3 (mp-24972) <1 0 0> <0 0 1> 0.176 214.3
GdScO3 (mp-5690) <0 1 0> <0 0 1> 0.176 134.0
SiO2 (mp-6930) <1 1 0> <0 0 1> 0.215 241.1
TiO2 (mp-390) <1 1 0> <1 1 0> 0.226 259.9
WS2 (mp-224) <1 0 1> <1 0 0> 0.237 137.6
ZrO2 (mp-2858) <1 1 -1> <0 0 1> 0.253 180.8
GaP (mp-2490) <1 1 1> <0 0 1> 0.281 207.6
MgF2 (mp-1249) <1 1 0> <1 0 0> 0.282 162.6
Te2W (mp-22693) <1 1 0> <0 0 1> 0.283 221.0
Ga2O3 (mp-886) <1 0 0> <1 1 0> 0.284 108.3
TeO2 (mp-2125) <0 1 1> <1 0 0> 0.287 75.0
LiAlO2 (mp-3427) <0 0 1> <1 0 0> 0.300 137.6
BaF2 (mp-1029) <1 1 1> <0 0 1> 0.303 207.6
Au (mp-81) <1 0 0> <0 0 1> 0.303 140.7
GaN (mp-804) <1 0 1> <1 1 0> 0.307 173.3
ZrO2 (mp-2858) <1 0 1> <0 0 1> 0.310 214.3
LiNbO3 (mp-3731) <0 0 1> <0 0 1> 0.319 167.5
GaP (mp-2490) <1 1 0> <0 0 1> 0.328 214.3
NdGaO3 (mp-3196) <1 0 1> <0 0 1> 0.334 53.6
WS2 (mp-224) <0 0 1> <0 0 1> 0.337 26.8
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.340 26.8
ZnSe (mp-1190) <1 0 0> <0 0 1> 0.355 294.7
ZrO2 (mp-2858) <0 1 1> <1 0 1> 0.361 198.6
ZrO2 (mp-2858) <1 1 1> <0 0 1> 0.379 154.1
MgO (mp-1265) <1 1 1> <0 0 1> 0.387 127.3
Te2Mo (mp-602) <1 0 1> <1 0 0> 0.392 112.6
Te2W (mp-22693) <0 1 0> <1 0 1> 0.426 212.8
ZrO2 (mp-2858) <0 0 1> <1 0 0> 0.437 137.6
Up to 50 entries displayed.
minimal coincident interface area.

Surfaces

Reference for surface energies and properties: Periodic Table of Wulff Shapes
Weighted surface energy γ
2.97 J/m2 (0.19 eV/Å2)
Weighted work function Φ
4.55 eV
Shape factor η
5.14
Surface energy anisotropy αγ
0.096
Miller Indices
(hklm)
Surface Energy
(J/m2, eV/Å2)
Work Function
(eV)
Area Fraction Slab
(CIF)
(0001) 2.57, 0.16 4.77 0.22
(1010) 2.86, 0.18 4.58 0.33
(1120) 3.07, 0.19 4.30 0.10
(2130) 3.10, 0.19 4.06 0.00
(2021) 3.16, 0.20 4.54 0.03
(2241) 3.26, 0.20 4.19 0.00
(1011) 3.28, 0.20 4.67 0.08
(1012) 3.29, 0.21 4.42 0.16
(2131) 3.32, 0.21 4.27 0.00
(1121) 3.36, 0.21 4.06 0.02
(2112) 3.44, 0.21 4.38 0.05
(2132) 3.45, 0.22 4.24 0.00

Grain Boundaries

Reference for grain boundary energies and properties:
Sigma, Σ
type
rotation axis rotation angle GB plane Energy, 𝛾GB
(J/m2)
Work of Separation, Wsep
(J/m2)
Structure
(CIF)
7 twist [0001] 21.79 (0001) 0.97 4.19

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
607 273 214 0 0 0
273 607 214 0 0 0
214 214 670 0 0 0
0 0 0 156 0 0
0 0 0 0 156 0
0 0 0 0 0 167
Compliance Tensor Sij (10-12Pa-1)
2.2 -0.8 -0.4 0 0 0
-0.8 2.2 -0.4 0 0 0
-0.4 -0.4 1.8 0 0 0
0 0 0 6.4 0 0
0 0 0 0 6.4 0
0 0 0 0 0 6
Shear Modulus GV
175 GPa
Bulk Modulus KV
365 GPa
Shear Modulus GR
171 GPa
Bulk Modulus KR
365 GPa
Shear Modulus GVRH
173 GPa
Bulk Modulus KVRH
365 GPa
Elastic Anisotropy
0.10
Poisson's Ratio
0.30

Equations of State

Reference:
Equation E0 (eV) V0 (Å3) B C
mie_gruneisen -12.445 15.083 20.152 6.478
pack_evans_james -12.445 15.084 2.232 3.495
vinet -12.448 15.074 20.526 5.352
tait -12.446 15.073 2.258 5.638
birch_euler -12.446 15.082 2.526 0.507
pourier_tarantola -12.452 15.070 0.389 2.553
birch_lagrange -12.470 15.078 1.450 6.174
murnaghan -12.441 15.100 2.178 3.359
Equations reference

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Cr8Ni50Mo15W2 (mp-767372) 0.2673 0.028 4
CrFeCoNi (mp-1012640) 0.2058 0.065 4
CrFeCoNi (mp-1096923) 0.4091 0.193 4
AsAu3 (mp-984353) 0.0089 0.151 2
Re3Ni (mp-862604) 0.0079 0.000 2
LiMg15 (mp-1023493) 0.0106 0.028 2
Mg15Cd (mp-1023489) 0.0093 0.032 2
Mg2Sb (mp-1094541) 0.0030 0.261 2
Sb (mp-80) 0.0032 0.290 1
Co (mp-987206) 0.0066 0.000 1
Tl (mp-82) 0.0001 0.004 1
Na (mp-10172) 0.0078 0.010 1
Cs (mp-11832) 0.0078 0.035 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Re_pv
Final Energy/Atom
-12.4445 eV
Corrected Energy
-24.8891 eV
Uncorrected energy = -24.8891 eV Corrected energy = -24.8891 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 650067
  • 650066
  • 40355
  • 181195
  • 650069
  • 187306
  • 169880
  • 64719
  • 650068
  • 56135
  • 109248
  • 638452
  • 426968
  • 650071
Submitted by
User remarks:
  • Rhenium

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)